| 海水飞溅区Ni-Cu-P钢的锈层和耐点蚀性能研究 |
| 曹国良 李国明 陈珊 常万顺 陈学群 |
| 海军工程大学理学院化学与材料系, 武汉 430033 |
|
| STUDY ON RUST LAYERS AND PITTING CORROSION RESISTANCE OF Ni-Cu-P STEEL EXPOSED IN MARINE SPLASH ZONE |
| CAO Guoliang, LI Guoming, CHEN Shan, CHANG Wanshun, CHEN Xuequn |
| Department of Chemistry and Materials, College of Sciences, Naval University of Engineering, Wuhan 430033 |
引用本文:
曹国良 李国明 陈珊 常万顺 陈学群. 海水飞溅区Ni-Cu-P钢的锈层和耐点蚀性能研究[J]. 金属学报, 2011, 47(2): 145-151.
,
,
,
,
.
STUDY ON RUST LAYERS AND PITTING CORROSION RESISTANCE OF Ni-Cu-P STEEL EXPOSED IN MARINE SPLASH ZONE[J]. Acta Metall Sin, 2011, 47(2): 145-151.
| [1] Matsushima I, translated by Jin Y K. Low Alloy Corrosion Resistant Steel—A History of Development Application and Research. Beijin: Metallurgical Industry Press, 2004: 100(松岛 岩, 靳裕康, 译. 低合金钢耐蚀钢---开发、发展及研究. 北京: 冶金工业出版社, 2004: 100)[2] Melchers R E. Corros Sci, 2004; 46: 1669[3] Huang J Z, Zuo Y. Resistance to Corrosion and Corrosive Data of Materials. Beijin: Chemical Industry Press, 2003: 97(黄建中, 左 禹. 材料的耐蚀性和腐蚀数据. 北京: 化学工业出版社, 2003: 97)[4] Townsend H E. Corrosion, 2001; 57: 497[5] Suzuki S, Takahashi Y, Kamimura T, Miyuhi H, Shinoda K, Tohji K, Waseda Y. Corros Sci, 2004; 46: 1751[6] Wang JM, Chen X Q, Li G M. J Univ Sci Technol Beijing (Engl Ed), 2004; 11: 555[7] Cao G L, Li G M, Chen S, Chang W S, Chen X Q. Acta Metall Sin, 2010; 46: 748(曹国良, 李国明, 陈 珊, 常万顺, 陈学群. 金属学报, 2010; 46: 748)[8] Cui X L, Wang X R, Ma J H, Zhang L, Huang G Q. J Iron Steel Res, 1995; 7(4): 43(崔秀岭, 王相润, 马巾华, 张陆, 黄桂桥. 钢铁研究学报, 1995; 7(4): 43)[9] Zhang Q C, Wu J S, Zheng W L, Wang J J. J Mater Sci Technol, 2002; 18: 455[10] Choi Y S, Shim J J, Kim J G. Mater Sci Eng, 2004; A385: 148[11] Kimura M, Kihira H, Ohta N, Hashimoto M. Corros Sci, 2005; 47: 2499[12] Ishikawa T, Maeda A, Kandori K. Corrosion, 2006; 62: 559[13] Chen Y Y, Tzeng H J, Wei L I, Wang L H, Oung J C, Shih H C. Corros Sci, 2005; 47: 1001[14] Chen X H, Dong J H, Han E H. Mater Lett, 2007; 61: 4050[15] Zhang C, Cai D, Liao B, Zhao T, Fan Y. Mater Lett, 2004; 58: 1524[16] Yang W, Gu J X, Li Q S, Xiao J X. Localized Corrosion of Metals. Beijin: Chemical Industry Press, 1995: 59(杨 武, 顾\濬祥, 黎樵燊 , 肖京先. 金属的局部腐蚀. 北京: 化学工业出版社, 1995: 59)[17] Wang J M, Chen X Q, Chang W S, Zhu X. J Harbin Inst Technol, 2006; 38: 1943(王建民, 陈学群, 常万顺, 朱 锡. 哈尔滨工业大学学报, 2006; 38: 1943)[18] Li Q X, Wang Z Y, Han W, Han E H. Acta Phys Chim Sin, 2008; 24: 1459(李巧霞, 王振尧, 韩 薇, 韩恩厚. 物理化学学报, 2008; 24: 1459)[19] Stratmann M, Bohnenkamp K, Ramchandran T. Corros Sci, 1987; 27: 905[20] Dillmann P, Balasubramaniam R, Beranger G. Corros Sci, 2002; 44: 2231[21] Bijayani P, Balasubramaniam R, Gopal D. Corros Sci, 2008; 50: 1684[22] Yang X Z, Yang W. Corrosive Electrochemical Thermodynamic Potential—pH Diagram and Application of Metals. Beijin: Chemical industry Press, 1991: 138(杨熙珍, 杨 武. 金属腐蚀电化学热力学电位-pH图及其应用. 北京: 化学工业出版社, 1991: 138)[23] Sourisseau T, Chauveau E, Baroux B. Corros Sci, 2005; 47: 1117[24] Kihira H, Ito S, Murata T. Corros Sci, 1990; 31: 383[25] Zhang H, Chen X Q, Chang W S. J Univ Sci Technol Beijing, 2008; 30: 1133(张恒, 陈学群, 常万顺. 北京科技大学学报, 2008; 30: 1133) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|