| 无Ni型锆基块体非晶合金在生物模拟体液中的摩擦磨损性能 |
| 黄彩云; 谌祺; 柳林 |
| 华中科技大学材料成形与模具技术国家重点实验室; 武汉 430074 |
|
| FRICTION AND WEAR PROPERTIES OF Ni–FREE Zr–BASED BULK METALLIC GLASSES IN SIMULATED BODY FLUID |
| HUANG Caiyun; CHEN Qi; LIU Lin |
| The State Key Laboratory of Material Processing and Die & Mould Technology; Deportment of Materials Science and Engineering; Huazhong University of Science and Technology; Wuhan 430074 |
引用本文:
黄彩云 谌祺 柳林. 无Ni型锆基块体非晶合金在生物模拟体液中的摩擦磨损性能[J]. 金属学报, 2010, 46(6): 681-686.
,
,
.
FRICTION AND WEAR PROPERTIES OF Ni–FREE Zr–BASED BULK METALLIC GLASSES IN SIMULATED BODY FLUID[J]. Acta Metall Sin, 2010, 46(6): 681-686.
| [1] Yang S H. Joint Replacement Surgery. Beijing: Tsinghua University Press, 2005: 1
(杨述华. 关节置换外科学. 北京: 清华大学出版社, 2005: 19)
[2] Wang A, Sun D C, Yau S S, Edwards B, Sokol M, Essner A, Polineni V K, Stark C, Dumbleton J H. Wear, 1997; 230: 203
[3] Ge S R, Wang Q L, Zhang D K, Zhu H, Xiong D S, Huang C H, Huang X L. Wear, 2003; 255: 1069
[4] Chen W R, Wang Y M, Qiang J B, Xu W P, Wang D H, Dong C, Xu T, Zhang A M. Tribology, 2003; 23: 14
(陈伟荣, 王英敏, 羌建兵, 徐卫平, 王德和, 董闯, 徐洮, 张爱民. 摩擦学学报, 2003; 23: 14)
[5] Xiao H X, Chen G, La P Q. Tribology, 2006; 26: 140
(肖华星, 陈光, 喇培清. 摩擦学学报, 2006; 26: 140)
[6] Parlar Z, Bakkal M, Shih A J. Intermetallics, 2008; 16: 34
[7] Li G, Wang Y Q, Gao Y P. J Mater Res, 2002; 17: 1877
[8] Jin H W, Ayer R, Koo J Y. J Mater Res, 2007; 22: 264
[9] Blau P J. Wear, 2001; 250: 431
[10] Qiu C L, Chen Q, Liu L, Chan K C, Zhou J X, Chen P P, Zhang S M. Scr Mater, 2006; 55: 605
[11] Mischler S, Spiegel A, Landolt D. Wear, 1999; 225–229: 1078
[12] Wen S Z. Principles of Tribology. Beijing: Tsinghua University Press, 1990: 385
(温诗铸. 摩擦学原理. 北京: 清华大学出版社, 1990: 385)
[13] Rabinowitcz E, Dunn L A, Russel P G. Wear, 1961; 4: 345
[14] Fu X, Kasai T, Falk M L, Rigney D A. Wear, 2001; 250: 409
[15] Tam C Y, Shek C H. Mater Sci Eng, 2004; A384: 138
[16] Ma M Z, Liu R P, Xiao Y, Lou D C, Liu L, Wang Q, Wang W K. Mater Sci Eng, 2004; A386: 326
[17] Ishida M, Takeda H, Nishiyama N, Kita K, Shimizu Y, Saotome Y, Inoue A. Mater Sci Eng, 2007; A449–451: 149
[18] Miyoshi K, Buckley D H. Wear, 1986, 110: 295
[19] Kishore U S, Sudarsan U, Chandran N, Chattopadhyay K. Acta Metall, 1987; 35: 1463 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|