| 异种材料连接技术及其在复杂结构制造中的应用 |
冯吉才1,2, 宋晓国1,2( ), 刘多2, 周利2, 檀财旺2, 陈波2 |
1 哈尔滨工业大学 材料结构精密焊接与连接全国重点实验室 哈尔滨 150001 2 哈尔滨工业大学(威海) 山东省特种焊接技术重点实验室 威海 264200 |
|
| Joining Technology of Dissimilar Materials and Its Application in Complex Structure Manufacturing |
FENG Jicai1,2, SONG Xiaoguo1,2( ), LIU Duo2, ZHOU Li2, TAN Caiwang2, CHEN Bo2 |
1 State Key Laboratory of Precision Welding & Joining of Materials and Structures, Harbin Institute of Technology, Harbin 150001, China 2 Shandong Provincial Key Laboratory of Special Welding Technology, Harbin Institute of Technology at Weihai, Weihai 264200, China |
引用本文:
冯吉才, 宋晓国, 刘多, 周利, 檀财旺, 陈波. 异种材料连接技术及其在复杂结构制造中的应用[J]. 金属学报, 2026, 62(5): 835-854.
Jicai FENG,
Xiaoguo SONG,
Duo LIU,
Li ZHOU,
Caiwang TAN,
Bo CHEN.
Joining Technology of Dissimilar Materials and Its Application in Complex Structure Manufacturing[J]. Acta Metall Sin, 2026, 62(5): 835-854.
| [1] |
Fu W. Research on the mechanism of wetting and low-temperature bonding of graphite and ceramics by Sn-Ti [D]. Harbin: Harbin Institute of Technology, 2019
|
| [1] |
付 伟. Sn-Ti对石墨和陶瓷的润湿及低温连接机理研究 [D]. 哈尔滨: 哈尔滨工业大学, 2019
|
| [2] |
Song X G, Zhao Y X, Hu S P, et al. Wetting of AgCu-Ti filler on porous Si3N4 ceramic and brazing of the ceramic to TiAl alloy [J]. Ceram. Int., 2018, 44: 4622
doi: 10.1016/j.ceramint.2017.11.212
|
| [3] |
Fu W, Song X G, Zhao Y X, et al. Effect of Ti content on the wetting behavior of Sn0.3Ag0.7Cu/AlN system [J]. Mater. Des., 2017, 115: 1
doi: 10.1016/j.matdes.2016.11.041
|
| [4] |
Sui R, Lin Q L. Wetting behavior of monocrystalline Si by SnAgCu-xTi alloys [J]. Trans. China Weld. Inst., 2020, 41(4): 90
|
| [4] |
隋 然, 林巧力. SnAgCu-xTi在单晶硅表面的润湿行为 [J]. 焊接学报, 2020, 41(4): 90
|
| [5] |
Li K, Zhang X Y, Lu Y J, et al. Influence of Nb on Co-based brazing filler metal [J]. Chin. J. Rare Met., 2013, 37: 744
|
| [5] |
李 锴, 张小勇, 陆艳杰 等. 金属Nb对Co基钎料焊接的影响 [J]. 稀有金属, 2013, 37: 744
|
| [6] |
Li C, Chen L, Si X Q, et al. Review of the research on the control of the residual stress in ceramic-metal joints [J]. J. Mech. Eng., 2024, 60(22): 21
|
| [6] |
李 淳, 陈 雷, 司晓庆 等. 陶瓷-金属接头残余应力调控研究综述 [J]. 机械工程学报, 2024, 60(22): 21
|
| [7] |
Wang N, Wang D P, Yang Z W, et al. Interfacial microstructure and mechanical properties of zirconia ceramic and niobium joints vacuum brazed with two Ag-based active filler metals [J]. Ceram. Int., 2016, 42: 12815
doi: 10.1016/j.ceramint.2016.05.045
|
| [8] |
Singh M, Fernandez J M, Asthana R, et al. Effect of Mo and W interlayers on microstructure and mechanical properties of Si3N4-nickel-base superalloy joints [J]. Int. J. Appl. Ceram. Technol., 2023, 20: 987
doi: 10.1111/ijac.v20.2
|
| [9] |
Qin Y Q, Feng J C. Active brazing carbon/carbon composite to TC4 with Cu and Mo composite interlayers [J]. Mater. Sci. Eng., 2009, A525: 181
|
| [10] |
Li X Y. GNPs reinforced composite filler alloy design & brazing process and mechansim of Cf/SiC-GH99 [D]. Harbin: Harbin Institute of Technology, 2021
|
| [10] |
李星仪. GNPs增强复合钎料设计及其钎焊Cf/SiC-GH99工艺和机理研究 [D]. 哈尔滨: 哈尔滨工业大学, 2021
|
| [11] |
Li M S, Li C, Si X Q, et al. Research Progress on diffusion bonding of dissimilar metal materials [J]. J. Harbin Inst. Technol., 2025, 57(12): 81
|
| [11] |
李鸣申, 李 淳, 司晓庆 等. 异种金属材料扩散连接研究进展[J]. 哈尔滨工业大学学报, 2025, 57(12): 81
|
| [12] |
Rao C J, Wan W C, Wang P, et al. Research status of ceramic/metal diffusion welding [J]. Trans. Mater. Heat Treat., 2023, 44(4): 13
|
| [12] |
