| 下贝氏体球墨铸铁在腐蚀介质中的磨粒磨损行为 |
孙挺, 宋仁伯( ), 杨富强, 李亚萍, 吴春京 |
| 北京科技大学材料科学与工程学院, 北京 100083 |
|
| ABRASIVE WEAR BEHAVIOR OF LOWER BAINITE DUCTILE IRON IN CORROSION MEDIA |
SUN Ting, SONG Renbo( ), YANG Fuqiang, LI Yaping, WU Chunjing |
| School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
孙挺, 宋仁伯, 杨富强, 李亚萍, 吴春京. 下贝氏体球墨铸铁在腐蚀介质中的磨粒磨损行为[J]. 金属学报, 2014, 50(11): 1327-1334.
Ting SUN,
Renbo SONG,
Fuqiang YANG,
Yaping LI,
Chunjing WU.
ABRASIVE WEAR BEHAVIOR OF LOWER BAINITE DUCTILE IRON IN CORROSION MEDIA[J]. Acta Metall Sin, 2014, 50(11): 1327-1334.
| [1] |
Labrecque C, Gagné M. Can Metall Quart, 1998; 37: 343
|
| [2] |
Pal S, Daniel W J T, Farjoo M. Int J Fatigue, 2013; 52: 144
|
| [3] |
Laino S, Sikora J A, Dommarco R C. Wear, 2008; 265: 1
|
| [4] |
Meena A, El Mansori M. Wear, 2011; 271: 2412
|
| [5] |
Reed P A S, Thomson R C, James J S, Putman D C, Lee K K, Gunn S R. Mater Sci Eng, 2003; A346: 273
|
| [6] |
Chaengkham P, Srichandr P. J Mater Process Technol, 2011; 211: 1372
|
| [7] |
Bakhtiari R, Ekrami A. Mater Sci Eng, 2009; A525: 159
|
| [8] |
Abbaszadeh K, Saghafian H, Kheirandish S. J Mater Sci Technol, 2012; 28: 336
|
| [9] |
Kutsov A, Taran Y, Uzlov K, Krimmel A, Evsyukov M. Mater Sci Eng, 1999; A273-275: 480
|
| [10] |
Abedi H R, Fareghi A, Saghafian H, Kheirandish S H. Wear, 2010; 268: 622
|
| [11] |
Slatter T, Lewis R, Jones A H. Wear, 2011; 271: 1481
|
| [12] |
Zhou Y, Lu Z, Zhan M. Mater Des, 2007; 28: 260
|
| [13] |
Efremenko V G, Shimizu K, Noguchi T, Efremenko A V, Chabak Y G. Wear, 2013; 305: 155
|
| [14] |
Lv Z L, Deng Y S, Rao Q C. Mater Mech Eng, 2011; 25(5): 32
|
| [14] |
(吕振林, 邓月声, 饶启昌. 机械工程材料, 2011; 25(5): 32)
|
| [15] |
Nie X, Meletis E I, Jiang J C, Leyland A, Yerokhin A L, Matthews A. Surf Coat Technol, 2002; 149: 245
|
| [16] |
Cheng X, Hu S, Song W, Xiong X S. Appl Surf Sci, 2013; 286: 334
|
| [17] |
Ji Y, Zhao W, Zhou M, Ma H R, Zeng P. Constr Build Mater, 2013; 47: 104
|
| [18] |
Mansfeld F. Corros Sci, 2005; 47: 3178
|
| [19] |
Dai P Q, He Z R, Mao Z Y. J Iron Steel Res, 2004; 13(6): 47
|
| [19] |
(戴品强, 何则荣, 毛志远. 钢铁研究学报, 2004; 13(6): 47)
|
| [20] |
Stokes B, Gao N, Reed P A S. Mater Sci Eng, 2007; A445-446: 374
|
| [21] |
Wu W Q. J Iron Steel Res, 2004; 16(5): 56
|
| [21] |
(吴维青. 钢铁研究学报, 2004; 16(5): 56)
|
| [22] |
Cavallini M, Di Bartolomeo O, Iacoviello F. Eng Fract Mech, 2008; 75: 694
|
| [23] |
Abareshi M, Emadoddin E. Mater Des, 2011; 32: 5099
|
| [24] |
Wang Y, Zhang K, Guo Z, Chen N L, Rong Y H. Mater Sci Eng, 2012; A552: 288
|
| [25] |
Zhang A F, Xing J D, Gao Y M, Su J Y. Acta Metall Sin, 2000; 36: 765
|
| [25] |
(张安峰, 邢建东, 高义民, 苏俊义. 金属学报, 2000; 36: 765)
|
| [26] |
Zhang P, Zhang F C, Yan Z G. Wear, 2011; 271: 697
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|