| Mg-Zn-Y-Zr合金在NaCl溶液中的腐蚀行为 |
| 张亚丛, 王锦程, 吕文泉 |
| 西北工业大学凝固技术国家重点实验室, 西安 710072 |
|
| CORROSION BEHAVIOR OF Mg-Zn-Y-Zr ALLOYS IN NaCl SOLUTION |
| ZHANG Yacong, WANG Jincheng, LU Wenquan |
| State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072 |
引用本文:
张亚丛 王锦程 吕文泉. Mg-Zn-Y-Zr合金在NaCl溶液中的腐蚀行为[J]. 金属学报, 2011, 47(9): 1174-1180.
,
,
.
CORROSION BEHAVIOR OF Mg-Zn-Y-Zr ALLOYS IN NaCl SOLUTION[J]. Acta Metall Sin, 2011, 47(9): 1174-1180.
| [1] Li W X. Non–ferrous Metal Material Engineering Introduction. Beijing: Metallurgical Industry Press, 2007: 39(黎文献. 有色金属材料工程概论. 北京: 冶金工业出版社, 2007: 39)[2] Xu D K, Liu L, Xu Y B, Han E H. Acta Mater, 2008; 56: 985[3] Jia S C. PhD Thesis, Jilin University, 2006(贾素秋. 吉林大学博士学位论文, 2006)[4] Bae D H, Kim S H, Kim D H, Kim W T. Acta Mater, 2002; 50: 2343[5] Singh A, Nakamura A M, Watanabe M, Kato A, Tsai A P. Scr Mater, 2003; 49: 417[6] Popov I, Starosvetsky D, Shechtman D. J Mater Sci, 2000; 251: 1[7] Zhang E L, He W W, Du H, Yang K. Mater Sci Eng, 2008; A488: 102[8] Li Z J, Gu X N, Lou S Q, Zheng Y F. Biomaterials, 2008; 29: 1329[9] Song Y W, Shan D Y, Chen R S, Han E H. Corros Sci, 2010; 52: 1830[10] Zhang Y C, Wang J C, Zhang Q, L¨u W Q. Foundry Technol, 2010; 31: 1299(张亚丛, 王锦程, 张琪, 吕文泉. 铸造技术, 2010; 31: 1299)[11] Xu Y D, Hu S S, Zhu L P, Cheng F J, Zhu X R. Ordnance Mater Sci Eng, 2009; 32: 42(徐永东, 胡绳荪, 朱利萍, 程方杰, 朱秀荣. 兵器材料科学与工程, 2009; 32: 42)[12] Chang J W, Guo X W, Fu P H, Peng L M, Ding W J. Electrochim Acta, 2007; 52: 3160[13] Si L. Master Dissertation, Xi’an: Northwestern Polytechnical University, 2010(司林. 西安: 西北工业大学硕士学位论文, 2010)[14] Song G L, Atrens A, Dargusch M. Corros Sci, 1999; 41: 249[15] Xia L T, Gao S, Luo X P, Zang D M. Foundry, 2005; 15: 794(夏兰廷, 高珊, 罗小萍, 臧东勉. 铸造, 2005; 15: 794)[16] Chen X Y. Master Dissertation, Xi’an: Northwestern Polytechnical University, 2009(陈先毅. 西安: 西北工业大学硕士学位论文, 2009)[17] Lunder O, Lein J E, Aune T K, Nisancioglu K. Corrosion, 1989; 45: 74l |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|