饶程杰, 万维财, 王 鹏 等. 陶瓷/金属扩散焊研究现状 [J]. 材料热处理学报, 2023, 44(4): 13
doi: 10.13289/j.issn.1009-6264.2022-0458
|
| [13] |
Fang H Y, Feng J C. Interface Behavior During Material Joining [M]. Harbin: Harbin Institute of Technology Press, 2005: 125
|
| [13] |
方洪渊, 冯吉才. 材料连接过程中的界面行为 [M]. 哈尔滨: 哈尔滨工业大学出版社, 2005: 125
|
| [14] |
Shang J, Wang K H, Zhou Q, et al. Effec of joining temperature on microstructure and properties of diffusion bonded Mg/Al joints [J]. Trans. Nonferrous Met. Soc. China, 2012, 22: 1961
doi: 10.1016/S1003-6326(11)61414-3
|
| [15] |
Chen X, Xiao H, Shi Y M, et al. The influence of bonding time on microstructure and mechanical properties of vacuum diffusion bonded joints between commercial pure titanium and medium carbon steel [J]. Vacuum, 2023, 214: 112158
doi: 10.1016/j.vacuum.2023.112158
|
| [16] |
Zhou Z, Ding Y L, Sun Y, et al. Research progress on welding technology of Mg/Al dissimilar metal [J]. Weld. Join., 2024, (12): 33
|
| [16] |
周 正, 丁云龙, 孙 岩 等. 镁/铝异种金属焊接技术的研究进展 [J]. 焊接, 2024, (12): 33
|
| [17] |
Meng X C, Huang Y X, Cao J, et al. Recent progress on control strategies for inherent issues in friction stir welding [J]. Prog. Mater. Sci., 2021, 115: 100706
doi: 10.1016/j.pmatsci.2020.100706
|
| [18] |
Morisada Y, Imaizumi T, Fujii H. Clarification of material flow and defect formation during friction stir welding [J]. Sci. Technol. Weld. Join., 2015, 20: 130
doi: 10.1179/1362171814Y.0000000266
|
| [19] |
Gao S K, Zhou L, Zhang X M, et al. Microstructure and properties of friction stir welded joints for 6061-T6/7075-T6 dissimilar aluminum alloy [J]. Trans. China Weld. Inst., 2022, 43: 35
|
| [19] |
高士康, 周 利, 张欣盟 等. 6061-T6/7075-T6异种铝合金搅拌摩擦焊接头组织与性能 [J]. 焊接学报, 2022, 43: 35
doi: 10.12073/j.hjxb.20210616003
|
| [20] |
Ma L H, Xu Z Y, Zhang T, et al. In-situ formed amorphous phase in aluminum/steel friction stir welds: Interface evolution and strength improvement [J]. J. Adv. Join. Process., 2024, 9: 100220
|
| [21] |
Liu H J, Shen J J, Zhou L, et al. Microstructural characterisation and mechanical properties of friction stir welded joints of aluminium alloy to copper [J]. Sci. Technol. Weld. Join., 2011, 16: 92
doi: 10.1179/1362171810Y.0000000007
|
| [22] |
Huang Y B. The research of process and properties of magnesium alloys and steel friction stir welding [D]. Nanchang: Nanchang Hangkong University, 2013
|
| [22] |
黄勇兵. 镁/钢异种金属搅拌摩擦焊工艺及性能研究 [D]. 南昌: 南昌航空大学, 2013
|
| [23] |
Liu Y C, Wang X B, Zhou L, et al. Achievement of high-strength Al/CFRP hybrid joint via high-speed friction stir lap joining and laser texturing pretreatment parameters variation [J]. Thin Wall. Struct., 2024, 199: 111762
doi: 10.1016/j.tws.2024.111762
|
| [24] |
Li J Q, Liu H J. Characteristics of the reverse dual-rotation friction stir welding conducted on 2219-T6 aluminum alloy [J]. Mater. Des., 2013, 45: 148
doi: 10.1016/j.matdes.2012.08.068
|
| [25] |
Li J Q, Liu H J. Effects of tool rotation speed on microstructures and mechanical properties of AA2219-T6 welded by the external non-rotational shoulder assisted friction stir welding [J]. Mater. Des., 2013, 43: 299
doi: 10.1016/j.matdes.2012.07.011
|
| [26] |
Liu H J, Zhang H J, Yu L. Effect of welding speed on microstructures and mechanical properties of underwater friction stir welded 2219 aluminum alloy [J]. Mater. Des., 2011, 32: 1548
doi: 10.1016/j.matdes.2010.09.032
|
| [27] |
