Please wait a minute...
金属学报  2026, Vol. 62 Issue (5): 756-769    DOI: 10.11900/0412.1961.2025.00301
  综述 本期目录 | 过刊浏览 |
综述:定向凝固枝晶生长的数值模拟
董洪标1(), 郝文硕2
1 School of Metallurgy and Materials, University of Birmingham, Birmingham, B15 2TT, UK
2 清华大学 材料学院 北京 100084
Numerical Modeling of Dendrite Growth During Directional Solidification: A Review
DONG Hongbiao1(), HAO Wenshuo2
1 School of Metallurgy and Materials, University of Birmingham, Birmingham, B15 2TT, UK
2 School of Materials Science and Engineering, Tsinghua University, Beijing 100084, China
引用本文:

董洪标, 郝文硕. 综述:定向凝固枝晶生长的数值模拟[J]. 金属学报, 2026, 62(5): 756-769.
Hongbiao DONG, Wenshuo HAO. Numerical Modeling of Dendrite Growth During Directional Solidification: A Review[J]. Acta Metall Sin, 2026, 62(5): 756-769.

全文: PDF(3046 KB)   HTML
摘要: 

金属凝固作为先进制造的关键基础过程,对工件微观组织和服役性能具有决定性影响。定向凝固是高温合金单晶构件制备的重要技术,但精确控制凝固组织仍面临诸多难点。为系统梳理定向凝固枝晶生长模拟的研究现状和发展趋势,揭示多尺度模拟在预测枝晶形貌、枝晶竞争及缺陷形成中的关键作用,本文以枝晶生长为切入点,系统归纳了凝固成分过冷理论、枝晶生长模型和典型定向凝固工艺,重点综述了有限元、有限差分、元胞自动机和相场法等多尺度模拟方法,并论述了这些方法从宏观物理场模拟到微观枝晶生长建模中的适用性及其代表性成果。最后,本文归纳了定向凝固枝晶生长数值模拟当前面临的挑战,并展望了未来的发展方向。

关键词 : 凝固,  枝晶生长,  定向凝固,  数值模拟    
Abstract:

Solidification is a fundamental process in advanced manufacturing, playing a pivotal role in determining the microstructure and performance of components. Directional solidification is a critical technique for producing single-crystal superalloy components; however, precise control of dendritic structure remains challenging. This article aims to systematically review the current status and future trends of dendrite growth simulations in directional solidification. In addition, it seeks to elucidate the key role of multiscale modeling in predicting dendritic morphology, dendrite competition, and defect formation. This article focuses on dendritic growth and summarizes the constitutional undercooling theory, dendrite growth models, and typical directional solidification processes. Multiscale numerical simulation methods, including finite element, finite difference, cellular automaton, and phase-field approaches, are emphasized, with an analysis of their applicability and a discussion of their representative achievements from macroscopic physical-field simulation to microscopic dendrite growth modeling. Finally, the key challenges are outlined, and prospective advancements in the numerical simulation of dendrite growth in directional solidification are delineated.

Key words: solidification    dendrite growth    directional solidification    numerical simulation
收稿日期: 2025-09-30     
ZTFLH:  TG291  
通讯作者: 董洪标,h.dong.1@bham.ac.uk,主要从事金属凝固数值模拟的研究
Corresponding author: DONG Hongbiao, professor, Tel: 0044(116)2522528, E-mail: h.dong.1@bham.ac.uk
作者简介: 董洪标,男,教授,博士,英国皇家工程院院士
图1  凝固前沿固/液界面处的溶质浓度分布和成分过冷区
图2  定向凝固过程中枝晶竞争生长示意图[19]
图3  高速凝固法和液态金属冷却法定向凝固工艺示意图[17]
ScaleRepresentative methodCharacteristicApplicable problem
Macroscopic scaleFinite element (FE) method, finite difference (FD) method, finite volume method (FVM)Capable of computing the temperature, flow, and stress fields of entire castings or furnacesProcess optimization, temperature gradient, cooling rate, deformation prediction

