Please wait a minute...
金属学报  2026, Vol. 62 Issue (5): 785-802    DOI: 10.11900/0412.1961.2025.00289
  综述 本期目录 | 过刊浏览 |
矩张量机器学习势模型的发展与应用
陈星秋1(), 王建韬1,2, 刘培涛1()
1 中国科学院金属研究所 沈阳材料科学国家研究中心 沈阳 110016
2 中国科学技术大学 材料科学与工程学院 沈阳 110016
Moment Tensor Machine-Learning Potential: Development and Applications
CHEN Xing-Qiu1(), WANG Jiantao1,2, LIU Peitao1()
1 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
2 School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China
引用本文:

陈星秋, 王建韬, 刘培涛. 矩张量机器学习势模型的发展与应用[J]. 金属学报, 2026, 62(5): 785-802.
Xing-Qiu CHEN, Jiantao WANG, Peitao LIU. Moment Tensor Machine-Learning Potential: Development and Applications[J]. Acta Metall Sin, 2026, 62(5): 785-802.

全文: PDF(3459 KB)   HTML
摘要: 

近年来,基于人工智能的材料计算模拟技术快速发展,机器学习的原子间相互作用势函数是其中最为重要的分支之一。机器学习势函数通过机器学习算法对第一性原理计算数据进行高精度拟合,将其转化为连续可微的数学表达,使其在保持量子力学计算精度的同时显著降低计算成本,有效解决了第一性原理方法难以处理大体系和长时间模拟的瓶颈问题。凭借这一独特优势,机器学习势函数已成为衔接微观原子模拟与宏观材料性能预测的关键桥梁,为材料计算领域带来了革命性机遇。本文聚焦于兼顾精度和效率的矩张量势(MTP)模型,从理论框架、算法优化和应用实践三个层面进行系统评述:深入解析了MTP的数学基础和架构设计原理;详细讨论了其精度提升策略和计算加速技术;通过典型材料体系的模拟案例验证了模型的优越性能,并对其发展趋势进行了展望。

关键词 : 原子间相互作用势,  机器学习,  矩张量,  原子模拟    
Abstract:

In recent years, artificial intelligence-based computational materials modeling has advanced rapidly, with machine learning potentials (MLPs) emerging as a central research direction. By fitting ab initio reference data into continuous and differentiable functional forms, MLPs retain near-quantum-mechanical accuracy while substantially reducing computational cost. This capability alleviates the limitations of ab initio methods in simulations of large-scale systems and long timescales. Consequently, MLPs serve as a critical link between atomistic simulations and macroscopic material property predictions, enabling new possibilities in computational materials science. This review focuses on the moment tensor potential (MTP), which offers an excellent balance between accuracy and computational efficiency. This paper provides a systematic overview from three perspectives: theoretical framework, algorithmic optimization, and practical applications. First, the mathematical foundations and design principles of MTP are analyzed. Next, strategies for improving accuracy and accelerating computation are discussed. Finally, representative case studies on typical material systems are presented to demonstrate the performance of MTP, and future development directions are outlined.

Key words: interatomic potential    machine learning    moment tensor    atomistic simulation
收稿日期: 2025-09-28     
ZTFLH:  O469  
基金资助:国家自然科学基金项目(52422112);国家自然科学基金项目(52188101);新材料重大专项项目(2025ZD0618901);中国科学院战略性先导科技专项项目(XDA041040402);辽宁省重大专项项目(2024JH1/11700032)
通讯作者: 陈星秋,xingqiu.chen@imr.ac.cn,主要从事合金计算和智能设计研究; 刘培涛,ptliu@imr.ac.cn,主要从事材料电子结构计算和原子模拟研究
Corresponding author: CHEN Xing-Qiu, professor, Tel: 15002491386, E-mail: xingqiu.chen@imr.ac.cn; LIU Peitao, professor, Tel: 17696608803, E-mail: ptliu@imr.ac.cn
作者简介: 陈星秋,男,1975年生,研究员,博士
图1  机器学习力场构建流程
图2  典型的机器学习势函数发展过程
图3  各种势函数模型的计算精度和效率评估[60]
图4  标量基组Bα及Bβ分解路径示意[66]
图5  结合主动学习采样方法的矩张量势(MTP)模型开发流程
图6  MTP模型在QM9数据集上的主动学习与随机选择策略的效率和性能比较[64]
图7  MTP模型在Ni-Al合金体系中的应用[66,96,97]
图8  MTP模型在高熵合金体系中的应用[103~105]
图9  MTP模型在固-固相变中的应用[111~113]
图10  MTP模型在表面及界面体系中的应用[121,122,125]
[1] Agrawal A, Choudhary A. Perspective: Materials informatics and big data: Realization of the “fourth paradigm” of science in materials science [J]. APL Mater., 2016, 4: 053208
[2] Meyer M, Pontikis V. Computer Simulation in Materials Science [M]. Dordrecht: Springer, 1991, 205: 3
