| SiCf/TiAl复合材料界面反应及热稳定性 |
沈莹莹1,2, 张国兴1, 贾清1( ), 王玉敏1, 崔玉友1, 杨锐1( ) |
1.中国科学院金属研究所 师昌绪先进材料创新中心 沈阳 110016 2.中国科学技术大学 材料科学与工程学院 沈阳 110016 |
|
| Interfacial Reaction and Thermal Stability of the SiCf/TiAl Composites |
SHEN Yingying1,2, ZHANG Guoxing1, JIA Qing1( ), WANG Yumin1, CUI Yuyou1, YANG Rui1( ) |
1.Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2.School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China |
引用本文:
沈莹莹, 张国兴, 贾清, 王玉敏, 崔玉友, 杨锐. SiCf/TiAl复合材料界面反应及热稳定性[J]. 金属学报, 2022, 58(9): 1150-1158.
Yingying SHEN,
Guoxing ZHANG,
Qing JIA,
Yumin WANG,
Yuyou CUI,
Rui YANG.
Interfacial Reaction and Thermal Stability of the SiCf/TiAl Composites[J]. Acta Metall Sin, 2022, 58(9): 1150-1158.
| 1 |
Leyens C, Kocian F, Hausmann J, et al. Materials and design concepts for high performance compressor components [J]. Aerosp. Sci. Technol., 2003, 7: 201
doi: 10.1016/S1270-9638(02)00013-5
|
| 2 |
Wang Y M, Zhang G X, Zhang X, et al. Advances in SiC fiber reinforced titanium matrix composites [J]. Acta Metall. Sin., 2016, 52: 1153
|
| 2 |
王玉敏, 张国兴, 张 旭 等. 连续SiC纤维增强钛基复合材料研究进展 [J]. 金属学报, 2016, 52: 1153
doi: 10.11900/0412.1961.2016.00347
|
| 3 |
Ward-Close C M, Minor R, Doorbar P J. Intermetallic-matrix composites—A review [J]. Intermetallics, 1996, 4: 217
doi: 10.1016/0966-9795(95)00037-2
|
| 4 |
Beaumont P W R, Zweben C H. Comprehensive Composite Materials II [M]. 2nd Ed., Amsterdam: Elsevier, 2018: 482
|
| 5 |
Zhang Y G, Han Y F, Chen G L, et al. Structural Intermetallics [M]. Beijing: National Defense Industry Press, 2001: 686
|
| 5 |
张永刚, 韩雅芳, 陈国良 等. 金属间化合物结构材料 [M]. 北京: 国防工业出版社, 2001: 686
|
| 6 |
Dimiduk D M. Gamma titanium aluminide alloys—An assessment within the competition of aerospace structural materials [J]. Mater. Sci. Eng., 1999, A263: 281
|
| 7 |
Appel F, Brossmann U, Christoph U, et al. Recent progress in the development of gamma titanium aluminide alloys [J]. Adv. Eng. Mater., 2000, 2: 699
doi: 10.1002/1527-2648(200011)2:11<699::AID-ADEM699>3.0.CO;2-J
|
| 8 |
Yang R. Advances and challenges of TiAl base alloys [J]. Acta Metall. Sin., 2015, 51: 129
|
| 8 |
杨 锐. 钛铝金属间化合物的进展与挑战 [J]. 金属学报, 2015, 51: 129
|
| 9 |
Froes F H, Suryanarayana C, Eliezer D. Synthesis, properties and applications of titanium aluminides [J]. J. Mater. Sci., 1992, 27: 5113
doi: 10.1007/BF02403806
|
| 10 |
Bewlay B P, Nag S, Suzuki A, et al. TiAl alloys in commercial aircraft engines [J]. Mater. High Temp., 2016, 33: 549
doi: 10.1080/09603409.2016.1183068
|
| 11 |
Mah T, Hecht N L, McCullum D E, et al. Thermal stability of SiC fibres (Nicalon®) [J]. J. Mater. Sci., 1984, 19: 1191
doi: 10.1007/BF01120029
|
| 12 |
Dicarlo J A. Creep of chemically vapour deposited SiC fibres [J]. J. Mater. Sci., 1986, 21: 217
doi: 10.1007/BF01144723
|
| 13 |
Zhang X, Yang Q, Wang Y M, et al. Tensile property of SiCf/TC17 composite at room temperature [J]. Chin. J. Nonferrous Met., 2010, 20(spec.1) : s203
|
| 13 |
张 旭, 杨 青, 王玉敏 等. SiCf/TC17复合材料的室温拉伸性能 [J]. 中国有色金属学报, 2010, 20(专辑1) : s203
|
| 14 |
Ochiai S, Yagihashi M, Osamura K. Influence of interfacial reaction on tensile strength of SiC fiber embedded in a γ-titanium-aluminide alloy [J]. Intermetallics, 1994, 2: 1
doi: 10.1016/0966-9795(94)90045-0
|
| 15 |
