| 铌微合金钢高温变形的本构关系 |
| 贾斌, 彭艳 |
| 燕山大学亚稳材料制备技术与科学国家重点实验室, 轧制设备及成套技术教育部工程研究中心, 秦皇岛 066004 |
|
| CONSTITUTIVE RELATIONSHIPS OF Nb MICROALLOYED STEEL DURING HIGH TEMPERATURE DEFORMATION |
| JIA Bin, PENG Yan |
| State Key Laboratory of Metastable Materials Science and Technology, Engineering Research Center of Rolling Equipment and Complete Technology of Ministry of Education, Yanshan University, Qinhuangdao 066004 |
引用本文:
贾斌 彭艳. 铌微合金钢高温变形的本构关系[J]. 金属学报, 2011, 47(4): 507-512.
,
.
CONSTITUTIVE RELATIONSHIPS OF Nb MICROALLOYED STEEL DURING HIGH TEMPERATURE DEFORMATION[J]. Acta Metall Sin, 2011, 47(4): 507-512.
| [1] Qi J J. Microalloyed Steels. Beijing: Metallurgy Industry Press, 2006: 1(齐俊杰. 微合金化钢. 北京: 冶金工业出版社, 2006: 1)[2] Tamura I, translated byWang G D. Controlled Rolling and Controlled Cooling of HSLA Steels. Beijing: Metallurgy Industry Press, 1992: 4(田村今男, 王国栋译. 高强度低合金钢的控制轧制与控制冷却. 北京: 冶金工业出版社, 1992: 4)[3] Ebranimi R, Zahiri S H, Najafizadeh A. J Mater Process Technol, 2006; 171: 301[4] Wang M, Hong H P, Wang X M. J Wuhan Univ Sci Technol, 1999; 33: 134(王孟, 洪慧平, 王晓明. 武汉科技大学学报, 1999; 33: 134)[5] Lin Y C, Chen M S, Zhong J. J Cent South Univ (Sci Technol), 2008; 39: 549(蔺永诚, 陈明松, 钟掘. 中南大学学报(自然科学版), 2008; 39: 549)[6] Xu G, Xu C S, Zhao J R. ISIJ Int, 2006; 46: 166[7] Nakata N, Militzer M. ISIJ Int, 2005; 45: 82[8] Najafizadeh A, Jonas J J. ISIJ Int, 2005; 46: 1679[9] Lin W, Li H Y, Zeng C T, Bin J, Wei D D. J Cent South Univ (Sci Technol), 2010; 41: 940(林武, 李红英, 曾翠婷, 宾杰, 魏冬冬. 中南大学学报(自然科学版), 2010; 41: 940)[10] Zhang H Y, Zhang H B, Chen H S. Mater Mech Eng, 2007; 31: 92(张红英, 张鸿冰, 陈浩时. 机械工程材料, 2007; 31: 92)[11] Pu Z J. Mater Sci Eng, 1995; A192: 780[12] Laasraoui A, Jonas J J. Metall Trans, 1991; 22A: 1545[13] He Y Z, Chen D H, Lei T Q. Iron Steel, 1999; 34: 29(何宜柱, 陈大宏, 雷廷权. 钢铁, 1999; 34 : 29)[14] Suh D W, Cho J Y, Oh K H, Lee H C. ISIJ Int, 2002; 42: 564[15] Humphreys F J, Hatherly M. Recrystallization and Related Annealing Phenomena. Oxford: Pergamon Press, 1995: 363[16] Yoshie A, Fujita T, Fujioka M, Okamoto K, Morikawa H. ISIJ Int, 1996; 36: 474[17] Minami K, Siciliano Jr F, Maccagno, T M, Jonas J J. ISIJ Int, 1996; 36: 1507[18] Hodgson P D, Gibbs R K. ISIJ Int, 1992; 32: 1329[19] Manohar P A, Kyuhwan L, Rollett A D, Youngseog L. ISIJ Int, 2003; 43: 1421[20] Ma B, Peng Y, Liu Y F, Jia B. Trans Mater Heat Treat, 2010; 31: 141(马博, 彭艳, 刘云飞, 贾斌. 材料热处理学报, 2010; 31: 141) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|