| Fe-BTC表面氨基化及对染料和重金属离子的吸附性能研究 |
曹梦薇,蔡桃,张霞( ) |
| 东北大学理学院 沈阳 110819 |
|
| Study on Amination Modification of Fe-BTC and Their Adsorption for Dyes and Heavy Metal Ions |
Mengwei CAO,Tao CAI,Xia ZHANG( ) |
| College of Sciences, Northeastern University, Shenyang 110819, China |
引用本文:
曹梦薇,蔡桃,张霞. Fe-BTC表面氨基化及对染料和重金属离子的吸附性能研究[J]. 金属学报, 2019, 55(7): 821-830.
Mengwei CAO,
Tao CAI,
Xia ZHANG.
Study on Amination Modification of Fe-BTC and Their Adsorption for Dyes and Heavy Metal Ions[J]. Acta Metall Sin, 2019, 55(7): 821-830.
| [1] | Gao Q, Xu J, Bu X H. Recent advances about metal-organic frameworks in the removal of pollutants from wastewater [J]. Coord. Chem. Rev., 2019, 378: 17 | | [2] | Ahmad A, Mohd-Setapar S H, Chuong C S, et al. Recent advances in new generation dye removal technologies: Novel search for approaches to reprocess wastewater [J]. RSC Adv., 2015, 5: 30801 | | [3] | Yagub M T, Sen T K, Afroze S, et al. Dye and its removal from aqueous solution by adsorption: A review [J]. Adv. Colloid Interface Sci., 2014, 209: 172 | | [4] | Kadirvelu K, Kavipriya M, Karthika C, et al. Utilization of various agricultural wastes for activated carbon preparation and application for the removal of dyes and metal ions from aqueous solutions [J]. Bioresourc. Technol., 2003, 87: 129 | | [5] | Wen J, Fang Y, Zeng G M. Progress and prospect of adsorptive removal of heavy metal ions from aqueous solution using metal-organic frameworks: A review of studies from the last decade [J]. Chemosphere, 2018, 201: 627 | | [6] | Sun D T, Peng L, Reeder W S, et al. Rapid, selective heavy metal removal from water by a metal-organic framework/polydopamine composite [J]. ACS Cent. Sci., 2018, 4: 349 | | [7] | Haque E, Lee J E, Jang I T, et al. Adsorptive removal of methyl orange from aqueous solution with metal-organic frameworks, porous chromium-benzenedicarboxylates [J]. J. Hazard. Mater., 2010, 181: 535 | | [8] | Bolto B, Gregory J. Organic polyelectrolytes in water treatment [J]. Water Res., 2007, 41: 2301 | | [9] | Savage N, Diallo M S. Nanomaterials and water purification: Opportunities and challenges [J]. J. Nanopart. Res., 2005, 7: 331 | | [10] | Cao Y, Li X B. Adsorption of graphene for the removal of inorganic pollutants in water purification: A review [J]. Adsorption, 2014, 20: 713 | | [11] | Dias J M, Alvim-Ferraz M C M, Almeida M F, et al. Waste materials for activated carbon preparation and its use in aqueous-phase treatment: A review [J]. J. Environ. Manage., 2007, 85: 833 | | [12] | Tao Y S, Kanoh H, Abrams L, et al. Mesopore-modified zeolites: Preparation, characterization, and applications [J]. Chem. Rev., 2006, 106: 896 | | [13] | Lee B, Kim Y, Lee H, et al. Synthesis of functionalized porous silicas via templating method as heavy metal ion adsorbents: The introduction of surface hydrophilicity onto the surface of adsorbents [J]. Micropor. Mesopor. Mater., 2001, 50: 77 | | [14] | Hua M, Zhang S J, Pan B C, et al. Heavy metal removal from water/wastewater by nanosized metal oxides: A review [J]. J. Hazard. Mater., 2012, 211-212: 317 | | [15] | Zhang W X, Liao P Q, Lin R B, et al. Metal cluster-based functional porous coordination polymers [J]. Coord. Chem. Rev, 2015, 293: 263 | | [16] | Eddaoudi M, Kim J, Rosi N, et al. Systematic design of pore size and functionality in isoreticular MOFs and their application in methane storage [J]. Science, 2002, 295: 469 | | [17] | Wu Y N, Zhou M M, Li S, et al. Magnetic metal-organic frameworks: γ-Fe2O3@ MOFs via confined in situ pyrolysis method for drug delivery [J]. Small, 2014, 10: 2927 | | [18] | Li Y W, Li J R, Wang L F, et al. Microporous metal-organic frameworks with open metal sites as sorbents for selective gas adsorption and fluorescence sensors for metal ions [J]. J. Mater. Chem., 2013, 1A: 495 | | [19] | Xu Y, Jin J J, Li X L, et al. Magnetization