[3] Hafner J. Atomic-scale computational materials science [J]. Acta Mater., 2000, 48: 71
doi: 10.1016/S1359-6454(99)00288-8
[4] Steinhauser M O, Hiermaier S. A review of computational methods in materials science: Examples from shock-wave and polymer physics [J]. Int. J. Mol. Sci., 2009, 10: 5135
doi: 10.3390/ijms10125135 pmid: 20054467
[5] Daw M S, Baskes M I. Embedded-atom method: Derivation and application to impurities, surfaces, and other defects in metals [J]. Phys. Rev., 1984, 29B: 6443
[6] Finnis M W, Sinclair J E. A simple empirical N-body potential for transition metals [J]. Philos. Mag., 1984, 50A: 45
[7] Baskes M I. Modified embedded-atom potentials for cubic materials and impurities [J]. Phys. Rev., 1992, 46B: 2727
[8] Tersoff J. New empirical approach for the structure and energy of covalent systems [J]. Phys. Rev., 1988, 37B: 6991
[9] Blank T B, Brown S D, Calhoun A W, et al. Neural network models of potential energy surfaces [J]. J. Chem. Phys., 1995, 103: 4129
[10] Brown D F R, Gibbs M N, Clary D C. Combining ab initio computations, neural networks, and diffusion Monte Carlo: An efficient method to treat weakly bound molecules [J]. J. Chem. Phys., 1996, 105: 7597
doi: 10.1063/1.472596
[11] Gassner H, Probst M, Lauenstein A, et al. Representation of intermolecular potential functions by neural networks [J]. J. Phys. Chem., 1998, 102A: 4596
[12] Prudente F V, Acioli P H, Neto J J S. The fitting of potential energy surfaces using neural networks: Application to the study of vibrational levels of H 3 + [J]. J. Chem. Phys., 1998, 109: 8801
doi: 10.1063/1.477550
[13] Huang X C, Braams B J, Bowman J M. Ab initio potential energy and dipole moment surfaces for H 5 O 2 + [J]. J. Chem. Phys., 2005, 122: 044308
[14] Manzhos S, Carrington T. Using neural networks to represent potential surfaces as sums of products [J]. J. Chem. Phys., 2006, 125: 194105
doi: 10.1063/1.2387950
[15] Behler J, Parrinello M. Generalized neural-network representation of high-dimensional potential-energy surfaces [J]. Phys. Rev. Lett., 2007, 98: 146401
doi: 10.1103/PhysRevLett.98.146401
[16] Bartók A P, Payne M C, Kondor R, et al. Gaussian approximation potentials: The accuracy of quantum mechanics, without the electrons [J]. Phys. Rev. Lett., 2010, 104: 136403
doi: 10.1103/PhysRevLett.104.136403
[17] Bartόk A P. The gaussian approximation potential: An interatomic potential derived from first principles quantum mechanics [D]. Berlin, Heidelberg: Springer, 2010
[18] Bartók A P, Kondor R, Csányi G. On representing chemical environments [J]. Phys. Rev., 2013, 87B: 184115
[19] Jinnouchi R, Karsai F, Kresse G. On-the-fly machine learning force field generation: Application to melting points [J]. Phys. Rev., 2019, 100B: 014105
[20] Jinnouchi R, Lahnsteiner J, Karsai F, et al. Phase transitions of hybrid perovskites simulated by machine-learning force fields trained on the fly with Bayesian inference [J]. Phys. Rev. Lett., 2019, 122: 225701
doi: 10.1103/PhysRevLett.122.225701
[21] Shapeev A V. Moment tensor potentials: A class of systematically improvable interatomic potentials [J]. Multiscale Model. Simul., 2016, 14: 1153
doi: 10.1137/15M1054183
[22] Thompson A P, Swiler L P, Trott C R, et al. Spectral neighbor analysis method for automated generation of quantum-accurate interatomic potentials [J]. J. Comput. Phys., 2015, 285: 316
[23] Wood M A, Thompson A P. Extending the accuracy of the SNAP interatomic potential form [J]. J. Chem. Phys., 2018, 148: 241721
doi: 10.1063/1.5017641
