晶界碳化物对Fe-Cr15-Ni25合金蠕变裂纹扩展行为的影响 |
王富岗;祝苏明;朱世杰;任晓民;谭毅;张俊善 |
大连理工大学;大连理工大学;大连理工大学;大连理工大学;大连理工大学;大连理工大学 |
|
EFFECT OF BOUNDARY CARBIDE ON CREEP CRACK GROWTH IN Fe-Cr15-Ni25 ALLOY |
WANG Fugang;ZHU Suming;ZHU Shijie;REN Xiaoming;TAN Yi;ZHANG Junshan Dalian University of Technology |
引用本文:
王富岗;祝苏明;朱世杰;任晓民;谭毅;张俊善. 晶界碳化物对Fe-Cr15-Ni25合金蠕变裂纹扩展行为的影响[J]. 金属学报, 1991, 27(4): 54-58.
,
,
,
,
,
.
EFFECT OF BOUNDARY CARBIDE ON CREEP CRACK GROWTH IN Fe-Cr15-Ni25 ALLOY[J]. Acta Metall Sin, 1991, 27(4): 54-58.
1 Horton G A P. Acta Metall, 1972; 20: 427 2 张俊善,陈卫星,曹智本.金属学报,1989;25:A141 3 Perry A J. J Mater Sci, 1974; 9: 1016 4 Cadek J. Creep in Metallic Materials, Elsevier Science Publishers, 1988: 189 5 Chen I-W. Scr Metall, 1983; 17: 17y |
|