Mesoscopic/microscopic scale

Phase-field (PF) method

Currently the most widely used method. By introducing phase-field variables, it avoids explicit interface tracking and can naturally simulate complex phenomena such as dendritic morphology, branching, and coarsening

Dendritic growth, interface evolution, micro segregation

Cellular automaton (CA)

Simple rules, high computational efficiency, and easy coupling with macroscopic modelsGrain structure evolution, competitive grain growth, stray grain prediction

Multiscale coupling

CA-FE/FD or PF-FE/FD

Couples macroscopic thermal/flow fields with mesoscopic grain/dendrite growth, balancing computational efficiency and microstructural detailMicrostructure prediction of practical industrial components (e.g., turbine blades)
表1  定向凝固和枝晶生长的多尺度数值模拟方法
图4  利用高速凝固法(恒定抽拉速率3 mm/min)和液态金属冷却法(恒定抽拉速率8 mm/min)制备单晶叶片时的温度场和糊状区演变[18]
图5  翼型内的凝固顺序和流动形态以及凸侧和凹侧溶质分布的数值模拟结果[14]
图6  起晶块三维晶粒组织结构、距底部不同高度处横截面晶粒结构和相应<100>极图的元胞自动机有限元(CAFE)预测结果[64]
图7  螺旋段3D晶粒组织结构、不同高度处横截面晶粒组织结构和对应的<100>极图及晶粒偏转角度分布的CAFE预测结果[9]
图8  利用元胞自动机有限差分(CAFD)法模拟预测柱状晶-等轴晶转变[88]
图9  利用相场法模拟定向凝固过程中汇聚侧枝晶的反常淘汰现象[40]
[1] Zhou Y H, Hu Z Q, Jie W Q. Solidification technology [M]. Beijing: China Machine Press, 1998: 1
[1] 周尧和, 胡壮麒, 介万奇. 凝固技术 [M]. 北京: 机械工业出版社, 1998: 1
[2] Hao W S, Ma S D, Dong Z H, et al. Atomic characteristics of heterogeneous nucleation during solidification of aluminum alloys: A critical review [J]. Mater. Genome Eng. Adv., 2025, 3: e65
[3] Zhang D Y, Qiu D, Gibson M A, et al. Additive manufacturing of ultrafine-grained high-strength titanium alloys [J]. Nature, 2019, 576: 91
doi: 10.1038/s41586-019-1783-1
[4] Ren N, Li J, Zhang R Y, et al. Solute trapping and non-equilibrium microstructure during rapid solidification of additive manufacturing [J]. Nat Commun, 2023, 14: 7990
doi: 10.1038/s41467-023-43563-x pmid: 38042908
[5] Kurz W, Fisher D J, Trivedi R. Progress in modelling solidification microstructures in metals and alloys: Dendrites and cells from 1700 to 2000 [J]. Int. Mater. Rev., 2019, 64: 311
doi: 10.1080/09506608.2018.1537090
[6] Kurz W, Rappaz M, Trivedi R. Progress in modelling solidification microstructures in metals and alloys. Part II: Dendrites from 2001 to 2018 [J]. Int Mater Rev, 2021, 66: 30
doi: 10.1080/09506608.2020.1757894
[7] Dong H, Dai H. Single-crystal casting/directional solidification [J]. Compr. Mater. Process., 2014, 5: 89
[8] Dai H J, D'Souza N, Dong H B. Grain selection in spiral selectors during investment casting of single-crystal turbine blades: Part I. Experimental investigation [J]. Metall. Mater. Trans., 2011, 42A: 3430
[9] Dai H J, Dong H B, D'Souza N, et al. Grain selection in spiral selectors during investment casting of single-crystal components: Part II. Numerical modeling [J]. Metall. Mater. Trans., 2011, 42A: 3439
[10] Yang L W, Ren N, Li J, et al. Thermal-solutal convection-induced low-angle grain boundaries in single-crystal nickel-based superalloy solidification [J]. J. Mater. Sci. Technol., 2025, 208: 214
doi: 10.1016/j.jmst.2024.04.054