[24] Drautz R. Atomic cluster expansion for accurate and transferable interatomic potentials [J]. Phys. Rev., 2019, 99B: 014104
[25] Huang S D, Shang C, Kang P L, et al. LASP: Fast global potential energy surface exploration [J]. WIREs Comput. Mol. Sci., 2019, 9: e1415
doi: 10.1002/wcms.1415
[26] Kang P L, Shang C, Liu Z P. Recent implementations in LASP 3.0: Global neural network potential with multiple elements and better long-range description [J]. Chin. J. Chem. Phys., 2021, 34: 583
doi: 10.1063/1674-0068/cjcp2108145
[27] Kang P L, Shang C, Liu Z P. Glucose to 5-hydroxymethylfurfural: Origin of site-selectivity resolved by machine learning based reaction sampling [J]. J. Am. Chem. Soc., 2019, 141: 20525
doi: 10.1021/jacs.9b11535
[28] Ma S C, Huang S D, Liu Z P. Dynamic coordination of cations and catalytic selectivity on zinc-chromium oxide alloys during syngas conversion [J]. Nat. Catal., 2019, 2: 671
doi: 10.1038/s41929-019-0293-8
[29] Huang S D, Shang C, Kang P L, et al. Atomic structure of boron resolved using machine learning and global sampling [J]. Chem. Sci., 2018, 9: 8644
doi: 10.1039/C8SC03427C
[30] Huang S D, Shang C, Zhang X J, et al. Material discovery by combining stochastic surface walking global optimization with a neural network [J]. Chem. Sci., 2017, 8: 6327
doi: 10.1039/C7SC01459G
[31] Eckhoff M, Behler J. High-dimensional neural network potentials for magnetic systems using spin-dependent atom-centered symmetry functions [J]. npj Comput. Mater., 2021, 7: 170
doi: 10.1038/s41524-021-00636-z
[32] Behler J. Four generations of high-dimensional neural network potentials [J]. Chem. Rev., 2021, 121: 10037
doi: 10.1021/acs.chemrev.0c00868 pmid: 33779150
[33] Ko T W, Finkler J A, Goedecker S, et al. A fourth-generation high-dimensional neural network potential with accurate electrostatics including non-local charge transfer [J]. Nat. Commun., 2021, 12: 398
doi: 10.1038/s41467-020-20427-2 pmid: 33452239
[34] Han J Q, Zhang L F, Car R, et al. Deep potential: A general representation of a many-body potential energy surface [J]. Commun. Comput. Phys., 2018, 23: 629
doi: 10.4208/cicp
[35] Wang H, Zhang L F, Han J Q, et al. DeePMD-kit: A deep learning package for many-body potential energy representation and molecular dynamics [J]. Comput. Phys. Commun., 2018, 228: 178
doi: 10.1016/j.cpc.2018.03.016
[36] Chen M Y, Hu J W, Yu Y C, et al. Advances in machine learning molecular dynamics to assist materials nucleation and solidification research [J]. Acta Metall. Sin., 2024, 60: 1329
doi: 10.11900/0412.1961.2024.00192
[36] 陈名毅, 胡俊伟, 余耀辰 等. 机器学习分子动力学辅助材料凝固形核研究进展 [J]. 金属学报, 2024, 60: 1329
doi: 10.11900/0412.1961.2024.00192
[37] Liu S, Huang J W, Wu J. Application of machine learning force fields for modeling ferroelectric materials [J]. Acta Metall. Sin., 2024, 60: 1312
doi: 10.11900/0412.1961.2024.00177
[37] 刘 仕, 黄佳玮, 武 静. 机器学习势在铁电材料研究中的应用 [J]. 金属学报, 2024, 60: 1312
[38] Wen T Q, Zhang L F, Wang H, et al. Deep potentials for materials science [J]. Mater. Futures, 2022, 1: 022601
[39] Gilmer J, Schoenholz S S, Riley P F, et al. Neural message passing for quantum chemistry [A]. Proceedings of the 34th International Conference on Machine Learning [C]. Sydney: PMLR, 2017
[40] Schütt K T, Sauceda H E, Kindermans P J, et al. SchNet—A deep learning architecture for molecules and materials [J]. J. Chem. Phys., 2018, 148: 241722
doi: 10.1063/1.5019779
[41] Unke O T, Meuwly M. PhysNet: A neural network for predicting energies, forces, dipole moments, and partial charges [J]. J. Chem. Theory Comput., 2019, 15: 3678