Goo G K, Graves J A, Mecartney M L. Interfacial reaction of coated SiC fibers with gamma-TiAl [J]. Scr. Metall. Mater., 1992, 26: 1043
doi: 10.1016/0956-716X(92)90227-6
|
| 16 |
Djanarthany S, Viala J C, Bouix J. Development of SiC/TiAl composites: Processing and interfacial phenomena [J]. Mater. Sci. Eng., 2001, A300: 211
|
| 17 |
Zhang G X, Kang Q, Li G P, et al. Interfacial reaction of SiCf reinforced Ti-48Al-1.5Mn Matrix Composite [J]. Acta Metall. Sin., 2003, 39: 329
|
| 17 |
张国兴, 康 强, 李阁平 等. SiCf增强Ti-48Al-1.5Mn复合材料的界面反应 [J]. 金属学报, 2003, 39: 329
|
| 18 |
Zhang D, Sun Y B, Zhao Y Q, et al. Interfacial products in SiC fiber reinforced Ti-Al based intermetallic alloys [J]. Rare Met., 2011, 30: 524
doi: 10.1007/s12598-011-0338-x
|
| 19 |
Zhang W, Yang Y Q, Zhao G M, et al. Investigation of interfacial reaction in SiC fiber reinforced Ti-43Al-9V composites [J]. Intermetallics, 2013, 33: 54
doi: 10.1016/j.intermet.2012.09.025
|
| 20 |
Zhang W, Yang Y Q, Zhao G M, et al. Interfacial reaction studies of B4C-coated and C-coated SiC fiber reinforced Ti-43Al-9V composites [J]. Intermetallics, 2014, 50: 14
doi: 10.1016/j.intermet.2014.02.003
|
| 21 |
Zhang X, Wang Y M, Lei J F, et al. The interfacial thermal stability and element diffusion mechanism of SiCf/TC17 composite [J]. Acta Metall. Sin., 2012, 48: 1306
doi: 10.3724/SP.J.1037.2012.00347
|
| 21 |
张 旭, 王玉敏, 雷家峰 等. SiCf/TC17复合材料界面热稳定性及元素扩散机理 [J]. 金属学报, 2012, 48: 1306
|
| 22 |
Wang C, Zhang X, Wang Y M, et al. Mechanisms of interfacial reaction and matrix phase transition in SiCf/Ti65 composites [J]. Acta Metall. Sin., 2020, 56: 1275
|
| 22 |
王 超, 张 旭, 王玉敏 等. SiCf/Ti65复合材料界面反应与基体相变机理 [J]. 金属学报, 2020, 56: 1275
|
| 23 |
Zhu Y. Study on the interfacial reactions of SiC fiber reinforced Ti-matrix composites [D]. Xi'an: Northwestern Polytechnical University, 2003
|
| 23 |
朱 艳. SiC纤维增强Ti基复合材料界面反应研究 [D]. 西安: 西北工业大学, 2003
|
| 24 |
Xun Y W, Tan M J, Zhou J T. Processing and interface stability of SiC fiber reinforced Ti-15V-3Cr matrix composites [J]. J. Mater. Process. Technol., 2000, 102: 215
doi: 10.1016/S0924-0136(00)00473-8
|
| 25 |
Backhaus-Ricoult M. Physicochemical Processes at Metal-Creamic Interfaces [M]. Oxford: Pergamon Press, 1990: 79
|
| 26 |
Zhang X. Study on interface reaction, residual stress and mechanial properites of SiCf/TC17 composite [D]. Shenyang: University of Chinese Academy of Sciences (Institute of Metal Research, Chinese Academy of Sciences), 2012
|
| 26 |
张 旭. SiCf/TC17复合材料界面反应、残余应力及力学性能研究 [D]. 沈阳: 中国科学院大学(中国科学院金属研究所), 2012
|
| 27 |
Yang Y Q, Luo X, Huang B, et al. Characterizing interfacial reaction of SiC fiber-reinforced titanium-matrix composites [J]. Chin. J. Stereol. Image Anal., 2016, 21: 58
|
| 27 |
杨延清, 罗 贤, 黄 斌 等. SiC纤维增强Ti基复合材料的界面反应规律 [J]. 中国体视学与图像分析, 2016, 21: 58
|
| 28 |
Yang J M, Jeng S M. Interfacial reactions in titanium-matrix composites [J]. JOM, 1989, 41(11): 56
|
| 29 |
Wang X H, Zhou Y C. Solid-liquid reaction synthesis and simultaneous densification of polycrystalline Ti2AlC [J]. Z. Metallkd., 2002, 93: 66
doi: 10.3139/146.020066
|
| 30 |
Xie X. Preparation and characterization of textured Ti2AlC and Ti3AlC2 composites [D]. Shenyang: University of Science and Technology of China, 2020
|
| 30 |
谢 曦. 取向Ti2AlC和Ti3AlC2复合材料的制备和性能研究 [D]. 沈阳: 中国科学技术大学, 2020
|
|