| 预形变和时效Al-2.73Li合金的断裂机制 |
| 孙东立;杨德庄;崔约贤;雷廷权 |
| 哈尔滨工业大学9系921教研室;讲师;哈尔滨(150006);哈尔滨工业大学;哈尔滨工业大学;哈尔滨工业大学 |
|
| FRACTURE MECHANISM OF PRE-DEFORMATION-AGED Al-2.73Li ALLOY |
| SUN Dongli;YANG Dezhuang;CUI Yuexian;LEI Tingquan Harbin Institute of Technology Faculty 921;Department No.9; Harbin Institute of Technology; Harbin 150006 |
引用本文:
孙东立;杨德庄;崔约贤;雷廷权. 预形变和时效Al-2.73Li合金的断裂机制[J]. 金属学报, 1990, 26(2): 57-63.
,
,
,
.
FRACTURE MECHANISM OF PRE-DEFORMATION-AGED Al-2.73Li ALLOY[J]. Acta Metall Sin, 1990, 26(2): 57-63.
1 Starke E A Jr., Sanders T H Jr. Aluminium-Lithium Alloys, TMS-AIMS, 1981 2 Starke E A Jr., Sanders T H Jr. Aluminium-Lithium Alloys II, TMS AIME, 1984 3 Baker C, Gregson P J, Harris S J, Pell C J, Aluminium-Lithium Alloys III, London: The Institute of Metals, 1986 4 Furulawa M, Miura Y, Nemoto M. Trans Jpn Inst Met, 1985; 26: 230 5 Sun D L (孙东立), Yang D Z (杨德庄), Lei T Q (雷廷权), In: Proc of Tokyo University of Technology and Harbin Institute of Technology Symp. on Materials Science, Tokyo: Tokyo University of Technology 1988; 58 6 Sun D L (孙东立), Yang D Z (杨德庄), Hong Y (洪云), Lei T Q (雷廷权). Strength of Metals and Alloys, (ICSMA 8) , New York: Pergamon, 1988 7 Williams D B, Edington J W. Met Sci, 1975; 9: 529 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|