doi: 10.1021/acs.jctc.9b00181 pmid: 31042390
[42] Klicpera J, Groß J, Günnemann S. Directional message passing for molecular graphs [A]. Proceedings of the 8th International Conference on Learning Representations [C]. Addis Ababa: OpenReview.net, 2020
[43] Schütt K T, Unke O T, Gastegger M. Equivariant message passing for the prediction of tensorial properties and molecular spectra [J]. arXiv: 2102. 03150, 2021
[44] Batzner S, Musaelian A, Sun L X, et al. E(3)-equivariant graph neural networks for data-efficient and accurate interatomic potentials [J]. Nat. Commun., 2022, 13: 2453
doi: 10.1038/s41467-022-29939-5 pmid: 35508450
[45] Musaelian A, Batzner S, Johansson A, et al. Learning local equivariant representations for large-scale atomistic dynamics [J]. Nat. Commun., 2023, 14: 579
doi: 10.1038/s41467-023-36329-y pmid: 36737620
[46] Batatia I, Kovács D P, Simm G N C, et al. MACE: Higher order equivariant message passing neural networks for fast and accurate force fields [J]. arXiv: 2206. 07697, 2023
[47] Wu Y B, Xia J F, Zhang Y L, et al. A simple and efficient equivariant message-passing neural network model for non-local potential energy surface [J]. J. Phys. Chem., 2024, 128A: 11061
[48] Batatia I, Batzner S, Kovács D P, et al. The design space of E(3)-equivariant atom-centered interatomic potentials [J]. arXiv: 2205. 06643, 2022
[49] Cheng B Q. Latent Ewald summation for machine learning of long-range interactions [J]. npj Comput. Mater., 2025, 11: 80
doi: 10.1038/s41524-025-01577-7
[50] Jain A, Ong S P, Hautier G, et al. Commentary: The materials project: A materials genome approach to accelerating materials innovation [J]. APL Mater., 2013, 1: 011002
[51] Chen C, Ye W K, Zuo Y X, et al. Graph networks as a universal machine learning framework for molecules and crystals [J]. Chem. Mater., 2019, 31: 3564
doi: 10.1021/acs.chemmater.9b01294
[52] Chen C, Ong S P. A universal graph deep learning interatomic potential for the periodic table [J]. Nat. Comput. Sci., 2022, 2: 718
doi: 10.1038/s43588-022-00349-3 pmid: 38177366
[53] Deng B W, Zhong P C, Jun K, et al. CHGNet as a pretrained universal neural network potential for charge-informed atomistic modelling [J]. Nat. Mach. Intell., 2023, 5: 1031
doi: 10.1038/s42256-023-00716-3
[54] Merchant A, Batzner S, Schoenholz S S, et al. Scaling deep learning for materials discovery [J]. Nature, 2023, 624: 80
doi: 10.1038/s41586-023-06735-9
[55] Zhang D, Bi H R, Dai F Z, et al. Pretraining of attention-based deep learning potential model for molecular simulation [J]. npj Comput. Mater., 2024, 10: 94
doi: 10.1038/s41524-024-01278-7
[56] Zhang D, Liu X Z J, Zhang X Y, et al. DPA-2: A large atomic model as a multi-task learner [J]. npj Comput. Mater., 2024, 10: 293
doi: 10.1038/s41524-024-01493-2
[57] Batatia I, Benner P, Chiang Y, et al. A foundation model for atomistic materials chemistry [J]. J. Chem. Phys., 2025, 163: 184110
doi: 10.1063/5.0297006
[58] Xie F K, Lu T L, Meng S, et al. GPTFF: A high-accuracy out-of-the-box universal AI force field for arbitrary inorganic materials [J]. Sci. Bull., 2024, 69: 3525
doi: 10.1016/j.scib.2024.08.039 pmid: 39278799
[59] Han T, Li J, Liu L P, et al. Accuracy evaluation of different machine learning force field features [J]. New J. Phys., 2023, 25: 093007
[60] Zuo Y X, Chen C, Li X G, et al. A performance and cost assessment of machine learning interatomic potentials [J]. J. Phys. Chem., 2020, 124A: 731
