| 基于中间过渡层的 5A06/0Cr18Ni10Ti 气化冲击焊接工艺研究 |
陈树君( ) |
1.北京工业大学汽车结构部件先进制造技术教育部工程研究中心 北京 100124
2.Impulse Manufacturing Laboratory, the Ohio State University, Columbus 43211, USA |
|
| Study on Vaporizing Foil Actuator Welding Process of 5A06/0Cr18Ni10Ti with Interlayer |
Shan SU( ) |
1.Engineering Research Center of Advanced Manufacturing Technology for Automotive Components, Ministry of Education, Beijing University of Technology, Beijing 100124, China
2. Impulse Manufacturing Laboratory, the Ohio State University, Columbus 43211, USA |
引用本文:
陈树君. 基于中间过渡层的 5A06/0Cr18Ni10Ti 气化冲击焊接工艺研究[J]. 金属学报, 2019, 55(8): 1041-1048.
Shan SU.
Study on Vaporizing Foil Actuator Welding Process of 5A06/0Cr18Ni10Ti with Interlayer[J]. Acta Metall Sin, 2019, 55(8): 1041-1048.
| [1] | Li Y J. Welding of Light Metals [M]. Beijing: National Defense Industry Press, 2011: 17 | | [1] | (李亚江. 轻金属焊接技术 [M]. 北京: 国防工业出版社, 2011: 17) | | [2] | Zhang H T, Liu J H, Feng J C. Effect of auxiliary TIG arc on formation and microstructures of aluminum alloy/stainless steel joints made by MIG welding-brazing process [J]. Trans. Nonferrous Met. Soc. China, 2014, 24: 2831 | | [3] | Shi Y, Wen J X, Huang J K, et al. Study on DE-GMAW MIG-brazing method for bonding steel with aluminum [J]. J. Mech. Eng., 2011, 47(16): 25 | | [3] | (石 玗, 温俊霞, 黄健康等. 基于旁路耦合电弧的铝钢MIG熔钎焊研究 [J]. 机械工程学报, 2011, 47(16): 25) | | [4] | Lv S X, Yang X D, Wan L, et al. Study on interfacial structure and mechanical properties of high frequency induction brazed joint of aluminum alloys to pre-coated stainless steel [J]. Trans. China Weld. Inst., 2017, 38(3): 22 | | [4] | (吕世雄, 杨旭东, 万 龙等. 预镀层不锈钢/铝异种金属高频感应钎焊接头界面及力学性能分析 [J]. 焊接学报, 2017, 38(3): 22) | | [5] | Ben-Artzy A, Stern A, Frage N, et al. Interface phenomena in aluminium-magnesium magnetic pulse welding [J]. Sci. Technol. Weld. Joining, 2008, 13: 402 | | [6] | Yu H P, Xu Z D, Li C F, et al. Experimental research on magnetic pulse joining of 3A21 aluminum alloy-20 steel tubes [J]. Acta Metall. Sin., 2011, 47: 197 | | [6] | (于海平, 徐志丹, 李春峰等. 3A21铝合金-20钢管磁脉冲连接实验研究 [J]. 金属学报, 2011, 47: 197) | | [7] | Wang T H, Sidhar H, Mishra R S, et al. Friction stir scribe welding technique for dissimilar joining of aluminium and galvanised steel [J]. Sci. Technol. Weld. Joining, 2018, 23: 249 | | [8] | Xue P, Zhang X X, Wu L H, et al. Research progress on friction stir welding and processing [J]. Acta Metall. Sin., 2016, 52: 1222 | | [8] | (薛 鹏, 张星星, 吴利辉等. 搅拌摩擦焊接与加工研究进展 [J]. 金属学报, 2016, 52: 1222) | | [9] | Dehghani M, Mousavi S A A A, Amadeh A. Effects of welding parameters and tool geometry on properties of 3003-H18 aluminum alloy to mild steel friction stir weld [J]. Trans. Nonferrous Met. Soc. China, 2013, 23: 1957 | | [10] | Winnicki M, Ma?achowska A, Korzeniowski M, et al. Aluminium to steel resistance spot welding with cold sprayed interlayer [J]. Surf. Eng., 2018, 34: 235 | | [11] | Han J H, Ahn J P, Shin M C. Effect of interlayer thickness on shear deformation behavior of AA5083 aluminum alloy/SS41 steel plates manufactured by explosive welding [J]. J. Mater. Sci., 2003, 38: 13 | | [12] | Zheng Y M. Explosion welding and dissimilar metals welding [J]. Weld. Technol., 2001, 30(5): 25 | | [12] | (郑远谋. 