Chen J, Ueji R, Fujii H. Double-sided friction-stir welding of magnesium alloy with concave-convex tools for texture control [J]. Mater. Des., 2015, 76: 181
doi: 10.1016/j.matdes.2015.03.040
|
| [28] |
Kumar S, Wu C S, Padhy G K, et al. Application of ultrasonic vibrations in welding and metal processing: A status review [J]. J. Manuf. Process., 2017, 26: 295
doi: 10.1016/j.jmapro.2017.02.027
|
| [29] |
Huang R R. Research of interface behavior and strengthening mechanism of surface texture on Al/steel laser welding brazing joints [D]. Harbin: Harbin Institute of Technology, 2021
|
| [29] |
黄蓉蓉. 表面微结构调控铝/钢激光熔钎焊界面行为与强化机制研究 [D]. 哈尔滨: 哈尔滨工业大学, 2021
|
| [30] |
Guo S, Zhou Q, Peng Y, et al. Study on strengthening mechanism of Ti/Cu electron beam welding [J]. Mater. Des., 2017, 121: 51
doi: 10.1016/j.matdes.2017.02.054
|
| [31] |
Gatzen M, Radel T, Thomy C, et al. Wetting behavior of eutectic Al-Si droplets on zinc coated steel substrates [J]. J. Mater. Process. Technol., 2014, 214: 123
doi: 10.1016/j.jmatprotec.2013.08.005
|
| [32] |
Li H Y, Li L Q, Zhang Z S, et al. Dynamic spreading and interfacial reactions during the laser-induced wetting process of aluminum on stainless steel [J]. Appl. Surf. Sci., 2022, 587: 152869
doi: 10.1016/j.apsusc.2022.152869
|
| [33] |
Xu R Z, Li H, Hou Y X, et al. Influencing mechanism of Al-Zn coating addition on interfacial microstructure and mechanical property of vacuum electron beam welded Mg/steel joint [J]. Vacuum, 2018, 158: 31
doi: 10.1016/j.vacuum.2018.09.026
|
| [34] |
Fan D, Yang N, Huang J K, et al. Plasma arc welding-brazing of aluminum to copper with SiO2 nanoparticles strengthening [J]. J. Manuf. Process., 2021, 69: 253
doi: 10.1016/j.jmapro.2021.07.051
|
| [35] |
Sun YM, Li H Y, Huang R R, et al. Improved wettability of Al-Si5 on DP980 steel during laser-induced heating by surface texture preparation [J]. J. Manuf. Process., 2023, 89: 111
doi: 10.1016/j.jmapro.2023.01.066
|
| [36] |
Li H Y, Li L Q, Huang R R, et al. The effect of surface texturing on the laser-induced wetting behavior of AlSi5 alloy on Ti6Al4V alloy [J]. Appl. Surf. Sci., 2021, 566: 150630
doi: 10.1016/j.apsusc.2021.150630
|
| [37] |
Wang C M, Cui L Y, Mi G Y, et al. The influence of heat input on microstructure and mechanical properties for dissimilar welding of galvanized steel to 6061 aluminum alloy in a zero-gap lap joint configuration [J]. J. Alloys Compd., 2017, 726: 556
doi: 10.1016/j.jallcom.2017.08.015
|
| [38] |
Kaisheva D, Kotlarski G, Ormanova M, et al. Effect of beam power on intermetallic compound formation of electron beam-welded Cu and Al6082-T6 dissimilar joints [J]. Eng, 2025, 6: 6
|
| [39] |
Huang J K, Liu Y L, Liu S E, et al. Process of welding-brazing and interface analysis of lap joint Ti-6Al-4V and aluminum by plasma arc welding [J]. J. Manuf. Process., 2021, 61: 396
doi: 10.1016/j.jmapro.2020.11.017
|
| [40] |
Fan D, Li Y P, Wu L J, et al. Effect of ultrasonic vibration on microstructure and mechanical properties of welding-brazing joint between aluminum and copper by plasma welding [J]. Mater. Rep., 2021, 35: 16115
|
| [40] |
樊 丁, 李永鹏, 武利建 等. 超声振动对铝/铜等离子弧熔钎焊接头组织及力学性能的影响 [J]. 材料导报, 2021, 35: 16115
|
| [41] |
Rong Y, Li H T, Xiong Z Y, et al. Microstructure and forming control of laser welding-brazing joint of magnesium alloy and steel dissimilar materials [J]. J. Mater. Eng., 2022, 50(5): 166
doi: 10.11868/j.issn.1001-4381.2021.000635
|
| [41] |
戎 易, 李海涛, 熊震宇 等. 镁合金/钢异种材料激光熔钎焊接头组织及成形调控 [J]. 材料工程, 2022, 50(5): 166
