| 燃料电池金属双极板的研究进展与展望 |
罗海文( ), 林雄, 刘高阳, 胡斌( ) |
| 北京科技大学 冶金与生态工程学院 北京 100083 |
|
| Progress and Perspectives on Metallic Bipolar Plates in Fuel Cells |
LUO Haiwen( ), LIN Xiong, LIU Gaoyang, HU Bin( ) |
| School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
罗海文, 林雄, 刘高阳, 胡斌. 燃料电池金属双极板的研究进展与展望[J]. 金属学报, 2026, 62(2): 263-274.
Haiwen LUO,
Xiong LIN,
Gaoyang LIU,
Bin HU.
Progress and Perspectives on Metallic Bipolar Plates in Fuel Cells[J]. Acta Metall Sin, 2026, 62(2): 263-274.
| [1] |
Du Z Z, Wang J, Wang J, et al. Research progress of key materials in proton exchange membrane fuel cell [J]. J. Mater. Eng., 2022, 50(12): 35
doi: 10.11868/j.issn.1001-4381.2022.000040
|
| [1] |
杜真真, 王 珺, 王 晶 等. 质子交换膜燃料电池关键材料的研究进展 [J]. 材料工程, 2022, 50(12): 35
doi: 10.11868/j.issn.1001-4381.2022.000040
|
| [2] |
Hermann A, Chaudhuri T, Spagnol P. Bipolar plates for PEM fuel cells: A review [J]. Int. J. Hydrogen Energy, 2005, 30: 1297
doi: 10.1016/j.ijhydene.2005.04.016
|
| [3] |
U.S. Department of Energy. Targets for bipolar plates [R]. DOE/GO-102020-5486, 2020
|
| [4] |
Hung Y, Tawfik H, Mahajan D. Durability and characterization studies of polymer electrolyte membrane fuel cell’s coated aluminum bipolar plates and membrane electrode assembly [J]. J. Power Sources, 2009, 186: 123
doi: 10.1016/j.jpowsour.2008.09.079
|
| [5] |
André J, Antoni L, Petit J P. Corrosion resistance of stainless steel bipolar plates in a PEFC environment: A comprehensive study [J]. Int. J. Hydrogen Energy, 2010, 35: 3684
doi: 10.1016/j.ijhydene.2010.01.062
|
| [6] |
Wilkinson D P, Zhang J J, Hui R, et al. Proton Exchange Membrane Fuel Cells: Materials Properties and Performance [M]. Boca Raton: CRC Press, 2009: 1
|
| [7] |
Wang H, Turner J A. Reviewing metallic PEMFC bipolar plates [J]. Fuel Cells, 2010, 10: 510
doi: 10.1002/fuce.v10:4
|
| [8] |
Hamilton P J, Pollet B G. Polymer electrolyte membrane fuel cell (PEMFC) flow field plate: Design, materials and characterisation [J]. Fuel Cells, 2010, 10: 489
doi: 10.1002/fuce.v10:4
|
| [9] |
Lee D, Lim J W, Lee D G. Cathode/anode integrated composite bipolar plate for high-temperature PEMFC [J]. Compos. Struct., 2017, 167: 144
doi: 10.1016/j.compstruct.2017.01.080
|
| [10] |
Barranco J, Barreras F, Lozano A, et al. Influence of CrN-coating thickness on the corrosion resistance behaviour of aluminium-based bipolar plates [J]. J. Power Sources, 2011, 196: 4283
doi: 10.1016/j.jpowsour.2010.11.069
|
| [11] |
Fetohi A E, Hameed R M A, El-Khatib K M, et al. Study of different aluminum alloy substrates coated with Ni-Co-P as metallic bipolar plates for PEM fuel cell applications [J]. Int. J. Hydrogen Energy, 2012, 37: 10807
doi: 10.1016/j.ijhydene.2012.04.066
|
| [12] |
Mawdsley J R, Carter J D, Wang X P, et al. Composite-coated aluminum bipolar plates for PEM fuel cells [J]. J. Power Sources, 2013, 231: 106
doi: 10.1016/j.jpowsour.2012.12.074
|
| [13] |
Tsai S Y, Lin C H, Jian Y J, et al. The fabrication and characteristics of electroless nickel and immersion Au-polytetrafluoroethylene composite coating on aluminum alloy 5052 as bipolar plate [J]. Surf. Coat. Technol., 2017, 313: 151
doi: 10.1016/j.surfcoat.2017.01.064
|
| [14] |
