| 铸铁熔体中石墨生长方式的转变与变质机理的探讨 |
| 刘永坤;杨士浩 |
| 西南技术工程研究所;山东工业大学 |
|
| GROWTH MODE AND MODIFICATION OF GRAPHITE IN CAST IRON MELT |
| LIU Yongkun;YANG Shihao Southwestern Institute of Technology and Engineering; Chongqing; Shandong Polytechnical University; Jinan |
引用本文:
刘永坤;杨士浩. 铸铁熔体中石墨生长方式的转变与变质机理的探讨[J]. 金属学报, 1992, 28(1): 85-89.
,
.
GROWTH MODE AND MODIFICATION OF GRAPHITE IN CAST IRON MELT[J]. Acta Metall Sin, 1992, 28(1): 85-89.
1 Hillert M, Lindblom Y. J Iron Steel Inst, 1954; 176: 388 2 Minkoff I, Nixon W C. J Appl Phys, 1966; 37: 4848--4855 3 陈熙琛.机械工程学报,1979;15(2) :122--152 4 Minkoff I,Lux B.见:Lux B, Minkoff I, Mollark F主编,上海工业大学,华中工学院,浙江大学合译.铸铁冶金学.北京:机械工业出版社,1983:315--328 5 Liu P C, Loper C R Jr., Kimura T, Park H K. Trans Am Foundrymen's Soc, 1980; 88: 97--118 6 刘永坤.山东工业大学硕士学位论文,1987 7 Jackson K A. In: Doremus R H, Robert B W, Turnbull D eds., Growth and Perfection of Crystals, Proc Int Conf on Crystal Growth, held Cooperstown, New York, August 27--29, 1958, New York: John Wiley Sons, 1958: 319 8 Purdy G R, Audier M. In: Fredriksson H, Hillert M eds., The Physical Metallurgy of Cast Iron. Proc 3rd Int Symp on the Physical Metalluregy of Cast Iron, Stockholm, Sweden, August 29--31, 1984. Elsevier Science, 1985: 13--24 9 Double D D, Hellawell A. Acta Metall, 1974; 22: 481--487 10 宋维锡,杨文英.金属学报,1987;23:B324 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|