| 再热恢复处理对蠕变损伤定向凝固高温合金γ′相的影响 |
唐文书( ),肖俊峰,李永君,张炯,高斯峰,南晴 |
| 1. 西安热工研究院有限公司 西安 710054 |
|
| Effect of Re-Heat Rejuvenation Treatment on γ′ Microstructure of Directionally SolidifiedSuperalloy Damaged by Creep |
Wenshu TANG( ),Junfeng XIAO,Yongjun LI,Jiong ZHANG,Sifeng GAO,Qing NAN |
| 1. Xi′an Thermal Power Research Institute Co., LTD., Xi′an 710054, China |
引用本文:
唐文书,肖俊峰,李永君,张炯,高斯峰,南晴. 再热恢复处理对蠕变损伤定向凝固高温合金γ′相的影响[J]. 金属学报, 2019, 55(5): 601-610.
Wenshu TANG,
Junfeng XIAO,
Yongjun LI,
Jiong ZHANG,
Sifeng GAO,
Qing NAN.
Effect of Re-Heat Rejuvenation Treatment on γ′ Microstructure of Directionally SolidifiedSuperalloy Damaged by Creep[J]. Acta Metall Sin, 2019, 55(5): 601-610.
| [1] | ZhangJ, LouL H, LiH. Material and processing technology of directionally solidified blade in heavy duty industrial gas turbines[J].Mater. China, 2013, 32: 12 | | [1] | (张 健, 楼琅洪, 李 辉. 重型燃气轮机定向结晶叶片的材料与制造工艺 [J]. 中国材料进展, 2013, 32: 12) | | [2] | FengQ, TongJ Y, ZhengY R, et al. Service induced degradation and rejuvenation of gas turbine blades[J].Mater. China, 2012, 31: 21 | | [2] | (冯 强, 童锦艳, 郑运荣等. 燃气涡轮叶片的服役损伤与修复 [J]. 中国材料进展, 2012, 31: 21) | | [3] | LiH, LouL H, ShiX J, et al. γ′coarsening and creep rupture property of DZ411(DSM11) superalloy [A]. High Temperature structure Material for Power and Energy: the Proceedings of 11th China's Superalloy[C]. Beijing: Metallurgical Industry Press, 2012: 392 | | [3] | (李 辉, 楼琅洪, 史学军, 等. DZ411(DSM11)合金γ′粗化与持久性能 [A]. 动力与能源用高温结构材料-第十一届中国高温合金年会论文集 [C]. 北京: 冶金出版社, 2012: 392) | | [4] | LeeB K, SongW Y, HanT K, et al. Change of microstructures of directionally solidified Ni base superalloy GTD-111 at high temperature[J]. Solid State Phenom., 2006, 118: 65 | | [5] | TawancyH M, Al-HadhramiL M. Comparative performance of turbine blades used in power generation: Damage vs. microstructure and superalloy composition selected for the application[J]. Eng. Fail. Anal., 2014, 46: 76 | | [6] | HosseiniS S, NateghS, EkramiA A. Microstructural evolution in damaged IN738LC alloy during various steps of rejuvenation heat treatments[J]. J. Alloys Compd., 2012, 512: 340 | | [7] | LvovaE, NorsworthyD. Influence of service-induced microstructural changes on the aging kinetics of rejuvenated Ni-based superalloy gas turbine blades[J]. J. Mater. Eng. Perform., 2001, 10: 299 | | [8] | JamesA. Review of rejuvenation process for nickel base superalloys[J]. Mater. Sci. Technol., 2001, 17: 481 | | [9] | LiburdiJ, LowdenP, NagyD, et al. Practical experience with the development of superalloy rejuvenation[A]. ASME Turbo Expo 2009: Power for Land, Sea, and Air[C]. Orlando: International Gas Turbine Institute, 2009, 4: 819 | | [10] | WangyaoP, HomkrajaiW, KrongtongV, et al. OM study of effect of HIP and heat treatments on microstructural restoration in cast nickel based superalloy, IN-738[J]. J. Met. Mater. Miner., 2017, 17: 87 | | [11] | ZhouY, ZhangZ, ZhaoZ H, et al. Effects of HIP temperature on the microstructural evolution and property restoration of a Ni-based superalloy[J]. J. Mater. Eng. Perform., 2013, 22: 215 | | [12] | WangyaoP, PolsilapaS, NisaratanapornE. The application of hot isostatic pressing process to rejuvenate serviced cast superalloy turbine blades[J]. Acta Metall. Slov., 2005, 11: 196 | | [13] | LindblomY. Refurbishing superalloy components for gas turbines[J]. Mater. Sci. Technol., 1985, 1: 636 | | [14] | BaldanA. Rejuvenation procedures to recover creep properties of nickel-base superalloys by heat treatment and hot isostatic pressing techniques[J]. J. Mater. Sci., 1991, 26: 3409 | | [15] | KimH I, ParkH S, KooJ M, et al. Microstructural investigation of GTD 111DS materials in the heat treatment conditions[J]. J. Mech. Sci. Technol., 2012, 26: 2019 | | [16] | GuoH M, ZhaoY S, ZhengS, et al. Effect of hot-isostatic pressing on microstructure and mechanical properties of second generation single crystal superalloy DD6[J]. J.Mater. Eng., 2016, 44(10): 60 | | [16] | (郭会明, 赵云松, 郑 帅等. 