[11] Yang X L, Dong H B, Wang W, et al. Microscale simulation of stray grain formation in investment cast turbine blades [J]. Mater. Sci. Eng., 2004, A386: 129
[12] Aveson J W, Tennant P A, Foss B J, et al. On the origin of sliver defects in single crystal investment castings [J]. Acta Mater., 2013, 61: 5162
doi: 10.1016/j.actamat.2013.04.071
[13] Liu Y, Wang F, Ma D X, et al. Freckle prediction model incorporating geometrical effects for Ni-based single-crystal superalloy components [J]. Acta Mater., 2024, 266: 119702
doi: 10.1016/j.actamat.2024.119702
[14] Ren N, Li J, Panwisawas C, et al. Insight into the sensitivities of freckles in the directional solidification of single-crystal turbine blades [J]. J. Manuf. Processes, 2022, 77: 219
doi: 10.1016/j.jmapro.2022.03.019
[15] Perry S J, D'Souza N, Collins D M, et al. An in situ resistance-based method for tracking the temporal evolution of recovery and recrystallization in Ni-base single-crystal superalloy at super-solvus temperatures [J]. Metall. Mater. Trans., 2023, 54A: 1582
[16] Reed R C. The Superalloys: Fundamentals and Applications [M]. Cambridge: Cambridge University Press, 2006: 1
[17] Xu Q Y, Yang C, Yan X W, et al. Development of numerical simulation in nickel-based superalloy turbine blade directional solidification [J]. Acta Metall. Sin., 2019, 55: 1175
doi: 10.11900/0412.1961.2019.00126
[17] 许庆彦, 杨 聪, 闫学伟 等. 高温合金涡轮叶片定向凝固过程数值模拟研究进展 [J]. 金属学报, 2019, 55: 1175
doi: 10.11900/0412.1961.2019.00126
[18] Xu Q Y, Yang C, Zhang H, et al. Multiscale modeling and simulation of directional solidification process of Ni-based superalloy turbine blade casting [J]. Metals, 2018, 8: 632
doi: 10.3390/met8080632
[19] Rappaz M, Gandin C A. Probabilistic modelling of microstructure formation in solidification processes [J]. Acta Metall. Mater., 1993, 41: 345
doi: 10.1016/0956-7151(93)90065-Z
[20] Kobayashi R. A numerical approach to three-dimensional dendritic solidification [J]. Exp. Math., 1994, 3: 59
doi: 10.1080/10586458.1994.10504577
[21] Swope W C, Andersen H C. 106-particle molecular-dynamics study of homogeneous nucleation of crystals in a supercooled atomic liquid [J]. Phys. Rev., 1990, 41B: 7042
[22] Hao W S, Ma S D, Hu Y W, et al. Solute adsorption energy criterion for discovering effective grain refiners in high-Si Al-Si alloys [J]. J. Mater. Res. Technol., 2025, 39: 506
doi: 10.1016/j.jmrt.2025.09.123
[23] Feng S, Zhou H Y, Dong H B. Using deep neural network with small dataset to predict material defects [J]. Mater. Des., 2019, 162: 300
doi: 10.1016/j.matdes.2018.11.060
[24] Bai X P, Zhang X C. Artificial intelligence-powered materials science [J]. Nano-Micro Lett., 2025, 17: 135
doi: 10.1007/s40820-024-01634-8 pmid: 39912967
[25] Jiang X, Xue D Z, Bai Y, et al. AI4Materials: Transforming the landscape of materials science and enigneering [J]. Rev. Mater. Res., 2025, 1: 100010
[26] Xu X W, Ren N, Lu Z Q, et al. A data-driven approach for the fast prediction of macrosegregation [J]. Metall. Mater. Trans., 2024, 55A: 2083