Hou K H, Lin C H, Ger M D, et al. Analysis of the corrosion behavior of Al alloy bipolar plate for proton exchange membrane fuel cell (PEMFC) under operating thermal conditions [J]. Int. J. Green Energy, 2012, 9: 71
doi: 10.1080/15435075.2011.621474
|
| [15] |
Tsai S Y, Bai C Y, Lin C H, et al. The characteristics and performance of electroless nickel and immersion Au plated aluminum alloy bipolar plates in polymer electrolyte membrane fuel cells [J]. J. Power Sources, 2012, 214: 51
doi: 10.1016/j.jpowsour.2012.04.030
|
| [16] |
Aukland N, Boudina A, Eddy D S, et al. Alloys that form conductive and passivating oxides for proton exchange membrane fuel cell bipolar plates [J]. J. Mater. Res., 2004, 19: 1723
doi: 10.1557/JMR.2004.0216
|
| [17] |
Dincer I. Technical, environmental and exergetic aspects of hydrogen energy systems [J]. Int. J. Hydrogen Energy, 2002, 27: 265
doi: 10.1016/S0360-3199(01)00119-7
|
| [18] |
Zhang D M, Duan L T, Guo L, et al. TiN-coated titanium as the bipolar plate for PEMFC by multi-arc ion plating [J]. Int. J. Hydrogen Energy, 2011, 36: 9155
doi: 10.1016/j.ijhydene.2011.04.123
|
| [19] |
Qian Y, Xu J. Properties of ZrC nanocrystalline coating on Ti alloy bipolar plates in simulated PEMFC environments [J]. Rare Met. Mater. Eng., 2017, 46: 1033
|
| [19] |
钱 阳, 徐 江. 模拟PEMFC环境下纳米晶ZrC涂层钛合金双及板的性能研究 [J]. 稀有金属材料与工程, 2017, 46: 1033
|
| [20] |
Qian Y, Xu J. Properties of Zr nanocrystalline coating on Ti alloy bipolar plates in simulated PEMFC environments [J]. Acta Phys.-Chim. Sin., 2015, 31: 291
doi: 10.3866/PKU.WHXB201411262
|
| [21] |
Xu J, Huang H J, Li Z Y, et al. Corrosion behavior of a ZrCN coated Ti alloy with potential application as a bipolar plate for proton exchange membrane fuel cell [J]. J. Alloys Compd., 2016, 663: 718
doi: 10.1016/j.jallcom.2015.12.197
|
| [22] |
Hsieh S S, Huang C F, Feng C L. A novel design and micro-fabrication for copper (Cu) electroforming bipolar plates [J]. Micron, 2008, 39: 263
doi: 10.1016/j.micron.2007.03.003
|
| [23] |
Tran T Q, Lee J K Y, Chinnappan A, et al. High-performance carbon fiber/gold/copper composite wires for lightweight electrical cables [J]. J. Mater. Sci. Technol., 2020, 42: 46
doi: 10.1016/j.jmst.2019.08.057
|
| [24] |
Lee H Y, Lee S H, Kim J H, et al. Thermally nitrided Cu-5.3Cr alloy for application as metallic separators in PEMFCs [J]. Int. J. Hydrogen Energy, 2008, 33: 4171
doi: 10.1016/j.ijhydene.2008.04.057
|
| [25] |
Pan T J, Zuo X W, Wang T, et al. Electrodeposited conductive polypyrrole/polyaniline composite film for the corrosion protection of copper bipolar plates in proton exchange membrane fuel cells [J]. J. Power Sources, 2016, 302: 180
doi: 10.1016/j.jpowsour.2015.10.027
|
| [26] |
Ashok Kumar P, Vasanth Kumar D, Davis Hans S J, et al. Investigation of stainless steel 316 coated with nickel [J]. Mater. Today Proc., 2022, 62: 2376
|
| [27] |
Mohanty S, Kumar Senapati A. Study on wear behavior of low nickel austenitic stainless steel by using ball on disc [J]. Mater. Today Proc., 2022, 66: 1961
|
| [28] |
Song S, Yu L, Xiao X, et al. Outstanding oxygen evolution reaction performance of nickel iron selenide/stainless steel mat for water electrolysis [J]. Mater. Today Phys., 2020, 13: 100216
|
| [29] |
