| 表面滚压对LZ50车轴钢疲劳短裂纹行为的影响 |
| 杨冰, 赵永翔 |
| 西南交通大学牵引动力国家重点实验室, 成都 610031 |
|
| INFLUENCE OF SURFACE ROLLING ON SHORT FATIGUE CRACK BEHAVIOR FOR LZ50 AXLE STEEL |
| YANG Bing, ZHAO Yongxiang |
| 西南交通大学牵引动力国家重点实验室, 成都 610031 |
引用本文:
杨冰 赵永翔. 表面滚压对LZ50车轴钢疲劳短裂纹行为的影响[J]. 金属学报, 2012, 48(8): 922-928.
.
INFLUENCE OF SURFACE ROLLING ON SHORT FATIGUE CRACK BEHAVIOR FOR LZ50 AXLE STEEL[J]. Acta Metall Sin, 2012, 48(8): 922-928.
| [1] Liu E Z, Zheng Z, Tong J, Ning L K, Guan X R. Acta Metall Sin, 2010; 46: 708(刘恩泽, 郑 志, 佟健, 宁礼奎, 管秀荣. 金属学报, 2010; 46: 708)[2] Hu Y H, Zhang Z, Zhong Q P, Han B C. J Mech Strength, 2009; 31: 979(胡燕慧, 张 峥, 钟群鹏, 韩邦成. 机械强度, 2009; 31: 979)[3] Suresh S, translated by Wang Z G. Fatigue of Materials. 2nd Ed, Beijing: National Defense Industry Press, 1999: 387(Suresh S著, 王中光译. 材料的疲劳. 第二版, 北京: 国防工业出版社, 1999: 387)[4] Pearson S. Eng Fract Mech, 1975; 7: 235[5] Maluf O, Milan M T, Spinelli D. J Mater Eng Perform, 2004; 13: 195[6] Ueji R, Tsuji N, Minamino Y. Acta Mater, 2002; 50: 4177[7] Mara N A, Sergueeva A V, Mara T D. Mater Sci Eng, 2007; A463: 238[8] Jia G W, Hua L, Mao H J. J Mater Process Technol, 2007; 187–188: 562[9] Ma B, Tieu A K, Lu C, Jiang Z. J Mater Process Technol, 2002; 125–126: 657[10] Yang B, Zhao Y X. Adv Mater Res, 2012; 463: 85[11] Zhao Y X, Gao Q, Wang J N. Acta Metall Sin, 2000; 36: 931(赵永翔, 高庆, 王金诺. 金属学报, 2000; 36: 931)[12] Zhao Y X, Gao Q, Wang J N. Acta Metall Sin, 2000; 36: 937(赵永翔, 高庆, 王金诺. 金属学报, 2000; 36: 937)[13] Zhao Y X, Yang B, Gao Q. Nucl Power Eng, 2003; 24: 127(赵永翔, 杨冰, 高庆. 核动力工程, 2003; 24: 127)[14] Zhao Y X, Yang B, Gao Q. Nucl Power Eng, 2005; 26:584(赵永翔, 杨冰, 高庆. 核动力工程, 2005; 26: 584)[15] Zhao Y X. PhD Thesis, Southwest Jiaotong University,Chengdu, 1998(赵永翔. 西南交通大学博士学位论文, 成都, 1998)[16] Zhao Y X, Gao Q, Wang J N. Fatigue Fract Eng Mater Struct, 1999; 22: 459[17] Miller K J. Fatigue Fract Eng Mater Struct, 1987; 10: 75[18] Miller K J. Fatigue Fract Eng Mater Struct, 1987; 10: 93[19] Obrtl´?k K, Pol´ak J, H´ajek M, Vaˇsek A. Int J Fatigue, 1997; 19: 471[20] Luo J, Bowen P. Int J Fatigue, 2004; 26: 113 [21] Ortiz J, Cisilino A P, Otegui J L. Fatigue Fract Eng Mater Struct, 2001; 24: 591[22] Ding C F, Liu J Z, Wu X R. J Aeronaut Mater, 2005; 25(6): 11(丁传富, 刘建中, 吴学仁. 航空材料学报, 2005; 25(6): 11)[23] Zhao Y X, Gao Q, Wang J N. Fatigue Fract Eng Mater Struct, 1999; 22: 469[24] Zhao Y X. J Mater Sci Technol, 2003; 19: 129[25] Yang B, Zhao Y X. Int J Fatigue, 2012; 35: 71[26] Yang B, Zhao Y X. Key Eng Mater, 2011; 474: 979[27] Yang B, Zhao Y X. Adv Mater Res, 2010; 118: 75[28] Zhao Y X, Sun Y F, Gao Q. J Mech Strength, 2001; 23: 102(赵永翔, 孙亚芳, 高庆. 机械强度, 2001; 23: 102) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|