| 高Ti合金中液析η相的研究 |
| 郭守仁;卢德忠 |
| 中国科学院金属研究所;副研究员;中国科学院金属研究所 |
|
| ON THE PRIMARY η-PHASE IN HIGH-Ti Ni-Fe-Cr BASED SUPERALLOY |
| GUO Shouren; LU Dezhong Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
郭守仁;卢德忠. 高Ti合金中液析η相的研究[J]. 金属学报, 1991, 27(6): 27-32.
,
.
ON THE PRIMARY η-PHASE IN HIGH-Ti Ni-Fe-Cr BASED SUPERALLOY[J]. Acta Metall Sin, 1991, 27(6): 27-32.