Ghorbani M M, Taherian R, Bozorg M. Investigation on physical and electrochemical properties of TiN-coated Monel alloy used for bipolar plates of proton exchange membrane fuel cell [J]. Mater. Chem. Phys., 2019, 238: 121916
doi: 10.1016/j.matchemphys.2019.121916
|
| [30] |
Ben Jadi S, El Jaouhari A, Aouzal Z, et al. Electropolymerization and corrosion resistance of polypyrrole on nickel bipolar plate for PEM fuel cell application [J]. Mater. Today Proc., 2020, 22: 52
|
| [31] |
Sun Y T, Tan X, Lei L L, et al. Revisiting the effect of molybdenum on pitting resistance of stainless steels [J]. Tungsten, 2021, 3: 329
doi: 10.1007/s42864-021-00099-1
|
| [32] |
Malik A U, Siddiqi N A, Ahmad S, et al. The effect of dominant alloy additions on the corrosion behavior of some conventional and high alloy stainless steels in seawater [J]. Corros. Sci., 1995, 37: 1521
|
| [33] |
Kim J K, Kim Y H, Lee B H, et al. New findings on intergranular corrosion mechanism of stabilized stainless steels [J]. Electrochim. Acta, 2011, 56: 1701
doi: 10.1016/j.electacta.2010.08.042
|
| [34] |
Davies D P, Adcock P L, Turpin M, et al. Stainless steel as a bipolar plate material for solid polymer fuel cells [J]. J. Power Sources, 2000, 86: 237
doi: 10.1016/S0378-7753(99)00524-8
|
| [35] |
Davies D P, Adcock P L, Turpin M, et al. Bipolar plate materials for solid polymer fuel cells [J]. J. Appl. Electrochem., 2000, 30: 101
doi: 10.1023/A:1003831406406
|
| [36] |
Wang H L, Sweikart M A, Turner J A. Stainless steel as bipolar plate material for polymer electrolyte membrane fuel cells [J]. J. Power Sources, 2003, 115: 243
doi: 10.1016/S0378-7753(03)00023-5
|
| [37] |
Chanda U K, Behera A, Roy S, et al. Evaluation of Ni-Cr-P coatings electrodeposited on low carbon steel bipolar plates for polymer electrolyte membrane fuel cell [J]. Int. J. Hydrogen Energy, 2018, 43: 23430
doi: 10.1016/j.ijhydene.2018.10.218
|
| [38] |
Zhang M, Kim K H, Shao Z G, et al. Effects of Mo content on microstructure and corrosion resistance of arc ion plated Ti-Mo-N films on 316L stainless steel as bipolar plates for polymer exchange membrane fuel cells [J]. J. Power Sources, 2014, 253: 201
doi: 10.1016/j.jpowsour.2013.12.075
|
| [39] |
Peng S, Xu J, Xie Z H, et al. Titanium bipolar plates augmented by nanocrystalline TiZrHfMoW coatings for application in proton exchange membrane fuel cells [J]. Appl. Surf. Sci., 2022, 591: 153200
doi: 10.1016/j.apsusc.2022.153200
|
| [40] |
Kumagai M, Myung S T, Katada Y, et al. Stability of type 310S stainless steel bipolar plates tested at various current densities in proton exchange membrane fuel cells [J]. Electrochim. Acta, 2016, 211: 754
doi: 10.1016/j.electacta.2016.06.106
|
| [41] |
Myung S T, Kumagai M, Asaishi R, et al. Nanoparticle TiN-coated type 310S stainless steel as bipolar plates for polymer electrolyte membrane fuel cell [J]. Electrochem. Commun., 2008, 10: 480
doi: 10.1016/j.elecom.2008.01.001
|
| [42] |
Wang Z Y, Feng K, Li Z G, et al. Self-passivating carbon film as bipolar plate protective coating in polymer electrolyte membrane fuel cell [J]. Int. J. Hydrogen Energy, 2016, 41: 5783
doi: 10.1016/j.ijhydene.2016.02.076
|
| [43] |
