C和Nb含量对TP347HFG钢在650 ℃析出相参量和持久寿命的影响 |
彭志方1,党莹樱1,彭芳芳2 |
1. 武汉大学动力与机械学院, 武汉 430072
2. 东方锅炉(集团)有限公司材料研究所, 自贡643001 |
|
EFFECT OF CARBON AND NIOBIUM CONTENTS ON PHASE PARAMETERS AND CREEP RUPTURE TIME AT 650 ℃ FOR TP347HFG STEEL |
PENG Zhifang1, DANG Yingying1,PENG Fangfang2 |
1. School of Power and Mechanical Engineering, Wuhan University, Wuhan 430072
2. Materials Research Department, Dongfang Boiler Group Co. LTD., Zigong 643001 |
引用本文:
彭志方,党莹樱,彭芳芳. C和Nb含量对TP347HFG钢在650 ℃析出相参量和持久寿命的影响[J]. 金属学报, 2012, 48(4): 450-454.
,
,
.
EFFECT OF CARBON AND NIOBIUM CONTENTS ON PHASE PARAMETERS AND CREEP RUPTURE TIME AT 650 ℃ FOR TP347HFG STEEL[J]. Acta Metall Sin, 2012, 48(4): 450-454.
[1] Iseda A, Okada H, Semba H, Igarashi M. Energy Mater, 2007; 2: 199
[2] Yagi K, Merckling G, Kern T U, Irie H, Warlimont H. Creep Properties of Heat Resistant Steels and Superalloys.Berlin: Springer-Verlag, 2004: 249
[3] Erneman J, Schwind M, Andren H O, Nilsson J O, Wilson A,Agren J. Acta Mater, 2006; 54: 67
[4] Nilsson J O. Mater Sci Forum, 2007; 539-543: 4920
[5] Sourmail T. Mater Sci Technol, 2001; 17: 1
[6] Thorvaldsson T, Dunlop G L. Met Sci, 1980; 1: 513
[7] Laha K, Kyono J, Sasaki T, Kishimoto S, Shinya. Metall Mater Trans,2005; 36A: 399
[8] Thorvaldsson T, Dunlop G L. Met Sci, 1982; 16: 184
[9] Grot A S, Spruiell J E. Metall Trans, 1975; 6A: 2023
[10] Keown S R, Pickering F B. Creep Strength in Steel and High-Temperature Alloys. London: The Metals Society, 1974: 134
[11] Wadsworth J, Keown S R, Woodhead J H. Met Sci, 1976; 10: 105
[12] Adamson J M, Martin J W. J Iron Steel Inst, 1972; 210: 271
[13] Yu H Y, Dong J X, Xie X S. Chin J Mater Res, 2010; 24: 449
(于鸿垚, 董建新, 谢锡善.材料研究学报, 2010; 24: 449)
[14] Guo F Q, Cheng S C, Liu Z D, Bao H S, Zhang D M. Mater Mech Eng, 2007; 31: 11
(郭富强, 程世长, 刘正东, 包汉生, 张代明. 机械工程材料, 2007; 31: 11)
[15] Taneike M, Sawada K, Abe F. Metall Mater Trans, 2004; 35A: 1255
[16] Peng Z F, Yang Z G, Yan G Z, Chen S G, Zhou Y G. In: Academic Committees of the Superalloys, CSM ed., High-Temperature Structural Materials for Power and Energy Resource-Proc 11th Annual Chinese Conference on Superalloys, Shanghai: Metallurgical Industry Press, 2007: 666
(彭志方, 杨志刚, 阎光宗, 陈盛广, 周元贵. 见: 中国金属学会高温材料分会主编,动力与能源用高温结构材料-第11届中国高温合金年会论文集, 上海: 冶金工业出版社,2007: 666)
[17] Peng F F, Peng Z F, Chen F Y. In: Chinese Society for Electrical Engineering ed., Symposium on Sinicization of New Type Steels for 600 MW/1000 MW Ultra-Supercritical Units, Yangzhou: China Electric Power Journal Net, 2009: 175
(彭芳芳, 彭志方, 陈方玉. 见: 中国电机工程学会主编, 600 MW /1000 MW超超临界机组新型钢国产化研讨会报告文集, 扬州: 中国电力期刊网, 2009: 175)
[18] Peng Z F, Peng F F, Chen F Y. Electr Power Constr, 2009; 30(12): 1
(彭志方, 彭芳芳, 陈方玉. 电力建设, 2009; 30(12): 1)
[19] Peng Z F, Cai L S, Dang Y Y, Zhao L, Peng F F, Yang Z G, Yan G Z,Chen S G, Zhou J, Zhou Y G. Mater Sci Forum, 2011; 706-709: 2450
[20] Kuai C G, Peng Z F. Acta Metall Sin, 2008; 44: 897
(蒯春光, 彭志方. 金属学报, 2008; 44: 897) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|