[27] Udu A G, Lecchini-Visintini A, Dong H B. Feature selection for aero-engine fault detection [A]. Database and Expert Systems Applications: 34th International Conference [C]. Penang: Springer, 2023: 522
[28] Dai H J, Dong H B, Atkinson H V, et al. Simulation of the columnar-to-equiaxed transition in alloy solidification—The effect of nucleation undercooling, density of nuclei in bulk liquid and alloy solidification range on the transition [J]. Solid State Phenom., 2008, 139: 129
doi: 10.4028/www.scientific.net/SSP
[29] Strickland J, Nenchev B, Dong H B. On directional dendritic growth and primary spacing—A review [J]. Crystals, 2020, 10: 627
doi: 10.3390/cryst10070627
[30] Hunt J D. Steady state columnar and equiaxed growth of dendrites and eutectic [J]. Mater. Sci. Eng., 1984, 65: 75
[31] Kurz W, Fisher D J. Fundamentals of Solidification [M]. Uetikon-Zuerich: Trans Tech Publications, 1998: 67
[32] Wang W, Lee P D, McLean M. A model of solidification microstructures in nickel-based superalloys: Predicting primary dendrite spacing selection [J]. Acta Mater., 2003, 51: 2971
doi: 10.1016/S1359-6454(03)00110-1
[33] Kermanpur A, Varahraam N, Engilehei E, et al. Directional solidification of Ni base superalloy IN738LC to improve creep properties [J]. Mater. Sci. Technol., 2000, 16: 579
doi: 10.1179/026708300101508117
[34] Hunt J D, Lu S Z. Numerical modeling of cellular/dendritic array growth: Spacing and structure predictions [J]. Metall. Mater. Trans., 1996, 27A: 611
[35] Dong H B. Evolution of dendritic patterns during directional solidification of Ni-base alloys: Towards hexagonally ordered, close-packed dendrite arrays [J]. Metall. Mater. Trans., 2026, 57A: 1709
[36] Strickland J, Nenchev B, Perry S, et al. On the nature of hexagonality within the solidification structure of single crystal alloys: Mechanisms and applications [J]. Acta Mater., 2020, 200: 417
doi: 10.1016/j.actamat.2020.09.019
[37] Strickland J, Nenchev B, Tassenberg K, et al. On the origin of mosaicity in directionally solidified Ni-base superalloys [J]. Acta Mater., 2021, 217: 117180
doi: 10.1016/j.actamat.2021.117180
[38] Walton D, Chalmers B. The origin of the preferred orientation in the columnar zone of ingots [J]. Trans. Metall. Soc. AIME, 1959, 215: 447
[39] Takaki T, Ohno M, Shimokawabe T, et al. Two-dimensional phase-field simulations of dendrite competitive growth during the directional solidification of a binary alloy bicrystal [J]. Acta Mater., 2014, 81: 272
doi: 10.1016/j.actamat.2014.08.035
[40] Takaki T, Sakane S, Ohno M, et al. Large-scale phase-field studies of three-dimensional dendrite competitive growth at the converging grain boundary during directional solidification of a bicrystal binary alloy [J]. ISIJ Int., 2016, 56: 1427
doi: 10.2355/isijinternational.ISIJINT-2016-156
[41] Ge H H, Li J, Han X J, et al. Dendritic model for macrosegregation prediction of large scale castings [J]. J. Mater. Process. Technol., 2016, 227: 308
doi: 10.1016/j.jmatprotec.2015.08.020
[42] Yang L W, Ren N, Panwisawas C, et al. Melt flow-induced mechanical deformation of dendrites in alloy solidification: A coupled thermal fluid-solid mechanics approach [J]. J. Mater. Res. Technol., 2023, 25: 4094