|
| [42] |
Wen Z L, Yu G Y, Li S Q, et al. Influence of Ni/Zn double coating on the steel on penetration welding-brazing by CMT arc-laser hybrid heat source [J]. Opt. Laser Technol., 2021, 134: 106602
doi: 10.1016/j.optlastec.2020.106602
|
| [43] |
Xia H B, Yang B Y, Han Y D, et al. Toward understanding the fractured mechanism in laser welded-brazed Al/steel interface by in-situ SEM tensile observations [J]. J. Mater. Process. Technol., 2024, 325: 118294
doi: 10.1016/j.jmatprotec.2024.118294
|
| [44] |
Tan Z, Liu J S, Zhou D W, et al. Laser heat-conduction welding and numerical simulation of double phase steel/magnesium alloy with Sn foil [J]. Chin. J. Nonferrous Met., 2016, 26: 1427
|
| [44] |
谭 哲, 刘金水, 周惦武 等. 双相钢/镁合金添加Sn箔激光热传导焊及数值模拟 [J]. 中国有色金属学报, 2016, 26: 1427
|
| [45] |
Wang T, Zhang B G, Chen G Q, et al. High strength electron beam welded titanium-stainless steel joint with V/Cu based composite filler metals [J]. Vacuum, 2013, 94: 41
doi: 10.1016/j.vacuum.2013.01.015
|
| [46] |
Wang T, Zhang B G, Wang H Q, et al. Microstructures and mechanical properties of electron beam-welded titanium-steel joints with vanadium, nickel, copper and silver filler metals [J]. J. Mater. Eng. Perform., 2014, 23: 1498
doi: 10.1007/s11665-014-0897-8
|
| [47] |
Wu D. Study on microstructures and properties of plasma arc welded joints of aluminum alloy/high-strength steel dissimilar materials [D]. Changchun: Jilin University, 2023
|
| [47] |
吴 迪. 铝合金/高强钢异种材料等离子弧焊接头微观组织及力学性能的研究 [D]. 长春: 吉林大学, 2023
|
| [48] |
Li Z Y. Research on laser welded-brazed joint strengthening of aluminum/steel dissimilar metals based on surface microstructure and preset AlSi12 interlayer [D]. Guilin: Guilin University of Electronic Technology, 2022
|
| [48] |
李兆艳. 基于表面微结构和预置AlSi12中间层调控的铝/钢异种金属激光熔钎焊接头强化研究 [D]. 桂林: 桂林电子科技大学, 2022
|
| [49] |
Li H Y, Xia H B, Li L Q, et al. Enhancing the reliability of laser welded-brazed aluminum/stainless steel joints via laser-chemical hybrid surface texturing [J]. Thin Walled Struct., 2024, 199: 111780
doi: 10.1016/j.tws.2024.111780
|
| [50] |
Zhang X Y, Feng Z W, Su J H, et al. Achieving the thermal reinforcement between aluminum sensing elements and composites in induction welding via silane layers [J]. Composites, 2025, 306B: 112782
|
| [51] |
Tan C W, Su J H, Liu Y F, et al. Enhanced interfacial bonding strength of laser bonded titanium alloy/CFRTP joint via hydrogen bonds interaction [J]. Composites, 2022, 239B: 109966
|
| [52] |
Xia H B. Research on interfacial fractureing behaviors and adjusted method of IMC layer for the laser welded-brazed Al/steel [D]. Harbin: Harbin Institute of Technology, 2019
|
| [52] |
夏鸿博. 铝/钢激光熔-钎焊的界面断裂行为及IMC层调控方法研究 [D]. 哈尔滨: 哈尔滨工业大学, 2019
|
| [53] |
Yang B Y. Study on the fracture behavior and homogenization regulation of aluminum/steel laser fusion brazing interface [D]. Yangzhou: Yangzhou University, 2024
|
| [53] |
杨柏云. 铝/钢激光熔钎焊界面断裂行为及均质化调控研究 [D]. 扬州: 扬州大学, 2024
|
| [54] |
Cheng N, Yang S L, Li Y L, et al. Analysis of fatigue fracture mechanism of laser spiral welding of dissimilar metals of 6082 high strength aluminum alloy and DP980 high strength dual phase steel [J]. Mater. Today Commun., 2024, 41: 110665
|
| [55] |
Liu Y Q, Zhu Z T, Che X L, et al. Fatigue properties and fracture behavior of Al/steel butt joints fabricated by laser‐MIG welding‐brazing [J]. Fatigue Fract. Eng. Mater. Struct., 2022, 45: 2187