热等静压对第二代单晶高温合金DD6显微组织和力学性能的影响 [J]. 材料工程, 2016, 44(10): 60) | | [17] | RuttertB, BürgerD, RonceryL M, et al. Rejuvenation of creep resistance of a Ni-base single-crystal superalloy by hot isostatic pressing[J]. Mater. Des., 2017, 134: 418 | | [18] | McleanM, TiplerH R. Assessment of damage accumulation and propertiy regeneration by hot isostatic pressing and heat treatment of laboratory-tested and service exposed IN738LC[A]. Proceedings of Superalloys[C]. London: AIME, 1984: 73 | | [19] | PalJ, SrinivasanD, ChengE. Effect of rejuvenation heat treatment and aging on the microstructure evolution in Rene N5 single crystal Ni base superalloy blades [A]. Superalloys 2016: Proceedings of the 13th International Symposium on Superalloys[C]. Pennsylvania: TMS, 2016: 285 | | [20] | YaoZ, DegnanC C, JepsonM A E, et al. Effect of rejuvenation heat treatments on gamma prime distributions in a Ni based superalloy for power plant applications[J]. Mater. Sci. Tech., 2013, 29: 775 | | [21] | KuipersJ, WiensK, RuggieroB. Rejuvenation heat treatment of single crystal gas turbine blades [A]. ASME Turbo Expo 2017: Turbomachinery Technical Conference and Exposition[C]. Charlotte: International Gas Turbine Institute, 2017, 6: 1 | | [22] | CheruvuN S, SwaminathanV P, KinneyC D. Recovery of microstructure and mechanical properties of service run GTD-111 DS buckets [A]. ASME 1999 International Gas Turbine and Aeroengine Congress and Exhibition[C]. Indianapolis, Indiana: International Gas Turbine Institute, 1999, 4: 1 | | [23] | YooK B, LeeH S. The microstructure and mechanical properties of Ni-based superalloy after service exposure in gas turbine[J]. Mater. Sci. Forum, 2010, 654-656: 2523 | | [24] | LeeH S, KimD H, KimD S, et al. Microstructural changes by heat treatment for single crystal superalloy exposed at high temperature[J]. J. Alloys Compd., 2013, 561: 135 | | [25] | SemiatinS L, KrambR C, TurnerR E, et al. Analysis of the homogenization of a nickel-base superalloy[J]. Scr. Mater., 2004, 51: 491 | | [26] | NingL K, ZhengZ, JinT, et al. Effect of heat treatments on the microstructure and property of a new nickel base single crystal superalloy[J].Acta Metall. Sin., 2014, 50: 1011 | | [26] | (宁礼奎, 郑 志, 金 涛等. 热处理对一种新型镍基单晶高温合金组织与性能的影响 [J]. 金属学报, 2014, 50: 1011) | | [27] | ChenH, DongJ X, ZhangM C. Effect of heat treatment process on microstructure of cast superalloy K480[J].Trans. Mater. Heat Treat., 2012, 33(7): 37 | | [27] | (陈 昊, 董建新, 张麦仓. 热处理工艺对铸造高温合金K480组织的影响 [J]. 材料热处理学报, 2012, 33(7): 37) | | [28] | WuQ Y, ZhangJ H, SunX K, et al. Diffusion and solubilization of hydrogen in Ni-base single crystal superalloys[J].Acta Metall. Sin., 1996, 32: 938 | | [28] | (吴秋允, 张静华, 孙秀魁等. 氢在镍基单晶高温合金中的扩散和溶解 [J]. 金属学报, 1996, 32: 938) | | [29] | BaldanA. Review progress in ostwald ripening theories and their applications to nickel-base superalloys Part I: Ostwald ripening theories[J]. J. Mater. Sci., 2002, 37: 2171 | | [30] | KusabirakiK, NagahamaH, WangL, et al. The growth of γ′ precipitates in nickel-base superalloys[J].Tetsu Hagané, 1990, 76: 1341 | | [30] | 草開清志, 長浜秀信, 王 理等. ニッケル基合金に析出したγ'相の長 [J]. 鉄と鋼, 1990, 76: 1341 |
|
|