doi: 10.1016/j.jmrt.2023.06.222
[43] Yang L W, Ren N, Panwisawas C, et al. Melt flow-induced mechanical deformation and fracture behaviour of dendrites in alloy solidification [J]. Metall. Mater. Trans., 2023, 54A: 4612
[44] Zhou Y Z, Sun X F. Effect of solidification rate on competitive grain growth in directional solidification of a nickel-base superalloy [J]. Sci. China Technol. Sci., 2012, 55: 1327
doi: 10.1007/s11431-012-4764-2
[45] Xie X L, Zhou L P, Yu J B, et al. Effect of weak transverse magnetic field on the competitive grain growth of Ni-based superalloy with divergent bi-crystals[J]. Acta Metall. Sin., 2025, 61: 1203
doi: 10.11900/0412.1961.2023.00438
[45] 谢信亮, 周丽萍, 余建波 等. 横向弱磁场对镍基高温合金发散双晶竞争生长行为的影响 [J]. 金属学报, 2025, 61: 1203
doi: 10.11900/0412.1961.2023.00438
[46] Li J J, Wang Z J, Wang Y Q, et al. Phase-field study of competitive dendritic growth of converging grains during directional solidification [J]. Acta Mater., 2012, 60: 1478
doi: 10.1016/j.actamat.2011.11.037
[47] Ma D X. Development of single crystal solidification technology for production of superalloy turbine blades [J]. Acta Metall. Sin., 2015, 51: 1179
[47] 马德新. 高温合金叶片单晶凝固技术的新发展 [J]. 金属学报, 2015, 51: 1179
[48] Hofmeister M, Franke M M, Koerner C, et al. Single crystal casting with fluidized carbon bed cooling: A process innovation for quality improvement and cost reduction [J]. Metall. Mater. Trans., 2017, 48B: 3132
[49] Wang F, Ma D X, Zhang J, et al. Effect of local cooling rates on the microstructures of single crystal CMSX-6 superalloy: A comparative assessment of the Bridgman and the downward directional solidification processes [J]. J. Alloys Compd., 2014, 616: 102
doi: 10.1016/j.jallcom.2014.07.084
[50] Giamei A F, Tschinkel J G. Liquid metal cooling: A new solidification technique [J]. Metall. Trans., 1976, 7A: 1427
[51] Elliott A J, Pollock T M, Tin S, et al. Directional solidification of large superalloy castings with radiation and liquid-metal cooling: A comparative assessment [J]. Metall. Mater. Trans., 2004, 35A: 3221
[52] Liu L. The progress of investment casting of nickel-based superalloys [J]. Foundry, 2012, 61: 1273
[52] 刘 林. 高温合金精密铸造技术研究进展 [J]. 铸造, 2012, 61: 1273
[53] Bondarenko Y A, Kablov E N, Surova V A, et al. Effect of high-gradient directed crystallization on the structure and properties of rhenium-bearing single-crystal alloy [J]. Met. Sci. Heat Treat., 2006, 48: 360
doi: 10.1007/s11041-006-0099-6
[54] Brundidge C L, Miller J D, Pollock T M. Development of dendritic structure in the liquid-metal-cooled, directional-solidification process [J]. Metall. Mater. Trans., 2011, 42A: 2723
[55] Miller J D, Yuan L, Lee P D, et al. Simulation of diffusion-limited lateral growth of dendrites during solidification via liquid metal cooling [J]. Acta Mater., 2014, 69: 47
doi: 10.1016/j.actamat.2014.01.035
[56] Miller J D, Pollock T M. Stability of dendrite growth during directional solidification in the presence of a non-axial thermal field [J]. Acta Mater., 2014, 78: 23