doi: 10.1111/ffe.v45.8
|
| [56] |
Narsimhachary D, Lavakumar A, Katiyar P K, et al. Effect of wire deposition rate on macro and microscopic characteristics of laser weld-brazed AA5083 aluminum alloy to galvanized steel joints and their corrosion response [J]. Adv. Mater. Process. Technol., 2025, 11: 1851
|
| [57] |
Karayel E, Bozkurt Y. Additive manufacturing method and different welding applications [J]. J. Mater. Res. Technol., 2020, 9: 11424
doi: 10.1016/j.jmrt.2020.08.039
|
| [58] |
Carlone P, Astarita A. Dissimilar metal welding [J]. Metals, 2019, 9: 1206
doi: 10.3390/met9111206
|
| [59] |
Andreiev A, Hoyer K P, Dula D, et al. Laser beam melting of functionally graded materials with application-adapted tailoring of magnetic and mechanical performance [J]. Mater. Sci. Eng., 2021, A822: 141662
|
| [60] |
Heer B, Bandyopadhyay A. Compositionally graded magnetic-nonmagnetic bimetallic structure using laser engineered net shaping [J]. Mater. Lett., 2018, 216: 16
doi: 10.1016/j.matlet.2017.12.129
|
| [61] |
Yan L, Chen Y T, Liou F. Additive manufacturing of functionally graded metallic materials using laser metal deposition [J]. Addit. Manuf., 2020, 31: 100901
|
| [62] |
Narayanaswamy S, Telasang G, Park N, et al. Additive manufacturing of SS316L-IN718 superalloy Bi-metallic structure: Interfacial microstructure and mechanical properties [J]. Prog. Addit. Manuf., 2025, 10: 7173
doi: 10.1007/s40964-025-01036-1
|
| [63] |
Karnati S, Sparks T E, Liou F W, et al. Laser metal deposition of functionally gradient materials from elemental copper and nickel powders [A]. Proceedings of the 26th Annual International Solid Freeform Fabrication Symposium [C]. Austin: University of Texas at Austin, 2015: 789
|
| [64] |
Onuike B, Bandyopadhyay A. Additive manufacturing of Inconel 718-Ti6Al4V bimetallic structures [J]. Addit. Manuf., 2018, 22: 844
|
| [65] |
Zhang X C, Li L, Liou F. Additive manufacturing of stainless steel-copper functionally graded materials via Inconel 718 interlayer [J]. J. Mater. Res. Technol., 2021, 15: 2045
doi: 10.1016/j.jmrt.2021.09.027
|
| [66] |
Schneider-Maunoury C, Weiss L, Acquier P, et al. Functionally graded Ti6Al4V-Mo alloy manufactured with DED-CLAD® process [J]. Addit. Manuf., 2017, 17: 55
|
| [67] |
Su Y, Chen B, Tan C W, et al. Influence of composition gradient variation on the microstructure and mechanical properties of 316 L/Inconel718 functionally graded material fabricated by laser additive manufacturing [J]. J. Mater. Process. Technol., 2020, 283: 116702
doi: 10.1016/j.jmatprotec.2020.116702
|
| [68] |
Song Y Y. Process and mechanism of nanosecond laser surface modification assisted brazing Si3N4 ceramic and Cu [D]. Harbin: Harbin Institute of Technology, 2022
|
| [68] |
宋延宇. Si3N4陶瓷与紫铜的纳秒激光表面改性辅助钎焊工艺及机理研究 [D]. 哈尔滨: 哈尔滨工业大学, 2022
|
| [69] |
Liu Y Z, Hu S P, Song Y G, et al. Multi-scale modeling for prediction of mechanical performance in brazed GH99 thin-walled structure [J]. Chin. J. Aeronaut., 2024, 37: 550
doi: 10.1016/j.cja.2024.01.010
|
| [70] |
HillA, WallachE. R.. Modelling solid-state diffusion bonding [J]. Acta Metall., 1989, 37: 2425
doi: 10.1016/0001-6160(89)90040-0
|
| [71] |
MishraR S, MaZ Y. Friction stir welding and processing [J]. Mater. Sci. Eng., 2005, R50(1-2): 1
|
| [72] |
Liu F C, Zhang Y N, Dong P S. Large area friction stir additive manufacturing of intermetallic-free aluminum-steel bimetallic components through interfacial amorphization [J]. J. Manuf. Process., 2022, 73: 725