爆炸焊与异种金属的焊接 [J]. 焊接技术, 2001, 30(5): 25) | | [13] | Wang D W, Xiu S C. Effect of bonding temperature on the interfacial micro-structure and performance of mild steel/austenite stainless steel diffusion-bonded joint [J]. Acta Metall. Sin., 2017, 53: 567 | | [13] | (王大伟, 修世超. 焊接温度对碳钢/奥氏体不锈钢扩散焊接头界面组织及性能的影响 [J]. 金属学报, 2017, 53: 567) | | [14] | Pan F, Cui L, Qian W, et al. Microstructures and mechanical properties of dual-beam laser keyhole welded joints of aluminum alloys to stainless steels [J]. Acta Metall. Sin., 2016, 52: 1388 | | [14] | (潘 峰, 崔 丽, 钱 伟等. 铝合金/不锈钢双光束激光深熔焊接接头组织及力学性能 [J]. 金属学报, 2016, 52: 1388) | | [15] | Vivek A, Hansen S R, Liu B C, et al. Vaporizing foil actuator: A tool for collision welding [J]. J. Mater. Process. Technol., 2013, 213: 2304 | | [16] | Vivek A, Taber G A, Johnson J R, et al. Electrically driven plasma via vaporization of metallic conductors: A tool for impulse metal working [J]. J. Mater. Process. Technol., 2013, 213: 1311 | | [17] | Vivek A, Daehn G S. Vaporizing foil actuator: A versatile tool for high energy-rate metal working [J]. Procedia Eng., 2014, 81: 2129 | | [18] | Li X J, Ma H H, Shen Z W. Research on explosive welding of aluminum alloy to steel with dovetail grooves [J]. Mater. Des., 2015, 87: 815 | | [19] | Zhang Y, Babu S S, Prothe C, et al. Application of high velocity impact welding at varied different length scales [J]. J. Mater. Process. Technol., 2011, 211: 944 | | [20] | Vivek A, Brune R C, Hansen S R, et al. Vaporizing foil actuator used for impulse forming and embossing of titanium and aluminum alloys [J]. J. Mater. Process. Technol., 2014, 214: 865 | | [21] | Hahn M, Weddeling C, Taber G, et al. Vaporizing foil actuator welding as a competing technology to magnetic pulse welding [J]. J. Mater. Process. Technol., 2016, 230: 8 | | [22] | Liu B, Vivek A, Daehn G S. Joining sheet aluminum AA6061-T4 to cast magnesium AM60B by vaporizing foil actuator welding: Input energy, interface, and strength [J]. J. Manuf. Process., 2017, 30: 75 | | [23] | Liu B, Vivek A, Presley M, et al. Dissimilar impact welding of 6111-T4, 5052-H32 aluminum alloys to 22MnB5, DP980 steels and the structure-property relationship of a strongly bonded interface [J]. Metall. Mater. Trans., 2018, 49A: 899 | | [24] | Nassiri A, Zhang S Y, Lee T, et al. Numerical investigation of CP-Ti & Cu110 impact welding using smoothed particle hydrodynamics and arbitrary Lagrangian-Eulerian methods [J]. J. Manuf. Process., 2017, 28: 558 | | [25] | Vivek A, Liu B C, Hansen S R, et al. Accessing collision welding process window for titanium/copper welds with vaporizing foil actuators and grooved targets [J]. J. Mater. Process. Technol., 2014, 214: 1583 |
|
|