| 含有微量O,S,C的Fe-Nb-Ce溶液热力学性质的研究 |
| 周谦莉;杜挺 |
| 冶金工业部钢铁研究总院;北京冶金部钢铁研究总院16室;高级工程师(教授级) |
|
| THERMODYNAMICS OF Fe-Nb-Ce LIQUID SOLUTIONS CONTAINING TRACE O, S AND C |
| ZHOU Qianli;DU Ting Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing |
引用本文:
周谦莉;杜挺. 含有微量O,S,C的Fe-Nb-Ce溶液热力学性质的研究[J]. 金属学报, 1989, 25(1): 91-95.
,
.
THERMODYNAMICS OF Fe-Nb-Ce LIQUID SOLUTIONS CONTAINING TRACE O, S AND C[J]. Acta Metall Sin, 1989, 25(1): 91-95.
1 Gschneidner K A Jr., Verkade M E. Selected Cerium Phase Diagrams, Rare-Earth Information Center, Energy and Minerals Resources Institute, Iowa State University, Ames, Iowa, 1974, ISRIC-7, 17 2 Janke D, Fischer W A. Arch Eisenhuettenwes, 1975; 46: 755 3 Schmalzried H. Z Phys Chem, Neue Fol, 1963; 38: 87 4 王龙妹,杜挺.稀土,1984;(4) :39 5 韩其勇,刘士伟,牛红兵,唐志伟.金属学报,1982;18:176 6 日本铁钢协会编.铁钢便览,第1卷:基础,第三版,东京:丸善株式会社,1981:15 7 王常珍,王福珍,杜英敏,张小平.金属学报,1980;16:83 8 Du Ting (杜挺). Proc Int Conf of the Production and Application of Less Common Metals, The Chinese Society of Metals, Hangzhou, China, 1982, Book 1, Paper 11 9 Wu Yieming (吴夜明), Wang Longmei (王龙妹), Du Ting (杜挺). J Less-Common Met, 1985; 110: 18 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|