doi: 10.1016/j.actamat.2014.05.040
[57] Liu L, Huang T W, Qu M, et al. High thermal gradient directional solidification and its application in the processing of nickel-based superalloys [J]. J. Mater. Process. Technol., 2010, 210: 159
doi: 10.1016/j.jmatprotec.2009.07.022
[58] Liu L, Sun D J, Huang T W, et al. Directional solidification under high thermal gradient and its application in superalloys processing [J]. Acta Metall. Sin., 2018, 54: 615
doi: 10.11900/0412.1961.2018.00075
[58] 刘 林, 孙德建, 黄太文 等. 高梯度定向凝固技术及其在高温合金制备中的应用 [J]. 金属学报, 2018, 54: 615
[59] Franke M M, Hilbinger R M, Lohmüller A, et al. The effect of liquid metal cooling on thermal gradients in directional solidification of superalloys: Thermal analysis [J]. J. Mater. Process. Technol., 2013, 213: 2081
doi: 10.1016/j.jmatprotec.2013.06.001
[60] Napolitano R E, Schaefer R J. The convergence-fault mechanism for low-angle boundary formation in single-crystal castings [J]. J. Mater. Sci., 2000, 35: 1641
doi: 10.1023/A:1004747612160
[61] Goulette M J, Spilling P D, Arthey R P. Cost effective single crystals [A]. Superalloys 1984: Fifth International Symposium [C]. TMS, 1984: 167
[62] D'Souza N, Jennings P A, Yang X L, et al. Seeding of single-crystal superalloys—Role of constitutional undercooling and primary dendrite orientation on stray-grain nucleation and growth [J]. Metall. Mater. Trans., 2005, 36B: 657
[63] Dantzig J A, Rappaz M. Solidification [M]. Lausanne: EPFL Press, 2016: 209
[64] Dai H J, Gebelin J C, Newell M, et al. Grain selection during solidification in spiral grain selector [A]. Superalloys 2008 [M]. Pittsburgh, PA. TMS, 2008: 367
[65] Ren N, Li J, Wang B Q, et al. Design of variable withdrawal rate for superalloy single-crystal blade fabrication [J]. Mater. Des., 2021, 198: 109347
doi: 10.1016/j.matdes.2020.109347
[66] Pan D, Xu Q Y, Liu B C. Modelling on directional solidification of superalloy blades with furnace wall temperature evolution [J]. Acta Metall. Sin., 2010, 46: 294
doi: 10.3724/SP.J.1037.2009.00578
[66] 潘 冬, 许庆彦, 柳百成. 考虑炉壁温度变化的高温合金叶片定向凝固过程模拟 [J]. 金属学报, 2010, 46: 294
[67] Li Z L. Experimental research and numerical simulation on primary recrystallization of nickel-based single crystal superalloy [D]. Beijing: Tsinghua University, 2016
[67] 李忠林. 镍基单晶高温合金静态再结晶实验研究及数值模拟 [D]. 北京: 清华大学, 2016
[68] Ren N, Li J, Panwisawas C, et al. Thermal-solutal-fluid flow of channel segregation during directional solidification of single-crystal nickel-based superalloys [J]. Acta Mater., 2021, 206: 116620
doi: 10.1016/j.actamat.2020.116620
[69] Ren N, Panwisawas C, Li J, et al. Solute enrichment induced dendritic fragmentation in directional solidification of nickel-based superalloys [J]. Acta Mater., 2021, 215: 117043
doi: 10.1016/j.actamat.2021.117043
[70] Rappaz M, Gandin C A, Desbiolles J L, et al. Prediction of grain structures in various solidification processes [J]. Metall. Mater. Trans., 1996, 27A: 695
[71] Gandin C A, Rappaz M. A coupled finite element-cellular automaton model for the prediction of dendritic grain structures in solidification processes [J]. Acta Metall. Mater., 1994, 42: 2233