[61] Dusson G, Bachmayr M, Csányi G, et al. Atomic cluster expansion: Completeness, efficiency and stability [J]. J. Comput. Phys., 2022, 454: 110946
doi: 10.1016/j.jcp.2022.110946
[62] Hodapp M, Shapeev A. Equivariant tensor network potentials [J]. Mach. Learn.: Sci. Technol., 2024, 5: 035075
[63] Podryabinkin E V, Shapeev A V. Active learning of linearly parametrized interatomic potentials [J]. Comput. Mater. Sci., 2017, 140: 171
doi: 10.1016/j.commatsci.2017.08.031
[64] Gubaev K, Podryabinkin E V, Shapeev A V. Machine learning of molecular properties: Locality and active learning [J]. J. Chem. Phys., 2018, 148: 241727
doi: 10.1063/1.5005095
[65] Novikov I S, Gubaev K, Podryabinkin E V, et al. The MLIP package: Moment tensor potentials with MPI and active learning [J]. Mach. Learn.: Sci. Technol., 2021, 2: 025002
[66] Wang J T, Liu P T, Zhu H T, et al. Efficient moment tensor machine-learning interatomic potential for accurate description of defects in Ni-Al Alloys [J]. Phys. Rev. Mater., 2025, 9: 053805
[67] Cohn D A, Ghahramani Z, Jordan M I. Active learning with statistical models [J]. J. Artif. Intell. Res., 1996, 4: 129
doi: 10.1613/jair.295
[68] Jinnouchi R, Miwa K, Karsai F, et al. On-the-fly active learning of interatomic potentials for large-scale atomistic simulations [J]. J. Phys. Chem. Lett., 2020, 11: 6946
doi: 10.1021/acs.jpclett.0c01061 pmid: 32787192
[69] Friederich P, Häse F, Proppe J, et al. Machine-learned potentials for next-generation matter simulations [J]. Nat. Mater., 2021, 20: 750
doi: 10.1038/s41563-020-0777-6 pmid: 34045696
[70] Laio A, Parrinello M. Escaping free-energy minima [J]. Proc. Natl. Acad. Sci. USA, 2002, 99: 12562
pmid: 12271136
[71] Allen R J, Frenkel D, ten Wolde P R. Simulating rare events in equilibrium or nonequilibrium stochastic systems [J]. J. Chem. Phys., 2006, 124: 024102
[72] Barducci A, Bussi G, Parrinello M. Well-tempered metadynamics: A smoothly converging and tunable free-energy method [J]. Phys. Rev. Lett., 2008, 100: 020603
[73] Han X, Lei Y K, Li M D, et al. A brief review of integrated tempering sampling molecular simulation [J]. Chem. Phys. Rev., 2024, 5: 011308
[74] Castellano A, Béjaud R, Richard P, et al. Machine learning assisted canonical sampling (MLACS) [J]. Comput. Phys. Commun., 2025, 316: 109730
doi: 10.1016/j.cpc.2025.109730
[75] Ramakrishnan R, Dral P O, Rupp M, et al. Quantum chemistry structures and properties of 134 kilo molecules [J]. Sci. Data, 2014, 1: 140022
doi: 10.1038/sdata.2014.22
[76] Glass C W, Oganov A R, Hansen N. USPEX—Evolutionary crystal structure prediction [J]. Comput. Phys. Commun., 2006, 175: 713
doi: 10.1016/j.cpc.2006.07.020
[77] Wang J J, Gao H, Han Y, et al. MAGUS: Machine learning and graph theory assisted universal structure searcher [J]. Natl. Sci. Rev., 2023, 10: nwad128
doi: 10.1093/nsr/nwad128
[78] Podryabinkin E V, Tikhonov E V, Shapeev A V, et al. Accelerating crystal structure prediction by machine-learning interatomic potentials with active learning [J]. Phys. Rev., 2019, 99B: 064114
[79] Gubaev K, Podryabinkin E V, Hart G L W, et al. Accelerating high-throughput searches for new alloys with active learning of interatomic potentials [J]. Comput. Mater. Sci., 2019, 156: 148
doi: 10.1016/j.commatsci.2018.09.031
[80] Novoselov I I, Yanilkin A V, Shapeev A V, et al. Moment tensor potentials as a promising tool to study diffusion processes [J]. Comput. Mater. Sci., 2019, 164: 46
doi: 10.1016/j.commatsci.2019.03.049
