金属学报  2010, Vol. 46 Issue (3): 340-345    DOI: 10.3724/SP.J.1037.2009.00210
  论文 本期目录 | 过刊浏览 |
垂直电场下BaTiO3单晶的畴变与压痕裂纹的演化
赵显武1); 褚武扬2); 乔利杰2)
1) 北京大学力学与空天技术系; 北京 100871 2) 北京科技大学腐蚀与防护中心; 北京100083
DOMAIN SWITCHING AND THE CHANGE IN INDENTATION CRACKS FOR BaTiO3 SINGLE CRYSTAL UNDER THE ELECTRIC FIELD PERPENDICULAR TO THE POLARIZATION
ZHAO Xianwu1); CHU Wuyang2); QIAO Lijie2)
1) Department of Mechanics and Aerospace Engineering; Peking University; Beijing 100871 2) Corrosion and Protection Center; University of Science and Technology Beijing; Beijing 100083
引用本文:

赵显武 褚武扬 乔利杰. 垂直电场下BaTiO3单晶的畴变与压痕裂纹的演化[J]. 金属学报, 2010, 46(3): 340-345.
, , , . DOMAIN SWITCHING AND THE CHANGE IN INDENTATION CRACKS FOR BaTiO3 SINGLE CRYSTAL UNDER THE ELECTRIC FIELD PERPENDICULAR TO THE POLARIZATION[J]. Acta Metall Sin, 2010, 46(3): 340-345.

全文: PDF(874 KB)  
摘要: 

利用微分干涉相衬显微镜, 在垂直于极化方向的电场下, 对BaTiO3单晶的畴变过程和单晶上压痕裂纹的变化过程进行了原位观察. 通过对压痕周围和远离压痕区畴变过程的对比, 研究了压痕对其周围畴变的影响. 结果显示, 面内极化试样在垂直于极化方向的面内电场作用下, 原有压痕和压痕裂纹随整个试样经历90o畴变后也要发生变化, 变化后其形貌与在新的极化状态下重新压制的压痕相似; 对离面极化试样加面内电场时, 畴变速度先增大后减小, 畴变完成一半时, 速度最大; 而且畴变初始阶段速度呈现大小相间的振荡性.

关键词 : BaTiO3单晶,  畴变,  压痕裂纹,  断裂    
Abstract:

As a ferroelectric material, BaTiO3 single crystal has the domain structure which can be changed by the application of mechanical stress and electric field. Therefore, the fracture behavior of the crystal is closely related with the domain switching. To understand the relationship between the fracture behavior and the domain switching clearly, the change of the indentation cracks and domain switching around the indentation under electric field perpendicular to the polarization of the samples were investigated through in situ observations by a differential interference contrast microscopy. The results show that for in-plane polarized sample, after completion of domain switching under the in-plane electric field perpendicular to the polarization of the crystal, the indentation cracks and the domains around the indentation are the same as the new indentation on the sample with new polarization state. In the case of applying in-plane electric field on the anti-plane polarized sample, the speed of the domain switching increases in the initial stage and decreases in the end stage, it has the maximum value as half of the domain switching completed. And the speed fluctuates in the\linebreak first stage.

Key words: BaTiO3 single crystal    domain switching    indentation crack    fracture
收稿日期: 2009-04-07     
基金资助:

国家自然科学基金项目50632010和50572006资助

作者简介: 赵显武, 男, 蒙古族, 1967年生, 讲师

[1] Yang W. Mechatronic Reliability. Beijing: Tsinghua University Press, 2001: 9
(杨卫. 力电失效学. 北京: 清华大学出版社, 2001: 9)
[2] Hao T H, Gong X, Suo Z. J Mech Phys Solids, 1996; 44: 23
[3] Li J Y, Rogan R C, Ustundag E, Bhattacharya E. Nat Mater, 2005; 4: 776
[4] Rogan R C, Tamura N, Swift G A, Ustundag E. Nat Mater, 2003; 2: 379
[5] Holt M, Hassani K, Sutton M. Phys Rev Lett, 2005; 95: 085504
[6] Park Y B, Ruglovsky J L, Atwater H A. Appl Phys Lett, 2004; 85: 455
[7] Li Z, Foster C M, Dai X H, Chan S K, Lam D J. J Appl Phys, 1992; 71: 4481
[8] Zhao X W, Chu W Y, Su Y J, Li J X, Gao K W, Qiao L J. Acta Metall Sin, 2006; 42: 13
(赵显武, 褚武扬, 宿彦京, 李金许, 高克玮, 乔利杰. 金属学报, 2006; 42: 13)