doi: 10.1016/0956-7151(94)90302-6
[72] Gandin C A, Rappaz M, Tintillier R. 3-dimensional simulation of the grain formation in investment castings [J]. Metall. Mater. Trans., 1994, 25A: 629
[73] Meng X B, Li J G, Jin T, et al. Evolution of grain selection in spiral selector during directional solidification of nickel-base superalloys [J]. J. Mater. Sci. Technol., 2011, 27: 118
[74] Meng X B, Lu Q, Li J G, et al. Modes of grain selection in spiral selector during directional solidification of nickel-base superalloys [J]. J. Mater. Sci. Technol., 2012, 28: 214
doi: 10.1016/S1005-0302(12)60044-9
[75] Zhang R L, Chen L N, Li C H, et al. Influence of spiral crystal selector on crystal orientation of single crystal superalloy [J]. Trans. Nonferrous Met. Soc. China, 2012, 22: 1092
doi: 10.1016/S1003-6326(11)61288-0
[76] Wang N, Liu L, Gao S F, et al. Simulation of grain selection during single crystal casting of a Ni-base superalloy [J]. J. Alloys Compd., 2014, 586: 220
doi: 10.1016/j.jallcom.2013.10.036
[77] Carter P, Cox D C, Gandin C A, et al. Process modelling of grain selection during the solidification of single crystal superalloy castings [J]. Mater. Sci. Eng., 2000, A280: 233
[78] Dai H J, Gebelin J C, D'Souza N, et al. Effect of spiral shape on grain selection during casting of single crystal turbine blades [J]. Int. J. Cast Met. Res., 2009, 22: 54
doi: 10.1179/136404609X367317
[79] Gao S F, Liu L, Zhang J, et al. Simulation of stray grain formation at the platform during Ni-base single crystal superalloy DD403 casting [J]. China Foundry, 2015, 12: 118
[80] Li Y F. Study on stray grain formation in the platform of Ni-based single crystal superalloys turbine blade [D]. Xi'an: Northwestern Polytechnical University, 2018
[80] 李亚峰. 镍基单晶高温合金涡轮叶片平台杂晶缺陷研究 [D]. 西安: 西北工业大学, 2018
[81] Ma D X, Wang F, Sun H Y, et al. Study on sliver defects in single crystal castings of superalloys [J]. Foundry, 2019, 68: 567
[81] 马德新, 王 富, 孙洪元 等. 高温合金单晶铸件中条纹晶缺陷的试验研究 [J]. 铸造, 2019, 68: 567
[82] Meng X B, Li J G, Chen Z Q, et al. Effect of platform dimension on the dendrite growth and stray grain formation in a Ni-base single-crystal superalloy [J]. Metall. Mater. Trans., 2013, 44A: 1955
[83] Sa S P, Yang W C, Qin J R, et al. Numerical simulation of blade arrangement on stray grains in a fourth-generation single crystal superalloy blade [J]. Mater. China, 2024, 43: 871
[83] 撒世鹏, 杨文超, 秦嘉润 等. 叶片排列方式对一种第四代单晶高温合金叶片杂晶影响的数值模拟研究 [J]. 中国材料进展, 2024, 43: 871
[84] Yang W C, Sa S P, Hao W S, et al. Temperature field and microstructure simulation of directional solidification process of single crystal blade prepared efficiently with different module structures [J]. Rare Met. Mater. Eng., 2023, 52: 3847
[84] 杨文超, 撒世鹏, 郝文硕 等. 不同模组结构高效制备单晶叶片定向凝固过程的温度场及组织模拟 [J]. 稀有金属材料与工程, 2023, 52: 3847
[85] Gandin C A, Rappaz M. A 3D Cellular Automaton algorithm for the prediction of dendritic grain growth [J]. Acta Mater., 1997, 45: 2187
doi: 10.1016/S1359-6454(96)00303-5
[86] Thévoz P, Desbiolles J L, Rappaz M. Modeling of equiaxed microstructure formation in casting [J]. Metall. Trans., 1989, 20A: 311
