| Ce对2090Al-Li合金疲劳裂纹扩展行为的影响 |
| 陈铮;李明利;何明 |
| 西北工业大学;讲师;西北工业大学;西北工业大学 |
|
| INFLUENCE OF Ce ON FATIGUE CRACK GROWTH OF 2O9O Al-Li ALLOY |
| CHEN Zheng;LI Mingli;HE Ming Northwestern Polytechnical University; Xi'an |
引用本文:
陈铮;李明利;何明. Ce对2090Al-Li合金疲劳裂纹扩展行为的影响[J]. 金属学报, 1991, 27(2): 75-78.
,
,
.
INFLUENCE OF Ce ON FATIGUE CRACK GROWTH OF 2O9O Al-Li ALLOY[J]. Acta Metall Sin, 1991, 27(2): 75-78.