| 冷却速率对GWZ1032K合金中14H-LPSO结构形成的影响 |
| 张松1,2,袁广银1,2,卢晨1,2,丁文江1,2 |
1.上海交通大学材料科学与工程学院 轻合金精密成型国家工程研究中心, 上海 200240
2.上海交通大学材料科学与工程学院 金属复合材料国家重点实验室, 上海 200240 |
|
| EFFECT OF COOLING RATE ON THE FORMATION OF 14H–LPSO STRUCTURE IN GWZ1032K ALLOY |
| ZHANG Song1,2, YUAN Guangyin1,2, LU Chen1,2, DING Wenjiang1,2 |
1. Light Alloy Net Forming National Engineering Research Center, School of Materials Science and Engineering, Shanghai
Jiao Tong University, Shanghai 200240
2, The State Key Laboratory of Metal Matrix Composite, School of Materials Science and Engineering, Shanghai
Jiao Tong University, Shanghai 200240 |
引用本文:
张松 袁广银 卢晨 丁文江. 冷却速率对GWZ1032K合金中14H-LPSO结构形成的影响[J]. 金属学报, 2010, 46(10): 1192-1199.
,
,
,
.
EFFECT OF COOLING RATE ON THE FORMATION OF 14H–LPSO STRUCTURE IN GWZ1032K ALLOY[J]. Acta Metall Sin, 2010, 46(10): 1192-1199.
| [1] Polmear I J. Mater Trans, 1996; 37: 12
[2] Froes F H, Eliezer D, Aghion E. JOM, 1998; 50: 30
[3] Kawamura Y, Hayashi K, Inoue A, Masumoto T. Mater Trans, 2001; 42: 1172
[4] Inoue A, Kawamura Y, Matsushita M, Hayashi K, Koike J. J Mater Res, 2001; 16: 1894
[5] Homma T, Kunito N, Kamado S. Scr Mater, 2009; 61: 644
[6] Kawamura Y, kasahara Y, Izumi S, Yamasaki M. Scr Mater, 2006; 55: 453
[7] YamasakiM, SasakiM, NishijimaM, Hiraga K, Kawamura Y. Acta Mater, 2007; 55: 6798
[8] Yamasaki M, Anan T, Yoshimoto S, Kawamura Y. Scr Mater, 2005; 53: 799
[9] Honma T, Ohkubo T, Kamado S, Hono K. Acta Mater, 2007; 55: 4137
[10] Wu Y J, Zeng X Q, Lin D L, Peng L M, Ding W J. J Alloys Compd, 2009; 477: 193
[11] Wu Y J, Lin D L, Zeng X Q, Peng L M, Ding W J. J Mater Sci, 2009; 44: 1607
[12] He S M, Zeng X Q, Peng L M, Guo X W, Chang J W, Ding W J. Mater Sci Forum, 2007; 101: 546
[13] Perminov V P. Powder Metall Met Ceram, 1967; 6: 409
[14] Liu X H, Johnson W L. J Appl Phys, 1995; 78: 6514
[15] Zhu Y M, Morton A J, Nie J F. Acta Mater, 2010; 58: 2936
[16] Itoi T, Seimiya T, Kawamura Y, Hirohashi M. Scr Mater, 2004; 51: 107
[17] Ping D H, Hono K, Kawamura Y, Inoue A. Philos Mag Lett, 2002; 82: 543
[18] Ping D H, Hono K, Nie J F. Scr Mater, 2003; 48: 1017
[19] Datta A, Waghmare U V, Ramamurty U. Acta Mater, 2009; 11: 2531
[20] Ding W J, Wu Y J, Peng L M, Zeng X Q, Yuan GY. J Mater Res, 2009; 24: 1842 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|