[81] Shapeev A V, Podryabinkin E V, Gubaev K, et al. Elinvar effect in β-Ti simulated by on-the-fly trained moment tensor potential [J]. New J. Phys., 2020, 22: 113005
doi: 10.1088/1367-2630/abc392
[82] Mukhamedov B, Tasnádi F, Abrikosov I A. Machine learning interatomic potential for the low-modulus Ti-Nb-Zr alloys in the vicinity of dynamical instability [J]. Mater. Des., 2025, 253: 113865
doi: 10.1016/j.matdes.2025.113865
[83] Mei H J, Cheng L Y, Chen L, et al. Development of machine learning interatomic potential for zinc [J]. Comput. Mater. Sci., 2024, 233: 112723
doi: 10.1016/j.commatsci.2023.112723
[84] Forslund A, Ruban A. Ab initio surface free energies of tungsten with full account of thermal excitations [J]. Phys. Rev., 2022, 105B: 045403
[85] Forslund A, Jung J H, Srinivasan P, et al. Thermodynamic properties on the homologous temperature scale from direct upsampling: Understanding electron-vibration coupling and thermal vacancies in bcc refractory metals [J]. Phys. Rev., 2023, 107B: 174309
[86] Srinivasan P, Shapeev A, Neugebauer J, et al. Anharmonicity in bcc refractory elements: A detailed ab initio analysis [J]. Phys. Rev., 2023, 107B: 014301
[87] Zhu L F, Srinivasan P, Gong Y L, et al. Melting properties of the refractory metals V and W and the binary VW alloy fully from first principles [J]. Phys. Rev., 2024, 109B: 094110
[88] Jung J H, Srinivasan P, Forslund A, et al. High-accuracy thermodynamic properties to the melting point from ab initio calculations aided by machine-learning potentials [J]. npj Comput. Mater., 2023, 9: 3
doi: 10.1038/s41524-022-00956-8
[89] Zhang X, Divinski S V, Grabowski B. Ab initio machine-learning unveils strong anharmonicity in non-Arrhenius self-diffusion of tungsten [J]. Nat. Commun., 2025, 16: 394
doi: 10.1038/s41467-024-55759-w
[90] Duff A I, Davey T, Korbmacher D, et al. Improved method of calculating ab initio high-temperature thermodynamic properties with application to ZrC [J]. Phys. Rev., 2015, 91B: 214311
[91] Grabowski B, Ikeda Y, Srinivasan P, et al. Ab initio vibrational free energies including anharmonicity for multicomponent alloys [J]. npj Comput. Mater., 2019, 5: 80
doi: 10.1038/s41524-019-0218-8
[92] Zotov N, Gubaev K, Wörner J, et al. Moment tensor potential for static and dynamic investigations of screw dislocations in bcc Nb [J]. Modell. Simul. Mater. Sci. Eng., 2024, 32: 035032
[93] Wang Y, Liu J B, Li J H, et al. Machine-learning interatomic potential for radiation damage effects in bcc-iron [J]. Comput. Mater. Sci., 2022, 202: 110960
doi: 10.1016/j.commatsci.2021.110960
[94] Kwon H, Shiga M, Kimizuka H, et al. Accurate description of hydrogen diffusivity in bcc metals using machine-learning moment tensor potentials and path-integral methods [J]. Acta Mater., 2023, 247: 118739
doi: 10.1016/j.actamat.2023.118739
[95] Kumar P, Körmann F, Grabowski B, et al. Machine learning potentials for hydrogen absorption in TiCr2 Laves phases [J]. Acta Mater., 2025, 297: 121319
doi: 10.1016/j.actamat.2025.121319
[96] Xu X, Zhang X, Ruban A, et al. Accurate complex-stacking-fault Gibbs energy in Ni3Al at high temperatures [J]. Scr. Mater., 2024, 242: 115934
doi: 10.1016/j.scriptamat.2023.115934
[97] Xu X, Zhang X, Bitzek E, et al. Origin of the yield stress anomaly in L12 intermetallics unveiled with physically informed machine-learning potentials [J]. Acta Mater., 2024, 281: 120423
doi: 10.1016/j.actamat.2024.120423
[98] Novikov B, Grabowski B, Körmann F, et al. Magnetic Moment Tensor Potentials for collinear spin-polarized materials reproduce different magnetic states of bcc Fe [J]. npj Comput. Mater., 2022, 8: 13
