纯Fe试样中晶粒的三维可视化重建 |
栾军华1), 刘国权1, 2), 王浩1) |
1) 北京科技大学材料科学与工程学院材料学系, 北京 100083
2) 北京科技大学新金属材料国家重点实验室, 北京 100083 |
|
THREE--DIMENSIONAL RECONSTRUCTION OF GRAINS IN PURE IRON SPECIMEN |
LUAN Junhua1), LIU Guoquan1,2), WANG Hao1) |
1) School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083
2) State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
栾军华 刘国权 王浩 . 纯Fe试样中晶粒的三维可视化重建[J]. 金属学报, 2011, 47(1): 69-73.
,
,
.
THREE--DIMENSIONAL RECONSTRUCTION OF GRAINS IN PURE IRON SPECIMEN[J]. Acta Metall Sin, 2011, 47(1): 69-73.
[1] Uchic M D, Kral M V, Spanos G, Dimiduk D M. Metall Mater Trans, 2004; 35A: 1925[2] MacPherson R D, Srolovitz D J. Nature, 2007; 446: 1053[3] von Neumann J. In: Herring C ed., Metal Interfaces. Cleveland: American Society for Metals, 1952: 108[4] Kinderlehrer D. Nature, 2007; 446: 995[5] Watanabe T. Mater Sci Forum, 2002; 408: 39[6] Watanabe T. Res Mech, 1984; 11: 47[7] Rohrer G S, Saylora D M, Dasherb B E, Adamsc B L, Rollett A D, Wynblatt P. Z Metall, 2004; 95: 197[8] Randle V, Rohrer G S, Miller H M, Coleman M, Owen G T. Acta Mater, 2008; 56: 2363[9] Fang X Y,WangWG, Rohrer G S, Zhou B X. Acta Metall Sin, 2010; 46: 404(方晓英, 王卫国, Rohrer G S, 周邦新. 金属学报, 2010; 46: 404)[10] Mishra S K, Pant P, Narasimhan K, Rollett A D, Samajdar I. Scr Mater, 2009; 61: 273[11] DeHoff R T. J Microsc, 1983; 131: 259[12] Holm E A, Duxbury P M. Scr Mater, 2006; 54: 1035[13] Desch C H. J Inst Met, 1919; 22: 241[14] Hull F C. Mater Sci Technol, 1988; 4: 778[15] Williams W M, Smith C S. Trans AIME, 1952; 194: 755[16] Rhines F N, Craig K R. Rousse Metal Trans, 1976; 7A: 1729[17] DeHoff R T, Liu G Q. Metall Trans, 1985; 16A: 2007[18] Sterio D C. J Microsc, 1985; 138: 127[19] Kral M V, Mangan M A, Spanos G, Rosenberg R O. Mater Charact, 2000; 45: 17[20] Wu K M. Acta Metall Sin, 2005; 41: 1237(吴开明. 金属学报, 2005; 41: 1237)[21] Wu K M, Enomoto M. Scr Mater, 2002; 46: 569[22] Chawla N, Sidhu R S, Ganesh V V. Acta Mater, 2006; 54: 1541[23] Dudek M A, Chawla N. Mater Charact, 2008; 59: 1364[24] Sharma H, Bohemen S M C, Petrov R H. Acta Mater, 2010; 58: 2399[25] Wu K M. Scr Mater, 2006; 54: 569[26] Dillon S J, Rohrer G S. In: Rollett A D ed., Proc 15th Int Conf Textures of Materials. Hoboken: John Wiley & Sons Pte Ltd, 2009: 117[27] Ghosh S, Bhandari Y, Groeber M. Computer–Aided Des, 2008; 40: 293[28] Groeber M, Ghosh S, Uchic M D, Dimiduk D M. Acta Mater, 2008; 56: 1257[29] Brahme A, Alvi M H, Saylor D, Fridyc J, Rollett A D. Scr Mater, 2006; 55: 75 |
|