Joseph S, McClure J C, Chianelli R, et al. Conducting polymer-coated stainless steel bipolar plates for proton exchange membrane fuel cells (PEMFC) [J]. Int. J. Hydrogen Energy, 2005, 30: 1339
doi: 10.1016/j.ijhydene.2005.04.011
|
| [44] |
Lee S H, Kakati N, Maiti J, et al. Corrosion and electrical properties of CrN- and TiN-coated 316L stainless steel used as bipolar plates for polymer electrolyte membrane fuel cells [J]. Thin Solid Films, 2013, 529: 374
doi: 10.1016/j.tsf.2012.09.027
|
| [45] |
Mani S P, Rajendran N. Corrosion and interfacial contact resistance behavior of electrochemically nitrided 316L SS bipolar plates for proton exchange membrane fuel cells [J]. Energy, 2017, 133: 1050
doi: 10.1016/j.energy.2017.05.086
|
| [46] |
Fu Y, Lin G, Hou M, et al. Optimized Cr-nitride film on 316L stainless steel as proton exchange membrane fuel cell bipolar plate [J]. Int. J. Hydrogen Energy, 2009, 34: 453
doi: 10.1016/j.ijhydene.2008.09.104
|
| [47] |
Mendizabal L, Oedegaard A, Kongstein O E, et al. TaN x coatings deposited by HPPMS on SS316L bipolar plates for polymer electrolyte membrane fuel cells: Correlation between corrosion current, contact resistance and barrier oxide film formation [J]. Int. J. Hydrogen Energy, 2017, 42: 3259
doi: 10.1016/j.ijhydene.2017.01.070
|
| [48] |
Turner J A, Wang H L, Brady M P. Corrosion protection of metallic bipolar plates for fuel cells [R]. Golden: National Renewable Energy Lab. (NREL), 2005
|
| [49] |
Zhang D M, Duan L T, Guo L, et al. Corrosion behavior of TiN-coated stainless steel as bipolar plate for proton exchange membrane fuel cell [J]. Int. J. Hydrogen Energy, 2010, 35: 3721
doi: 10.1016/j.ijhydene.2010.01.043
|
| [50] |
Wang L X, Sun J C, Kang B, et al. Electrochemical behaviour and surface conductivity of niobium carbide-modified austenitic stainless steel bipolar plate [J]. J. Power Sources, 2014, 246: 775
doi: 10.1016/j.jpowsour.2013.08.025
|
| [51] |
Wang S L, Hou M, Zhao Q, et al. Ti/(Ti, Cr)N/CrN multilayer coated 316L stainless steel by arc ion plating as bipolar plates for proton exchange membrane fuel cells [J]. J. Energy Chem., 2017, 26: 168
doi: 10.1016/j.jechem.2016.09.004
|
| [52] |
Bi F F, Peng L F, Yi P Y, et al. Multilayered Zr-C/a-C film on stainless steel 316L as bipolar plates for proton exchange membrane fuel cells [J]. J. Power Sources, 2016, 314: 58
doi: 10.1016/j.jpowsour.2016.02.078
|
| [53] |
Allahkaram S R, Mohammadi N. Corrosion behavior of two candidate PEMFC's bipolar plate materials [J]. Anti-Corros. Methods Mater., 2017, 64: 293
doi: 10.1108/ACMM-05-2015-1540
|
| [54] |
Wu B, Lin G Q, Fu Y, et al. Chromium-containing carbon film on stainless steel as bipolar plates for proton exchange membrane fuel cells [J]. Int. J. Hydrogen Energy, 2010, 35: 13255
doi: 10.1016/j.ijhydene.2010.09.036
|
| [55] |
Fu Y, Lin G, Hou M, et al. Carbon-based films coated 316L stainless steel as bipolar plate for proton exchange membrane fuel cells [J]. Int. J. Hydrogen Energy, 2009, 34: 405
doi: 10.1016/j.ijhydene.2008.10.068
|
| [56] |
Ujiro T, Yoshioka K, Staehle R W. Differences in corrosion behavior of ferritic and austenitic stainless steels [J]. Corrosion, 1994, 50: 953
doi: 10.5006/1.3293487
|
| [57] |