doi: 10.1038/s41524-022-00696-9
[99] Kotykhov A S, Gubaev K, Hodapp M, et al. Constrained DFT-based magnetic machine-learning potentials for magnetic alloys: a case study of Fe-Al [J]. Sci. Rep., 2023, 13: 19728
doi: 10.1038/s41598-023-46951-x pmid: 37957211
[100] Kotykhov A S, Gubaev K, Sotskov V, et al. Fitting to magnetic forces improves the reliability of magnetic moment tensor potentials [J]. Comput. Mater. Sci., 2024, 245: 113331
doi: 10.1016/j.commatsci.2024.113331
[101] Taylor A, Jones R M. Constitution and magnetic properties of iron-rich iron-aluminum alloys [J]. J. Phys. Chem. Solids, 1958, 6: 16
doi: 10.1016/0022-3697(58)90213-0
[102] Srinivasan P, Demuriya D, Grabowski B, et al. Electronic moment tensor potentials include both electronic and vibrational degrees of freedom [J]. npj Comput. Mater., 2024, 10: 41
doi: 10.1038/s41524-024-01222-9
[103] Gubaev K, Zaverkin V, Srinivasan P, et al. Performance of two complementary machine-learned potentials in modelling chemically complex systems [J]. npj Comput. Mater., 2023, 9: 129
doi: 10.1038/s41524-023-01073-w
[104] Shuang F, Ji Y C, Laurenti L, et al. Size-dependent strength superiority in multi-principal element alloys versus constituent metals: Insights from machine-learning atomistic simulations [J]. Int. J. Plast., 2025, 188: 104308
doi: 10.1016/j.ijplas.2025.104308
[105] Yin S, Zuo Y X, Abu-Odeh A, et al. Atomistic simulations of dislocation mobility in refractory high-entropy alloys and the effect of chemical short-range order [J]. Nat. Commun., 2021, 12: 4873
doi: 10.1038/s41467-021-25134-0 pmid: 34381027
[106] Jafary-Zadeh M, Khoo K H, Laskowski R, et al. Applying a machine learning interatomic potential to unravel the effects of local lattice distortion on the elastic properties of multi-principal element alloys [J]. J. Alloys Compd., 2019, 803: 1054
doi: 10.1016/j.jallcom.2019.06.318
[107] Gubaev K, Ikeda Y, Tasnádi F, et al. Finite-temperature interplay of structural stability, chemical complexity, and elastic properties of bcc multicomponent alloys from ab initio trained machine-learning potentials [J]. Phys. Rev. Mater., 2021, 5: 073801
[108] Hodapp M, Shapeev A. Machine-learning potentials enable predictive and tractable high-throughput screening of random alloys [J]. Phys. Rev. Mater., 2021, 5: 113802
[109] Zhu L F, Körmann F, Chen Q, et al. Accelerating ab initio melting property calculations with machine learning: Application to the high entropy alloy TaVCrW [J]. npj Comput. Mater., 2024, 10: 274
doi: 10.1038/s41524-024-01464-7
[110] Song Y M, Xian J W, Xu Y J, et al. Machine learning accelerated study on temperature dependent elastic properties of Ti-based refractory high entropy alloys [J]. Mater. Today Commun., 2025, 42: 111559
[111] Liu M F, Wang J T, Hu J W, et al. Layer-by-layer phase transformation in Ti3O5 revealed by machine-learning molecular dynamics simulations [J]. Nat. Commun., 2024, 15: 3079
doi: 10.1038/s41467-024-47422-1
[112] Liu M F, Wang J T, Liu P T, et al. Diverse polymorphs and phase transitions in van der Waals In2Se3 [J]. 2025, arXiv: 2506. 21248v1, 2025
[113] Wang J T, Zhang Y C, Liu Y, et al. Atomistic mechanisms of phase transitions in all-temperature barocaloric material KPF6 [J]. J. Mater. Sci. Technol., 2026, 263: 211
doi: 10.1016/j.jmst.2025.11.009
[114] Jung J H, Forslund A, Srinivasan P, et al. Dynamically stabilized phases with full ab initio accuracy: Thermodynamics of Ti, Zr, Hf with a focus on the hcp-bcc transition [J]. Phys. Rev., 2023, 108B: 184107