[87] Kurz W, Giovanola B, Trivedi R. Theory of microstructural development during rapid solidification [J]. Acta Metall., 1986, 34: 823
doi: 10.1016/0001-6160(86)90056-8
[88] Dong H B, Lee P D. Simulation of the columnar-to-equiaxed transition in directionally solidified Al-Cu alloys [J]. Acta Mater., 2005, 53: 659
doi: 10.1016/j.actamat.2004.10.019
[89] Karma A. Phase-field model of eutectic growth [J]. Phys. Rev., 1994, 49E: 2245
[90] Takaki T. Phase-field modeling and simulations of dendrite growth [J]. ISIJ Int., 2014, 54: 437
doi: 10.2355/isijinternational.54.437
[91] Warren J A, Boettinger W J. Prediction of dendritic growth and microsegregation patterns in a binary alloy using the phase-field method [J]. Acta Metall. Mater., 1995, 43: 689
doi: 10.1016/0956-7151(94)00285-P
[92] Karma A, Rappel W J. Quantitative phase-field modeling of dendritic growth in two and three dimensions [J]. Phys. Rev., 1998, 57E: 4323
[93] Steinbach I, Apel M. Multi phase field model for solid state transformation with elastic strain [J]. Physica, 2006, 217D: 153
[94] Ginzburg V L, Landau L D. On the theory of superconductivity [A]. On Superconductivity and Superfluidity: A Scientific Autobiography [M]. Berlin, Heidelberg: Springer, 2009: 113
[95] Yang C, Xu Q Y, Liu B C. Study of dendrite growth with natural convection in superalloy directional solidification via a multiphase-field-lattice Boltzmann model [J]. Comput. Mater. Sci., 2019, 158: 130
doi: 10.1016/j.commatsci.2018.11.024
[96] Xia H, Yang Y, Feng Q, et al. Generation mechanism and motion behavior of sliver defect in single crystal Ni-based superalloy [J]. J. Mater. Sci. Technol., 2023, 137: 232
doi: 10.1016/j.jmst.2022.07.045
[1] 胡亮, 王海鹏, 魏炳波. 基于空间站的金属材料研究进展[J]. 金属学报, 2026, 62(5): 685-704.
[2] 朱苗勇, 王卫领. 连铸凝固过程溶质偏析形成机理及其控制研究进展[J]. 金属学报, 2026, 62(5): 855-874.
[3] 谢洪吉, 李嘉荣, 骆宇时, 郑素杰, 骆凯伦. 凝固条件对DD6单晶高温合金组织演化的影响[J]. 金属学报, 2026, 62(4): 550-560.
[4] 朱宝丰, 李晨宇, 张士杰, 李日. Al-4.7%Cu合金枝晶凝固动态收缩的数值模拟[J]. 金属学报, 2026, 62(3): 509-522.
[5] 杨林洁, 张丽丽, 赵九洲, 江鸿翔, 何杰. Zn-Pb偏晶合金微量界面活性元素选取[J]. 金属学报, 2026, 62(3): 532-540.
[6] 贾玉亮, 张勇佳, 史泽楷, 沈旭, 殷亚军, 施长坤, 周建新, 吕志刚. 高温合金定向凝固雀斑形成机理及控制技术研究进展[J]. 金属学报, 2026, 62(2): 309-327.
[7] 韩鸿华, 史清宇, 杨诚乐, 孔德帅, 陈高强. 铝合金搅拌摩擦焊热-力-流耦合仿真及材料迁移轨迹解析[J]. 金属学报, 2026, 62(1): 148-158.
[8] 瞿铁, 谢杨, 王重阳, 李利霞, 徐侠剑, 毛峙溆, 骆文泽, 黄智泉, 邓德安. 34CrNi1Mo/Q355B异种钢对接接头残余应力及焊后热处理对残余应力的影响[J]. 金属学报, 2026, 62(1): 203-216.
[9] 王飞翔, 陈忠奉, 尹晓宇, 熊良华, 谢红兰, 邓彪, 肖体乔. 基于X射线体视成像实现高温合金熔体凝固三维显微结构的原位观测[J]. 金属学报, 2025, 61(7): 1109-1118.
[10] 王强, 李小兵, 郝俊杰, 陈波, 张滨, 张二林, 刘奎. 一种新型Ti-Al-Mn-Nb合金的固态相变行为[J]. 金属学报, 2025, 61(7): 1060-1070.
[11] 汤思璠, 魏晶晶, 岳怡心, 李鹏宇, 姚曼, 王旭东. 六重对称合金枝晶生长场变量扩散元胞自动机模型[J]. 金属学报, 2025, 61(6): 941-952.
[12] 赵广迪, 李阳, 姚晓雨, 王亮, 李渭滨, 潘玉华, 李维娟, 王兆宇. B对Fe-Cr-B-C合金凝固行为、强韧性及耐磨性的影响[J]. 金属学报, 2025, 61(5): 699-716.
[13] 杨明辉, 李星吾, 孙崇昊, 阮莹. 定向凝固与固态相变双联协控下Monel K-500合金的组织和力学性能[J]. 金属学报, 2025, 61(4): 561-571.
[14] 梁炫, 侯廷平, 张东, 谭昕暘, 吴开明. 中碳Nb合金化钢液析碳化物的析出行为[J]. 金属学报, 2025, 61(4): 653-664.
[15] 邹建新, 张嘉祺, 赵颖燕, 林羲, 丁文江. 高容量镁基储氢合金材料研究与应用进展[J]. 金属学报, 2025, 61(3): 420-436.