of a Cu (II)-1, 3, 5-benzenetricarboxylate metal-organic framework for efficient solid-phase extraction of Congo Red [J]. Microchim. Acta, 2015, 182: 2313 | | [20] | Haque E, Jun J W, Jhung S H. Adsorptive removal of methyl orange and methylene blue from aqueous solution with a metal-organic framework material, iron terephthalate (MOF-235) [J]. J. Hazard. Mater., 2011, 185: 507 | | [21] | Li Z Q, Yang J C, Sui K W, et al. Facile synthesis of metal-organic framework MOF-808 for arsenic removal [J]. Mater. Lett., 2015, 160: 412 | | [22] | Bai Z Q, Yuan L Y, Zhu L, et al. Introduction of amino groups into acid-resistant MOFs for enhanced U (VI) sorption [J]. J. Mater. Chem., 2015, 3A: 525 | | [23] | Luo X B, Ding L, Luo J M. Adsorptive removal of Pb (II) ions from aqueous samples with amino-functionalization of metal-organic frameworks MIL-101 (Cr) [J]. J. Chem. Eng. Data, 2015, 60: 1732 | | [24] | Martínez F, Leo P, Orcajo G, et al. Sustainable Fe-BTC catalyst for efficient removal of mehylene blue by advanced fenton oxidation[J]. Cataly. Today, 2018, 313: 6 | | [25] | Thommes M, Kaneko K, Neimark A V, et al. Physisorption of gases, with special reference to the evaluation of surface area and pore size distribution (IUPAC Technical Report) [J]. Pure Appl. Chem., 2015, 87: 1051 | | [26] | Ma W, Lv T F, Song X Y, et al. Characteristics of selective fluoride adsorption by biocarbon-Mg/Al layered double hydroxides composites from protein solutions: Kinetics and equilibrium isotherms study [J]. J. Hazard. Mater., 2014, 268: 166 | | [27] | Kumar K V, Sivanesan S. Comparison of linear and non-linear method in estimating the sorption isotherm parameters for safranin onto activated carbon [J]. J. Hazard. Mater., 2005, 123: 288 | | [28] | Quan X P, Sun Z Q, Meng H, et al. Polyethyleneimine (PEI) incorporated Cu-BTC composites: Extendedapplications in ultra-high efficient removal of congo red [J]. J. Solid State Chem., 2019, 270: 231 | | [29] | Namasivayam C, Kavitha D. Removal of Congo red from water by adsorption onto activated carbon prepared from coir pith, an agricultural solid waste [J]. Dyes Pigments, 2002, 54: 47 | | [30] | Masoomi M Y, Morsali A, Junk P C, et al. Ultrasonic assisted synthesis of two new coordination polymers and their applications as precursors for preparation of nano-materials [J]. Ultrason. Sonochem., 2017, 34: 984 | | [31] | Zhang X Q, Gao Y F, Liu H T, et al. Fabrication of porous metal-organic frameworks via a mixed-ligand strategy for highly selective and efficient dye adsorption in aqueous solution [J]. CrystEngComm., 2015, 17: 6037 | | [32] | Yang Q F, Wang Y, Wang J, et al. High effective adsorption/removal of illegal food dyes from contaminated aqueous solution by Zr-MOFs (UiO-67) [J]. Food Chem., 2018, 254: 241 | | [33] | Abdi J, Vossoughi M, Mahmoodi N M, et al. Synthesis of metal-organic framework hybrid nanocomposites based on GO and CNT with high adsorption capacity for dye removal [J]. Chem. Eng. J., 2017, 326: 1145 | | [34] | Xiao S L, Li Y H, Ma P J, et al. Synthesis and characterizations of two bis (benzimidazole)-based cobaltous coordination polymers with high adsorption capacity for congo red dye [J]. Inorg. Chem. Commun., 2013, 37: 54 | | [35] | Yang J M, Ying R J, Han C X, et al. Adsorptive removal of organic dyes from aqueous solution by a Zr-based metal-organic framework: Effects of Ce(III) doping [J]. Dalton Trans, 2018, 47: 3913 | | [36] | Saleem H, Rafique U, Davies R P. Investigations on post-synthetically modified UiO-66-NH2 for the adsorptive removal of heavy metal ions from aqueous solution [J]. Micropor. Mesopor. Mater., 2016, 221: 238 | | [37] | Yin N, Wang K, Li Z Q. Rapid microwave-promoted synthesis of Zr-MOFs: An efficient adsorbent for Pb (II) removal [J]. Chem. Lett., 2016, 45: 625 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|