| 9%-12%Cr铁素体耐热钢持久性能评估方法的研究 |
| 彭志方1; 党莹樱1;彭芳芳2 |
1.武汉大学动力与机械学院; 武汉 430072
2.东方锅炉(集团)股份有限公司材料研究所; 自贡 643001 |
|
| STUDY ON CREEP–RUPTURE PROPERTY ASSESSMENT METHOD FOR 9%—12%Cr FERRITIC HEAT–RESISTANT STEELS |
| PENG Zhifang1; DANG Yingying1; PENG Fangfang2 |
1.School of Power and Mechanical Engineering; Wuhan University; Wuhan 430072
2.Materials Research Department; Dong Fang Boiler Group Co. Ltd.; Zigong 643001 |
引用本文:
彭志方 党莹樱 彭芳芳. 9%-12%Cr铁素体耐热钢持久性能评估方法的研究[J]. 金属学报, 2010, 46(4): 435-443.
.
STUDY ON CREEP–RUPTURE PROPERTY ASSESSMENT METHOD FOR 9%—12%Cr FERRITIC HEAT–RESISTANT STEELS[J]. Acta Metall Sin, 2010, 46(4): 435-443.
| [1]Larson F R, Miller J. Trans ASME, 1952; 74: 765
[2]Orr R L, Sherby O DDorn H E. Trans ASM, 1954; 46: 113
[3]Kushima H, Kimura K, Abe F. Tetsu–to–Hagane, 1999; 85: 841
[4](九岛秀昭, 木村一弘, 阿部富士雄. 铁と钢, 1999; 85: 841)
[5]Lee J S, Armaki H G, Maruyama K, Muraki T, Asahi H. Mater Sci Eng, 2006; A428: 270
[6]Maruyama K, Yoshimi K. J Press Vessel Technol 2007, 129,449
[7]Armaki H G, Maruyama K, Yoshizawa K, Igarashi M. Mater Sci Eng, 2008; A490: 66
[8]Xiu Z L. The Performance & Strength Design and Engineering Application of High–temperature Metallic Materials. Beijing: Chemical Industry Press, 2006: 210
[9](徐自立. 高温金属材料的性能、强度设计及工程应用. 北京: 化学工业出版社, 2006: 210)
[10]Peng Z F, Cai L S, Peng F F, Hu Y P, Chen F Y. Acta Metall Sin, 2010; 46: 429
[11](彭志方, 蔡黎胜, 彭芳芳, 胡永平, 陈方玉. 金属学报,2010;46: 429)
[12]Zuo M, Chiovelli S, Nonaka Y. Trans ASME, 2000; 122:482
[13] Kimura K. NIMS Creep Data Sheet No. 51, 2006. http://tsuge.nims.go.jp/ top/creep.html
[14] Irie H. NIMS Creep Data Sheet No. 43, 1996. http://tsuge.nims.go.jp/ top/creep.html
[15] Motsulia S. NIMS Creep Data Sheet No. 48, 2002. http://tsuge.nims.go.jp/top/creep.html
[16]Maruyama K, Lee J S. In: Shibli I A, Holdsworth S R, eds., Creep and Fracture in High Temperature Components–Design and Life Assessment Issues, Lancaster, PA: DEStech Publications, 2005: 372
[17]Yoshizawa M, Igarashi M, Moriguchi M, Iseda A, Armaki H G, Maruyama K. Mater Sci Eng, 2009; A510–511: 162
[18]Wilshire B, Scharning P J, Hurst R. Mater Sci Eng, 2009; A510–511: 3
[19]Wilshire B, Scharning P J. Scr Mater 2007, 56,701
[20]Robertson D G. ECCC Data Sheets, 2005. http: //www.ommi.co.uk/etd/ecc/ advanced creep/index.html
[21]Yuan L. Therm Power Generation, 2009; 38(7): 10
[22](袁力. 热力发电, 2009; 38(7): 10) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|