| VIRALL复合板的振动阻尼特性 |
| 隋国鑫;何冠虎;白良愈;周本濂 |
| 中国科学院国际材料物理中心;中国科学院金属研究所 |
|
| VIBRATION DAMPING CHARACTERISTICS OF VIRALL LAMINATES |
| SUI Guoxin1;2); HE Guanhui1;2); BAI Liangyu 2); ZHO U Benlian1;2)1) International Centre for Materials Physics; Chinese Academy of Sciences;Shenyang 110015 2) Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015 (Manuscript received 1995-03-03; in revised form 1995-07-07) |
引用本文:
隋国鑫;何冠虎;白良愈;周本濂. VIRALL复合板的振动阻尼特性[J]. 金属学报, 1996, 32(1): 97-100.
,
,
,
.
VIBRATION DAMPING CHARACTERISTICS OF VIRALL LAMINATES[J]. Acta Metall Sin, 1996, 32(1): 97-100.
| 1LinDX,NiRG,AdamsRD.JCompMater,1984;18:1322BalisCremaL,CastellaniA,DragoU.Composites,1989;20(6):5933GibsonRF.ShockVibrationDigest,1987;19(7):134HwangSJ,GibsonRF.CompSciTechnol,1991;4:3795应怀樵.振动测试和分析.北京:中国铁道出版社,1987:16SuiGX,ZhouBL,ZhengZG,ZhouCT,ShiCX.Composites,1993;24(5):4337丁文镜.减振理论.北京:清华大学出版社,1988:1 |
|