doi: 10.1016/j.jmapro.2021.11.042
|
| [73] |
Liu F C, Dong P. From thick intermetallic to nanoscale amorphous phase at Al-Fe joint interface: Roles of friction stir welding conditions [J]. Scr. Mater., 2021, 191: 167
doi: 10.1016/j.scriptamat.2020.09.031
|
| [74] |
Yu M R, Nan X C, Zhou L, et al. Ultrasonic-induced amorphization and strengthening mechanisms of ultrasonic vibrations assisted friction stir Al/Ti welds [J]. Mater. Des., 2024, 246: 113313
doi: 10.1016/j.matdes.2024.113313
|
| [75] |
Li J H, Dai Y, Cui Y Y, et al. Atomistic theory for predicting the binary metallic glass formation [J]. Mater. Sci. Eng., 2011, R72: 1
|
| [76] |
Takeuchi A, Inoue A. Classification of bulk metallic glasses by atomic size difference, heat of mixing and period of constituent elements and its application to characterization of the main alloying element [J]. Mater. Trans., 2005, 46: 2817
doi: 10.2320/matertrans.46.2817
|
| [77] |
Baqer Y M, Ramesh S, Yusof F, et al. Challenges and advances in laser welding of dissimilar light alloys: Al/Mg, Al/Ti, and Mg/Ti alloys [J]. Int. J. Adv. Manuf. Technol., 2018, 95: 4353
doi: 10.1007/s00170-017-1565-6
|
| [78] |
Jadav H, Badheka V, Upadhyay G, et al. Dissimilar welding of magnesium alloy to aluminium alloy: A review [J]. Adv. Mater. Process. Technol., 2022, 8: 3794
|
| [79] |
Shen Y, Perepezko J H. Al-based amorphous alloys: Glass-forming ability, crystallization behavior and effects of minor alloying additions [J]. J. Alloys Compd., 2017, 707: 3
doi: 10.1016/j.jallcom.2016.11.079
|
| [80] |
Campanelli S L, Casalino G, Casavola C, et al. Analysis and comparison of friction stir welding and laser assisted friction stir welding of aluminum alloy [J]. Materials, 2013, 6: 5923
doi: 10.3390/ma6125923
pmid: 28788430
|
| [81] |
Zhu S H, Zhu X X, Lv W Y, et al. The influence of laser-induced tempering on the microstructure and mechanical properties of 1500 MPa martensitic steel friction stir welded joints [J]. Opt. Laser Technol., 2025, 182: 112094
doi: 10.1016/j.optlastec.2024.112094
|
| [82] |
Sun Y F, Konishi Y, Kamai M, et al. Microstructure and mechanical properties of S45C steel prepared by laser-assisted friction stir welding [J]. Mater. Des., 2013, 47: 842
doi: 10.1016/j.matdes.2012.12.078
|
| [83] |
Mohan D G, Wu C S. A review on friction stir welding of steels [J]. Chin. J. Mech. Eng., 2021, 34: 137
doi: 10.1186/s10033-021-00655-3
|
| [84] |
Chen X Y, Chen S J, Liu Z H, et al. Magnetic field-assisted ultra-high-speed friction stir welding [J]. Mater. Lett., 2023, 331: 133447
doi: 10.1016/j.matlet.2022.133447
|
| [85] |
Chen X Y, Lu Z P, Chen S J, et al. A novel method for improving the plastic flow and mechanical properties of spray-formed 7055-T76 (Sc-added) aluminum alloy FSW joint by rotating magnetic field [J]. J. Alloy. Compd., 2025, 1010: 178219
doi: 10.1016/j.jallcom.2024.178219
|
| [86] |
DebRoy T, Wei H L, Zuback J S, et al. Additive manufacturing of metallic components—Process, structure and properties [J]. Prog. Mater Sci., 2018, 92: 112
doi: 10.1016/j.pmatsci.2017.10.001
|
| [87] |
Svetlizky D, Das M, Tofail S A M, et al. Directed energy deposition of functionally graded materials: A review[J]. J. Mater. Sci., 2021, 56: 18290
|
| [88] |
Li P X, Yan Y T, Ba J, et al. The regulation strategy for releasing residual stress in ceramic-metal brazed joints [J]. J. Manuf. Processes, 2023, 85: 935