Jun S, Hong Y B, Xin L, et al. The effect of copper and molybdenum on pitting corrosion and stress corrosion cracking behavior of ultra-pure ferritic stainless steels [J]. Corros. Sci., 2012, 57: 89
doi: 10.1016/j.corsci.2011.12.030
|
| [58] |
Wang H L, Turner J A. Ferritic stainless steels as bipolar plate material for polymer electrolyte membrane fuel cells [J]. J. Power Sources, 2004, 128: 193
doi: 10.1016/j.jpowsour.2003.09.075
|
| [59] |
ASTM. ASTM A240/A240M-08 Standard specification for chromium and chromium-nickel stainless steel plate, sheet, and strip for pressure vessels and for general applications [S]. West Conshohocken: ASTM, 2008
|
| [60] |
Kim K M, Kim S N, Kim J H, et al. Study on surface topography of 446M stainless steel as a bipolar plate on interfacial contact resistance of polymer electrolyte membrane fuel cell [J]. J. Power Sources, 2012, 220: 42
doi: 10.1016/j.jpowsour.2012.07.102
|
| [61] |
Kim J, Jo K, Kim Y, et al. Stainless steel for polymer fuel cell separator and method for preparing same [P]. U.S. Pat, 20110294042, 2011
|
| [62] |
Brady M P, Abd Elhamid M, Dadheech G, et al. Manufacturing and performance assessment of stamped, laser welded, and nitrided FeCrV stainless steel bipolar plates for proton exchange membrane fuel cells [J]. Int. J. Hydrogen Energy, 2013, 38: 4734
doi: 10.1016/j.ijhydene.2013.01.143
|
| [63] |
Moretti G, Quartarone G, Tassan A, et al. Pitting corrosion behavior of superferritic stainless steel in waters containing chloride [J]. Mater. Corros., 1993, 44: 24
|
| [64] |
Clayton C R, Lu Y C. A bipolar model of the passivity of stainless steel: The role of Mo addition [J]. J. Electrochem. Soc., 1986, 133: 2465
doi: 10.1149/1.2108451
|
| [65] |
Sun J L, Tang H J, Wang C L, et al. Effects of alloying elements and microstructure on stainless steel corrosion: A review [J]. Steel Res. Int., 2022, 93: 2100450
doi: 10.1002/srin.v93.5
|
| [66] |
Olsson C O A, Landolt D. Passive films on stainless steels—Chemistry, structure and growth [J]. Electrochim. Acta, 2003, 48: 1093
doi: 10.1016/S0013-4686(02)00841-1
|
| [67] |
Sun Y L, Xie Z P, Li Y W. Enhanced lithium storage performance of V2O5 with oxygen vacancy [J]. RSC Adv., 2018, 8: 39371
doi: 10.1039/C8RA07326K
|
| [68] |
Kim K M, Park J H, Kim J H, et al. Effect of chemical and heat treatment on the interfacial contact resistance and corrosion resistance of 446M ferritic stainless steel as a bipolar plate for polymer electrolyte membrane fuel cells [J]. Int. J. Hydrogen Energy, 2011, 36: 9926
doi: 10.1016/j.ijhydene.2011.05.091
|
| [69] |
Cui J L, Yao Z D, Cui Y F, et al. Electrochemical properties of tungsten-alloying-modified AISI 430 stainless steel as bipolar plates for PEMFCs used in marine environment [J]. Acta Metall. Sin. (Engl. Lett.), 2016, 29: 920
doi: 10.1007/s40195-016-0464-4
|
| [70] |
Wang H L, Turner J A, Li X N, et al. Process modification for coating SnO2: F on stainless steels for PEM fuel cell bipolar plates [J]. J. Power Sources, 2008, 178: 238
doi: 10.1016/j.jpowsour.2007.12.010
|
| [71] |
Luo H W, Lin X. Ferritic stainless steel for bipolar plate of fuel cell and preparation method of ferritic stainless steel [P]. Chin Pat, 202510151353.X, 2025
|
| [71] |
罗海文, 林 雄. 一种燃料电池双极板用铁素体不锈钢及其制备方法 [P]. 中国专利, 202510151353.X, 2025
|
|