[9] Yang W, Fang F, Tao M. Int J Solids Struct, 2001; 38: 2203
[10] Busche M J, Hsia K J. Scr Mater, 2001; 44: 207
[11] Fang F, Yang W. Mater Lett, 2002; 57: 198
[12] Oliver W C, Pharr G M. J Mater Res, 1992; 7: 1564
[13] Bhushan B, Li X D. Int Mater Rev, 2003; 48: 125
[14] Li X D, Bhushan B. Mater Charact, 2002; 48: 11
[15] Gong J H. Fracture Mechanics of Ceramics. Beijing: Tsinghua University Press, 2001: 88
(龚江宏. 陶瓷材料断裂力学. 北京: 清华大学出版社, 2001: 88)
[16] Yoffe E H. Philos Mag, 1982; 46: 617
[17] Jiang B, Bai Y, Cao J L, Su Y J, Shi S Q, Chu W Y, Qiao L J. J Appl Phys, 2008; 103: 116102

[1] 谷瑞成, 张健, 张明阳, 刘艳艳, 王绍钢, 焦大, 刘增乾, 张哲峰. 三维互穿结构SiC晶须骨架增强镁基复合材料制备及其力学性能[J]. 金属学报, 2022, 58(7): 857-867.
[2] 吴进, 杨杰, 陈浩峰. 纳入残余应力时不同拘束下DMWJ的断裂行为[J]. 金属学报, 2022, 58(7): 956-964.
[3] 彭子超, 刘培元, 王旭青, 罗学军, 刘健, 邹金文. 不同服役条件下FGH96合金的蠕变特征[J]. 金属学报, 2022, 58(5): 673-682.
[4] 赵永好, 毛庆忠. 纳米金属结构材料的韧化[J]. 金属学报, 2022, 58(11): 1385-1398.
[5] 胡晨, 潘帅, 黄明欣. 高强高韧异质结构温轧TWIP钢[J]. 金属学报, 2022, 58(11): 1519-1526.
[6] 范国华, 缪克松, 李丹阳, 夏夷平, 吴昊. 从局域应力/应变视角理解异构金属材料的强韧化行为[J]. 金属学报, 2022, 58(11): 1427-1440.
[7] 陈瑞润, 陈德志, 王琪, 王墅, 周哲丞, 丁宏升, 傅恒志. Nb-Si基超高温合金及其定向凝固工艺的研究进展[J]. 金属学报, 2021, 57(9): 1141-1154.
[8] 周红伟, 白凤梅, 杨磊, 陈艳, 方俊飞, 张立强, 衣海龙, 何宜柱. 1100 MPa级高强钢的低周疲劳行为[J]. 金属学报, 2020, 56(7): 937-948.
[9] 杨杰, 王雷. 核电站DMWJ中材料拘束的影响与优化[J]. 金属学报, 2020, 56(6): 840-848.
[10] 于家英, 王华, 郑伟森, 何燕霖, 吴玉瑞, 李麟. 热浸镀锌高强汽车板界面组织对其拉伸断裂行为的影响[J]. 金属学报, 2020, 56(6): 863-873.
[11] 易红亮,常智渊,才贺龙,杜鹏举,杨达朋. 热冲压成形钢的强度与塑性及断裂应变[J]. 金属学报, 2020, 56(4): 429-443.
[12] 朱健, 张志豪, 谢建新. 基于原位TEM拉伸的稀土H13钢塑性形变行为和断裂机制[J]. 金属学报, 2020, 56(12): 1592-1604.
[13] 刘杨,王磊,宋秀,梁涛沙. DD407/IN718高温合金异质焊接接头的组织及高温变形行为[J]. 金属学报, 2019, 55(9): 1221-1230.
[14] 周丽,张鹏飞,王全兆,肖伯律,马宗义,于涛. B4C/6061Al复合材料热压缩断裂行为的多尺度研究[J]. 金属学报, 2019, 55(7): 911-918.
[15] 李一哲, 龚宝明, 刘秀国, 王东坡, 邓彩艳. 面外拘束效应对单边缺口拉伸试样断裂韧性的影响[J]. 金属学报, 2018, 54(12): 1785-1791.