Pd粉及Pd91.31Y8.50Ru0.19合金膜的氚老化效应
陈淼1;陆光达2;张桂凯1;张延志1;王小英1;任大鹏2
1. 表面物理与化学国家重点实验室; 绵阳 621907
2. 中国工程物理研究院; 绵阳 621900
AGING EFFECTS OF TRITIUM ON Pd POWDERS AND Pd91.31Y8.50Ru0.19 ALLOY FILM
CHEN Miao1; LU Guangda2; ZHANG Guikai 1; ZHANG Yanzhi 1; WANG Xiaoying 1; REN Dapeng 2
1. National Key Laboratory for Surface Physical and Chemistry; Mianyang 621907
2. China Academy of Engineering Physics; Mianyang 621900
引用本文:

陈淼 陆光达 张桂凯 张延志 王小英 任大鹏. Pd粉及Pd91.31Y8.50Ru0.19合金膜的氚老化效应[J]. 金属学报, 2009, 45(10): 1277-1280.
, , , , , . AGING EFFECTS OF TRITIUM ON Pd POWDERS AND Pd91.31Y8.50Ru0.19 ALLOY FILM[J]. Acta Metall Sin, 2009, 45(10): 1277-1280.

全文: PDF(1208 KB)  
摘要: 

为了解Pd及其合金贮氚(T)老化后,  3He在材料中的存在形式及分布状态, 利用XRD与TEM分别分析了贮T老化1.6和3.5 a的Pd粉, 以及贮T老化41和295 d的Pd91.31Y8.50Ru0.19 合金膜的结构变化. 结果表明: T老化使得Pd粉的XRD峰变宽且峰强降低, 晶格发生畸变, 同时, 衍射峰略向低角度偏移, 晶格发生膨胀, 1.6和3.5 a老化后, 晶格常数分别增加0.095%和0.11%; 在老化41 d的Pd91.31Y8.50Ru0.19 合金膜中, 观察到分布均匀、直径约为1 nm的He泡, 同时存在高密度的位错及位错环, 在老化295 d的样品中, He泡直径略微增加, 达1.2-1.4 nm, 且分布均匀, 位错及位错环密度降低.

关键词 Pd Pd91.31Y8.50Ru0.19 氚老化 3He He泡    
Abstract

During tritium (T) treatment, Pd and its alloys will be aged due to solution of 3He, a product of T decay, in lattices, which changes the microstructure and properties of the materials. The existing and distributing states of 3He in Pd and Pd91.31Y8.50Ru0.19 alloy during T aging were studied by XRD and TEM. XRD results for Pd powders aged up to 1.6 and 3.5 a show that the peaks widen, intensities of peaks reduce and lattice constants incease by 0.095% and 0.11%, respectivey. TEM observtions show thaabout 1 nm sized He bubbls appear n Pd91.31Y8.50Ru0.19 alloy aged for 41 d, nd more dislocaions and dislocation loops arobserved; after 295 d aging, the He bubbles grow slightly and reach 1.2—1.4 nm in diameter, but the amounts of dislocations nd dslocation loops decrease.

Key wordsPd    Pd91.31Y8.50Ru0.19    tritium aging    3He    He bubble
收稿日期: 2008-10-30     
ZTFLH: 