[115] Zhao X T, Zhang Z, Hattori T, et al. All-temperature barocaloric effects at pressure-induced phase transitions [J]. Nat. Commun., 2025, 16: 7713
doi: 10.1038/s41467-025-63068-z
[116] Chen B W J, Zhang X L, Zhang J. Accelerating explicit solvent models of heterogeneous catalysts with machine learning interatomic potentials [J]. Chem. Sci., 2023, 14: 8338
doi: 10.1039/d3sc02482b pmid: 37564405
[117] Klimanova O, Rybin N, Shapeev A. Accelerating the global search of adsorbate molecule positions using machine-learning interatomic potentials with active learning [J]. Phys. Chem. Chem. Phys., 2025, 27: 9201
doi: 10.1039/D5CP00532A
[118] Feibelman P J, Hammer B, Nørskov J K, et al. The CO/Pt(111) puzzle [J]. J. Phys. Chem., 2001, 105B: 4018
[119] Grinberg I, Yourdshahyan Y, Rappe A M. CO on Pt(111) puzzle: A possible solution [J]. J. Chem. Phys., 2002, 117: 2264
doi: 10.1063/1.1488596
[120] Ren X G, Rinke P, Joas C, et al. Random-phase approximation and its applications in computational chemistry and materials science [J]. J. Mater. Sci., 2012, 47: 7447
doi: 10.1007/s10853-012-6570-4
[121] Liu P T, Wang J T, Avargues N, et al. Combining machine learning and many-body calculations: Coverage-dependent adsorption of CO on Rh(111) [J]. Phys. Rev. Lett., 2023, 130: 078001
[122] Cao Y, Wang J T, Liu M F, et al. Quantum delocalization enables water dissociation on Ru(0001) [J]. Phys. Rev. Lett., 2025, 134: 178001
doi: 10.1103/PhysRevLett.134.178001
[123] Ou Y L, Ikeda Y, Scholz L, et al. Atomistic modeling of bulk and grain boundary diffusion in solid electrolyte Li6PS5Cl using machine-learning interatomic potentials [J]. Phys. Rev. Mater., 2024, 8: 115407
[124] Kim J H, Jun B, Jang Y J, et al. Highly reliable and large-scale simulations of promising argyrodite solid-state electrolytes using a machine-learned moment tensor potential [J]. Nano Energy, 2024, 124: 109436
doi: 10.1016/j.nanoen.2024.109436
[125] Holekevi Chandrappa M L, Qi J, Chen C, et al. Thermodynamics and kinetics of the cathode-electrolyte interface in all-solid-state Li-S batteries [J]. J. Am. Chem. Soc., 2022, 144: 18009
doi: 10.1021/jacs.2c07482
[1] 康国政, 张旭, 胡冰晖, 双思垚, 于峻石, 熊宇凯, 宋世杰. 基于机器学习的金属材料多尺度塑性力学研究进展[J]. 金属学报, 2026, 62(5): 803-821.
[2] 马成勇, 侯旭儒, 赵琳, 阚成玲, 曹洋, 彭云, 田志凌. 电弧增材制造高强度Al-Mg-Sc系合金研究进展:冶金缺陷、微观组织和力学性能[J]. 金属学报, 2026, 62(1): 29-46.
[3] 黄曾鑫, 蒋逸航, 赖春明, 吴庆捷, 刘大海, 杨亮. 基于原子模拟的金属Fe晶界能与晶界取向相关性分析[J]. 金属学报, 2024, 60(9): 1289-1298.
[4] 刘壮壮, 丁明路, 谢建新. 金属3D打印数字化制造研究进展[J]. 金属学报, 2024, 60(5): 569-584.
[5] 文通其, 刘怀忆, 龚小国, 叶贝琳, 刘思宇, 李卓远. 深度势能方法在材料科学中的应用[J]. 金属学报, 2024, 60(10): 1299-1311.
[6] 刘仕, 黄佳玮, 武静. 机器学习势在铁电材料研究中的应用[J]. 金属学报, 2024, 60(10): 1312-1328.
[7] 陈名毅, 胡俊伟, 余耀辰, 牛海洋. 机器学习分子动力学辅助材料凝固形核研究进展[J]. 金属学报, 2024, 60(10): 1329-1344.
[8] 王冠杰, 刘盛咸, 周健, 孙志梅. 材料研究中的可解释机器学习[J]. 金属学报, 2024, 60(10): 1345-1361.
[9] 沈雪阳, 褚瑞轩, 蒋宜辉, 张伟. 相变存储器材料设计与多尺度模拟的研究进展[J]. 金属学报, 2024, 60(10): 1362-1378.
[10] 李志尚, 赵龙, 宗洪祥, 丁向东. 机器学习型分子力场在金属材料相变与变形领域的研究进展[J]. 金属学报, 2024, 60(10): 1388-1404.
[11] 赵晋彬, 王建韬, 何东昌, 李俊林, 孙岩, 陈星秋, 刘培涛. 氢化物超导体临界转变温度的机器学习模型[J]. 金属学报, 2024, 60(10): 1418-1428.
[12] 张海峰, 闫海乐, 方烽, 贾楠. FeMnCoCrNi高熵合金双晶微柱变形机制的分子动力学模拟[J]. 金属学报, 2023, 59(8): 1051-1064.
[13] 穆亚航, 张雪, 陈梓名, 孙晓峰, 梁静静, 李金国, 周亦胄. 基于热力学计算与机器学习的增材制造镍基高温合金裂纹敏感性预测模型[J]. 金属学报, 2023, 59(8): 1075-1086.
[14] 冀秀梅, 侯美伶, 王龙, 刘玠, 高克伟. 基于机器学习的中厚板变形抗力模型建模与应用[J]. 金属学报, 2023, 59(3): 435-446.
[15] 杨累, 赵帆, 姜磊, 谢建新. 机器学习辅助2000 MPa级弹簧钢成分和热处理工艺开发[J]. 金属学报, 2023, 59(11): 1499-1512.