| 闭塞区中Ni2+对核级304不锈钢高温水氧化行为的影响 |
| 匡文军, 吴欣强, 韩恩厚 |
1) 中国科学院金属研究所金属腐蚀与防护国家重点实验室, 沈阳 110016
2) 中国科学院金属研究所辽宁省核电材料安全与评价技术重点实验室, 沈阳 110016 |
|
| EFFECT OF Ni2+ IN OCCLUDED VOLUME ON THE OXIDATION BEHAVIOR OF 304 STAINLESS STEEL IN HIGH TEMPERATURE WATER |
| KUANG Wenjun, WU Xinqiang, HAN En-Hou |
1) State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
2) Liaoning Key Laboratory for Safety and Assessment Technique of Nuclear Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
匡文军 吴欣强 韩恩厚. 闭塞区中Ni2+对核级304不锈钢高温水氧化行为的影响[J]. 金属学报, 2011, 47(7): 927-931.
.
EFFECT OF Ni2+ IN OCCLUDED VOLUME ON THE OXIDATION BEHAVIOR OF 304 STAINLESS STEEL IN HIGH TEMPERATURE WATER[J]. Acta Metall Sin, 2011, 47(7): 927-931.
| [1] Ford F P, Gordon B M, Horn R M. ASM Handbook. ASM International, 2006: 341[2] Scott P M, Combrade P. ASM Handbook. ASM International, 2006: 363[3] Kim Y J. Corrosion, 1999; 55: 81[4] Miyazawa T, Terachi T, Uchida S, Satoh T, Tsukada T, Satoh Y, Wada Y, Hosokawa H. J Nucl Sci Technol, 2006; 43: 884[5] Terachi T, Arioka K. NACE, Houston, TX, 2006, Paper No.06608[6] Kuang W J, Wu X Q, Han E H. Corros Sci, 2010; 52: 4081[7] Ziemniak S E, Hanson M. Corros Sci, 2002; 44: 2209[8] Kuang W J, Han E H, Wu X Q, Rao J C. Corros Sci, 2010; 52: 3654[9] Kuang W J, Wu X Q, Han E H, Ruan L Q. Corros Sci, 2011; 53: 1107[10] Kumai C S, Devine T M. Corrosion, 2007; 63: 1101[11] Thierry D, Persson D, Leygraf C, Boucherit N, Hugotlegoff A. Corros Sci, 1991; 32: 273[12] Oblonsky L J, Devine T M. Corros Sci, 1995; 37: 17[13] Maslar J E, Hurst W S, Bowers W J, Hendricks J H, Aquino M I. J Electrochem Soc, 2000; 147: 2532[14] Maslar J E, Hurst W S, Bowers W J, Hendricks J H. Corrosion, 2002; 58: 739[15] Stellwag B. Corros Sci, 1998; 40: 337[16] Kim Y J, Andresen P L. Corrosion, 2003; 59: 511[17] Kim U C, Kim K M, Kang J S, Lee E H, Kim H P. J Nucl Mater, 2002; 302: 104 |
|