doi: 10.1016/j.jmapro.2022.12.022
|
| [89] |
Jiang H, Li C, Mao X J, et al. Analysis of microstructure and residual stress in brazing ZrO2 ceramic and 441 stainless steel [J]. Mater. Charact., 2025, 225:
|
| [90] |
Yu H Y, Hu Z L. Interface microstructure and mechanical properties of dissimilar metal friction stir lap welding of DP590 steel and 7075 aluminum [J]. J. Mech. Eng., 2020, 56(6): 8
doi: 10.3901/JME.2020.22.008
|
| [90] |
于海洋, 胡志力. Dp590钢/7075铝异种金属搅拌摩擦搭接焊界面组织与力学性能研究[J]. 机械工程学报, 2020, 56(6); 8
|
| [91] |
Zapata J, Toro M, LópezD. Residual stresses in friction stir dissimilar welding of aluminum alloys [J]. J. Mater. Process. Technol., 2016, 229: 121
doi: 10.1016/j.jmatprotec.2015.08.026
|
| [92] |
Komerla K, Gach S, Akyel F, et al. Finite element simulation of residual stress induced by high energy beam welding in dual phase steel [J]. Lasers Manuf. Mater. Process., 2020, 7: 154
doi: 10.1007/s40516-020-00112-4
|
| [93] |
Liao W H, Dai N. Development and challenge of lightweight design and manufacturing technology for aerospace structures [J]. J. Nanjing Univ. Aeronaut. Astronaut., 2023, 55: 347
|
| [93] |
廖文和, 戴 宁. 航空航天结构轻量化设计制造技术发展现状与挑战 [J]. 南京航空航天大学学报, 2023, 55: 347
|
| [94] |
Schreiber F, Lippok T, Bätzel J U, et al. Applicability of snap joint design guidelines for additive manufacturing [A]. Proceedings of the 8th Changeable, Agile, Reconfigurable and Virtual Production Conference (CARV2021) and the 10th World Mass Customization & Personalization Conference [C]. Aalborg: Springer, 2022: 277
|
| [95] |
Cheng F, Zheng C G, Liu Y F, et al. Lightweight design of CFRP-laminated structures by combining microscopical homogenization and macroscopical optimization [J]. Int. J. Automot. Technol., 2021, 22: 1427
doi: 10.1007/s12239-021-0124-1
|
| [96] |
Li H Y, Liu Y J, Zhao Z X, et al. Interface microstructure and formation mechanism of oscillating laser brazed joints for aerial sensing element [J]. Acta Aeronaut. Astronaut. Sin., 2022, 43: 625020
|
| [96] |
李昊岳, 刘永江, 赵振兴 等. 航空传感元件振镜激光钎焊界面组织及连接机理 [J]. 航空学报, 2022, 43: 625020
doi: 10.7527/S1000-6893.2020.25020
|
| [97] |
Yang L J, Zou J J, Qi X J, et al. Research and application on welding technology of stainless steel and aluminum alloy dissimilar materials [J]. Hot Work. Technol., 2024, 53(15): 27
|
| [97] |
杨林杰, 邹建军, 祁小娟 等. 异种材料不锈钢和铝合金焊接技术研究及应用 [J]. 热加工工艺, 2024, 53(15): 27
|
| [98] |
Luo Y. Research on brazing process and mechanical properties of TiAl/GH3536 heterogeneous honeycomb sandwich structure [D]. Harbin: Harbin Institute of Technology, 2023
|
| [98] |
罗 云. TiAl/GH3536异质蜂窝夹层结构钎焊工艺及力学性能研究 [D]. 哈尔滨: 哈尔滨工业大学, 2023
|
| [99] |
Yao X J, Zhu Y Y, Han X, et al. Preparation of copper/nickel dissimilar metals by laser additive manufacturing based on copper alloy surface pretreatment [J]. Chin. J. Lasers, 2025, 52: 0402301
|
| [99] |
姚讯杰, 朱言言, 韩 曦 等. 基于铜合金表面预处理的激光增材制造铜/镍异种金属制备研究 [J]. 中国激光, 2025, 52: 0402301
|
| [100] |
Long W M, Qiao R L, Qin J, et al. Research progress in dissimilar material brazing technology and applications [J]. Trans. China Weld. Inst., 2025, 46(4): 1
|
| [100] |
龙伟民, 乔瑞林, 秦 建 等. 异质材料钎焊技术与应用研究进展 [J]. 焊接学报, 2025, 46(4): 1
|
| [101] |
Wang J Z. Study on mechanism and double pass process of friction stir welding for 6061-T6 Al/ZK61M Mg heterogeneous materials [D]. Dalian: Dalian Jiaotong University, 2025
|
| [101] |
王建洲. 6061-T6 Al/ZK61M Mg异材搅拌摩擦焊机理及双道次工艺研究 [D]. 大连: 大连交通大学, 2025