TG146.41

 
作者简介: 陈淼, 男, 1983年生, 硕士生

[1] Hu Z L. Hydrogen Storage Material. Beijing: Chemical Industry Press, 2002: 32
(胡子龙. 贮氢材料. 北京: 化学工业出版社, 2002: 32)
[2] Lasser R. Tritium and Helium–3 in Metals. Berlin: Spring–Verlag, 1989: 34, 109
[3] Wileman R C J, Harris I R. J Less–Common Met, 1985; 109: 367
[4] Suzuki Y, Kimura S. Nucl Technol, 1993; 103: 93
[5] Luo D L, Shen C S, Meng D Q. Fusion Sci Technol, 2002; 41: 1142
[6] Evans J, Harris I R. J Less–Common Met, 1983; 89: 407
[7] Abell G C, Matson L K, Steinmeyer R H. Phys Rev, 1990; 41B: 1220
[8] Fabre A, Decamps B, Finot E, Penission J M, Demoment J, Thiebaut S, Contreras S, Percheron–Guegan A. J Nucl Mater, 2005; 342: 101
[9] Klevtsov V G, Boitsov I E, Vedeneev A I, Glagolev M V, Lobanov V N, Malkov I L, Pimanikhin S A, Stengach A V. Fusion Eng Des, 2000; 49–50: 873
[10] Tebus V, Rivkis L, Dmitrievskaia E, Arutunova G, Golikov I, Ryazantseva N, Filin V, Kapychev V, Bulkin V. J Nucl Mater, 2002; 307–311: 966
[11] Thiebaut S, Paul–Boncour V, Percheron–Gu´egan A, Limacher B, Blaschko O, Maaier C, Tailland C, Lerov D. Phys Rev, 1998; 57B: 10379
[12] Thomas G J, Mintz J M. J Nucl Mater, 1983; 116: 336
[13] Thiebaut S, Decamps B, P´enisson J M, Limacher B, Percheron–Guegan A. J Nucl Mater, 2000; 277: 217
[14] Wang P X, Song J S. Helium in Materials and the Permeation of Tritium. Beijing: National Defense Industry Press, 2002: 3
(王佩璇, 宋家树. 材料中的氦及氚的渗透. 北京: 国防工业出版社, 2002: 3)
[15] Wang L B, Lu M Q, Li Y Y. Acta Metall Sin, 2003; 39: 449
(王隆保, 吕曼祺, 李依依. 金属学报, 2003, 39: 449)

[1] 林鹏程, 庞玉华, 孙琦, 王航舵, 刘东, 张喆. 45钢块体超细晶棒材3D-SPD轧制法[J]. 金属学报, 2021, 57(5): 605-612.
[2] 屈硕硕,祝清省,巩亚东,杨玉莹,李财富,高世安. 高浓度、高性能Pd胶体的制备及其活化机理[J]. 金属学报, 2017, 53(4): 487-493.
[3] 文怀梁, 董俊华, 柯伟, 陈文娟, 阳靖峰, 陈楠. 模拟高放废物地质处置环境下重碳酸盐浓度对低碳钢活化/钝化腐蚀倾向的影响*[J]. 金属学报, 2014, 50(3): 275-284.
[4] 佟振峰 戴勇 杨文 杨启法. 辐照与He协同作用对低活度铁素体/马氏体钢F82H微观结构的影响[J]. 金属学报, 2011, 47(7): 965-970.
[5] 周圣银 胡锐 蒋力 李金山 寇宏超 常辉 周廉. 深过冷凝固Co80Pd20合金中的枝晶生长[J]. 金属学报, 2011, 47(4): 391-396.
[6] 徐亮 唐鋆磊 左禹. 不锈钢表面Cr-Pd合金电沉积及镀层在强还原性介质中的耐蚀性[J]. 金属学报, 2011, 47(2): 209-213.
[7] 黄火根 陈亮 李嵘 罗德礼. Ti36Zr40Ni20Pd4准晶的热稳定性与室温储氘性能[J]. 金属学报, 2010, 46(5): 629-633.
[8] 孔凡荣 张海鸥 王桂兰. 等离子沉积直接成形传热传质与晶粒生长多尺度数值模拟[J]. 金属学报, 2009, 45(4): 415-421.
[9] 黄火根 贾建平 李嵘. Pd替代对Ti-Zr-Ni准晶合金结构的影响[J]. 金属学报, 2009, 45(10): 1272-1276.
[10] 曹为民; 陈浩; 石新红; 朱律均; 姬学彬; 张磊 ; 印仁和 . Co/Pd纳米多层膜的制备及其磁性能[J]. 金属学报, 2008, 44(4): 445-450 .
[11] 王雨晨 . FCC金属钯中晶内滑移和晶界滑移的研究[J]. 金属学报, 2008, 44(3): 257-262 .
[12] 齐卫宏 . Pd纳米微粒的晶格参数和结合能的尺寸形状效应研究[J]. 金属学报, 2006, 42(10): 1065-1070 .
[13] 李猛进; 孙晓峰; 管恒荣; 姜晓霞; 胡壮麒 . (Ni, Pd)Al涂层的高温热腐蚀[J]. 金属学报, 2004, 40(7): 773-778 .
[14] 张文魁; 黄辉; 甘永平 . Pd/Y薄膜在气态吸放氢过程中的表面形貌和可转换光学特性[J]. 金属学报, 2003, 39(9): 974-978 .
[15] 李猛进; 孙晓峰; 管恒荣 . Pd-Ni-Al涂层的高温长期氧化行为[J]. 金属学报, 2003, 39(7): 755-760 .