| 2D Cf/Mg-2.0Re-0.2Zr复合材料的尺寸稳定性 |
| 宋美慧1;宋坚2;陈国钦1;王宁1;武高辉1 |
1 哈尔滨工业大学材料科学与工程学院; 哈尔滨 150001
2 中国空间技术研究院研究发展部; 北京 100094 |
|
| DIMENSIONAL STABILITY OF 2D Cf/Mg--2.0Re--0.2Zr COMPOSITES |
| SONG Meihui 1;SONG Jian2;CHEN Guoqin1;WANG Ning1; WU Gaohui1 |
1 College of Material Science & Engineering; Harbin Institute of Technology; Harbin 150001
2 Research and Development Department; Chinese Academy of Space Technology; Beijing 100094 |
引用本文:
宋美慧 宋坚 陈国钦 王宁 武高辉 . 2D Cf/Mg-2.0Re-0.2Zr复合材料的尺寸稳定性[J]. 金属学报, 2009, 45(1): 119-123.
,
,
,
,
.
DIMENSIONAL STABILITY OF 2D Cf/Mg--2.0Re--0.2Zr COMPOSITES[J]. Acta Metall Sin, 2009, 45(1): 119-123.
| [1] Li K, Pei Z L, Gong J, Shi N L, Sun C. Acta Metall Sin, 2007; 43: 1281
(李坤, 裴志亮, 宫骏, 石南林, 孙超. 金属学报, 2007; 43: 1281)
[2] Goddard D M. Trans Am Foundrymen′s Soc, 1986; 94: 667
[3] Degischer H P. Mater Des, 1997; 18: 221
[4] Armin F, Eckhard P, J¨org W. Adv Eng Mater, 2002; 2:471
[5] Goddard D M. Met Prog, 1984; 125: 49
[6] Carolin K, Wolgang S, Markus O, Robert F S. Adv Eng Mater, 2000; 6: 327
[7] Wu F, Zhu J. Acta Metall Sin, 1998; 34: 449
(武凤, 朱静. 金属学报, 1998; 34: 449)
[8] Hufenbach W, Andrich M, Langkamp A, Czulak A. J Mater Process Technol, 2006; 175: 218
[9] Russell S M, Todd R, Papakyriacou M. Surf Interface Anal, 2005; 37: 336
[10] Russell S M, Todd R, Papakyriacou M. Mater Sci Eng, 2005; A397: 249
[11] McCartney L N, Kelly A. Compos Sci Technol, 2007; 67: 646
[12] Kor´ab J, ˇStef´anik P, Kavecky ˇS, ˇSebo P, Korb G. Composites, 2002; 33A: 133
[13] ˇ Stef´anik P, Kavecky ˇ S, Korb G, Groboth G, ˇ Sebo P. J Mater Sci Lett, 1997; 16: 392
[14] Wolff E G, Min B K, Kural M H. J Mater Sci, 1985; 20: 1141
[15] Russell S M, Todd R I, Papakyriacou M. J Mater Sci, 2006; 41: 6228
[16] Korb G, Kor´ab J, Groboth G. Composites, 1998; 29A: 1563
[17] Wang H H, Li X G, Fei Z M. Aerosp Mater Technol, 1995; 25(1): 41
(王鸿华, 李贤淦, 费铸铭. 宇航材料工艺, 1995; 25(1): 41)
[18] Taylor R E. Int J Thermophys, 1991; 12: 723
[19] Hufenbach W, Andrich M, Langkamp A, Czulak A. J Mater Process Technol, 2006; 175: 218
[20] Rupnowski P, Gentz M, Sutter J K, Kumosa M. Composites, 2005; 36A: 327
[21] Wang N. Master Degree Dissertation, Harbin Institute of Technology, 2007
(王 \ \ 宁. 哈尔滨工业大学硕士学位论文, 2007)
[22] Rojstaczer S, Cohn D, Marom G. J Mater Sci Lett, 1985; 4: 1233
[23] Rajendra U, Chawla K K. Compos Sci Technol, 1994; 50: 13
[24] Karadeniz Z H, Kumlutas D. Compos Struct, 2007; 78: 1
[25] Kelly A, Stearn R J, McCartney L N. Compos Sci Technol, 2006; 66: 154
[26] Zhang Q, Wu G H, Jiang L T, Chen G Q. Mater Chem Phys, 2003; 81: 780 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|