|
| [102] |
Boldsaikhan E, Fukada S, Fujimoto M, et al. Refill friction stir spot welding of surface-treated aerospace aluminum alloys with faying-surface sealant [J]. J. Manuf. Process., 2019, 42: 113
doi: 10.1016/j.jmapro.2019.04.027
|
| [103] |
Ahmed M M Z, El-Sayed Seleman M M, Fydrych D, et al. Friction stir welding of aluminum in the aerospace industry: The current progress and state-of-the-art review [J]. Materials, 2023, 16: 2971
doi: 10.3390/ma16082971
|
| [104] |
Xue S B, Zhang L, Gao L L, et al. Welding technology of aircraft manufacturing [J]. Aeronaut. Manuf. Technol., 2009, (19): 26
|
| [104] |
薛松柏, 张 亮, 皋利利 等. 航空器制造中的焊接技术 [J]. 航空制造技术, 2009, (19): 26
|
| [105] |
Gao Y, Morisada Y, Fujii H, et al. Friction stir lap welding of plastic to metal using adjustable tool [J]. Sci. Technol. Weld. Join., 2020, 25: 190
doi: 10.1080/13621718.2019.1665858
|
| [106] |
Joudaki J, Safari M, Joodaki M. Experimental investigation of friction stir spot welding of polymer-aluminum alloy weldments [J]. Proc. Inst. Mech. Eng., 2022, 236B: 1368
|
| [107] |
Xiao S N, Jiang L X, Jiang W, et al. Application and prospect of composite materials in rail transit vehicles [J]. J. Traffic Transp. Eng., 2021, 21(1): 23
|
| [107] |
肖守讷, 江兰馨, 蒋 维 等. 复合材料在轨道交通车辆中的应用与展望 [J]. 交通运输工程学报, 2021, 21(1): 23
|
| [108] |
Kong D Q. New progress in laser welding technology for Al/Cu dissimilar metals in automotive battery modules [J]. Met. Work. (Met. Cutt.), 2020, (S1): 153
|
| [108] |
孔德群. 汽车电池模组件Al/Cu异种金属激光焊接技术新进展 [J]. 金属加工(冷加工), 2020, (S1): 153
|
| [109] |
Wang G W. Research on lightweight design of composite battery pack for electric vehicle [D]. Changchun: Jilin University, 2020
|
| [109] |
王国旺. 复合材料电动汽车电池包轻量化设计研究 [D]. 长春: 吉林大学, 2020
|
| [110] |
Li H, Liao X L, Zeng Z, et al. Thermal coupling analysis in a multichip paralleled IGBT module for a DFIG wind turbine power converter [J]. IEEE Trans. Energy Convers., 2017, 32: 80
|
| [111] |
Entezarian M, Drew R A L. Direct bonding of copper to aluminum nitride [J]. Mater. Sci. Eng., 1996, A212: 206
|
| [112] |
Zhang M C, Xin C L, Li D Y. Research progress in metallization of ceramic substrate [J]. J. Chengdu Univ. (Nat. Sci.), 2023, 42: 392
|
| [112] |
张明昌, 辛成来, 李东亚. 陶瓷基板金属化制备技术的研究进展 [J]. 成都大学学报(自然科学版), 2023, 42: 392
|
| [113] |
Huang D, Liu Z, Harris J, alat. High thermal conductive AlN substrate for heat dissipation in high-power LEDs [J]. Ceram. Int., 2019, 45: 1412
doi: 10.1016/j.ceramint.2018.09.171
|
| [114] |
Wang H X. Active alloy brazing Al2O3 ceraics and metal [D]. Dalian: Dalian Jiaotong University, 2006
|
| [114] |
王洪潇. 氧化铝陶瓷与金属活性封接技术研究 [D]. 大连: 大连交通大学, 2006
|
| [115] |
Xu H F, Wang J, Fan F S, et al. The influence of Ti content in AgCuTi filler on its wetting and spreading mechanism on silicon nitride ceramics: An experiment and first-principles calculation study [J]. Mater. Today Commun., 2024, 41: 110833
|
| [116] |
Hofmann D C, Kolodziejska J, Roberts S, et al. Compositionally graded metals: A new frontier of additive manufacturing [J]. J. Mater. Res., 2014, 29: 1899
doi: 10.1557/jmr.2014.208
|
| [117] |
Chandrasekaran S, Hari S, Amirthalingam M. Functionally graded materials for marine risers by additive manufacturing for high-temperature applications: Experimental investigations [J]. Structures, 2022, 35: 931
doi: 10.1016/j.istruc.2021.12.004
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|