| GH4738合金涡轮盘锻造过程的集成式模拟及应用* |
李林翰, 董建新, 张麦仓, 姚志浩( ) |
| 北京科技大学材料科学与工程学院, 北京 100083 |
|
| INTEGRATED SIMULATION OF THE FORGING PROCESS FOR GH4738 ALLOY TURBINE DISK AND ITS APPLICATION |
LI Linhan, DONG Jianxin, ZHANG Maicang, YAO Zhihao( ) |
| School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
李林翰, 董建新, 张麦仓, 姚志浩. GH4738合金涡轮盘锻造过程的集成式模拟及应用*[J]. 金属学报, 2014, 50(7): 821-831.
Linhan LI,
Jianxin DONG,
Maicang ZHANG,
Zhihao YAO.
INTEGRATED SIMULATION OF THE FORGING PROCESS FOR GH4738 ALLOY TURBINE DISK AND ITS APPLICATION[J]. Acta Metall Sin, 2014, 50(7): 821-831.
| [1] |
Chang K M, Liu X B. Mater Sci Eng, 2001; A308: 1
|
| [2] |
Whelchel R L, Kelekanjeri V S K G, Gerhardt R A, Ilavsky J. Metall Mater Trans, 2011; 42A: 1362
|
| [3] |
Yao Z H, Dong J X, Zhang M C, Zheng L. Rare Met Mater Eng, 2010; 39: 1565
|
| [3] |
(姚志浩, 董建新, 张麦仓, 郑 磊. 稀有金属材料与工程, 2010; 39: 1565)
|
| [4] |
Tong J, Vermeulen B. Int J Fatigue, 2003; 25: 413
|
| [5] |
Semiatin S L, Fagin P N, Glavicic M G. Scr Mater, 2004; 50: 625
|
| [6] |
Liu X B, Kang B, Chang K M. Mater Sci Eng, 2003; A340: 8
|
| [7] |
Tin S, Lee P D, Kermanpur A, Rist M, McLean M. Metall Mater Trans, 2005; 36A: 2493
|
| [8] |
Bertrand C, Cabrera J M, HerreroA, Mateos P, Prado J M. Mater Sci Forum, 1993; 113-115: 39
|
| [9] |
Łukaszek-Sołek A, Krawczyk J, Chyła P. J Alloys Compd, doi: 10.1016/j.jallcom.2013.12.070
|
| [10] |
Bramley A N, Mynors D J. Mater Des, 2000; 21: 279
|
| [11] |
de Jaeger J, Solas D, BaudinT, FandeurO, Schmitt J H, Rey C. In: Huron E S, Reed R C, Hardy M C, Mills M J, Montero R E, Portella P D, Telesman J eds., Superalloys 2012, Pennsylvania: TMS, 2012: 663
|
| [12] |
Dandre C A, Walsh C A, Evans R W, Reed R C, Roberts S M. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, McLean M, Olson S, Schirra J J eds., Superalloys 2000, Pennsylvania: TMS, 2000: 85
|
| [13] |
Sun M Y. PhD Dissertation, Graduate School of the Chinese Academy of Sciences, Beijing, 2009
|
| [13] |
(孙明月. 中国科学院研究生院博士学位论文, 北京, 2009)
|
| [14] |
Yao Z H, Dong J X, Zhang M C. Acta Metall Sin, 2011; 47: 1581
|
| [14] |
(姚志浩, 董建新, 张麦仓. 金属学报, 2011; 47: 1581)
|
| [15] |
Yao Z H, Wang Q Y, Zhang M C, Dong J X. Acta Metall Sin, 2011; 47: 1591
|
| [15] |
(姚志浩, 王秋雨, 张麦仓, 董建新. 金属学报, 2011; 47: 1591)
|
| [16] |
Shen G S, Semiatin S L, Shivpuri R. Metall Mater Trans, 1995; 26A: 1795
|
| [17] |
Zhang H Y, Zhang S H, Li Z X, Cheng M. J Eng Manuf, 2010; 224: 103
|
| [18] |
Cha D J, Kim D K, Cho J R, Bae W B. Int J Preci Eng Manuf, 2011; 12: 331
|
| [19] |
Shen G S, Furrer D. J Mater Process Technol, 2000; 98: 189
|
| [20] |
Shahriari D, Amiri A, Sadeghi M H, Cheraghzadeh M. Int J Mater Form, 2008; 1(Suppl 1): 29
|
| [21] |
Jeong H S, Cho J R, Park H C. J Mater Process Technol, 2005; 162-163: 504
|
| [22] |
Ma Q, Lin Z Q, Yu Z Q. Int J Adv Manuf Technol, 2009; 40: 253
|
| [23] |
China Aeronautical Materials Handbook Editorial Committee. China Aeronautical Materials Handbook. 2nd Ed., Vol.2, Beijing: China Standards Press, 2001: 475
|
| [23] |
(中国航空材料手册编辑委员会编. 中国航空材料手册(第二版)/第二卷. 北京: 中国标准出版社, 2001: 475)
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|