| 基于全量理论的金属体积成形多步数值模拟 |
| 王鹏;董湘怀;傅立军 |
| 上海交通大学塑性成形工程系; 上海 200030 |
|
| MULTI-STEP NUMERICAL SIMULATION OF BULK METAL FORMING PROCESSES BASED ON DEFORMATION THEORY OF PLASTICITY |
| WANG Peng;DONG Xianghuai;FU Lijun |
| Department of Plasticity Technology; Shanghai Jiaotong University; Shanghai 200030 |
引用本文:
王鹏 董湘怀 傅立军. 基于全量理论的金属体积成形多步数值模拟[J]. 金属学报, 2009, 45(1): 124-128.
,
,
.
MULTI-STEP NUMERICAL SIMULATION OF BULK METAL FORMING PROCESSES BASED ON DEFORMATION THEORY OF PLASTICITY[J]. Acta Metall Sin, 2009, 45(1): 124-128.
| [1] Budiansky B. J Appl Mech, 1959; 26: 259
[2] Sewell M J. J Mech Phys Solids, 1974; 22: 469
[3] Levy S, Shih C F, Wilkinson J P D, Stine P, McWilson R C. ASTM STP 647, 1978: 238
[4] Guo Y Q, Bstoz J L, Detraux P. Int J Numer Methods Eng, 1990; 30: 1385
[5] Kim S H, Kim S H, Huh H. J Mater Process Technol, 2001; 113: 779
[6] Lee C H, Kobayashi S. J Eng Ind, 1973; 95: 865
[7] Rong L, Nie Z R, Zuo T Y. Acta Metall Sin, 2006; 42: 394
(荣莉, 聂祚仁, 左铁镛. 金属学报, 2006; 42: 394)
[8] Hodge P G, White G N, Providence R I. J Appl Mech, 1950; 17: 180
[9] Chung K, Alexandrov S. Appl Mech Rev, 2007; 60: 316
[10] Chung K, Richmond O. Int J Plast, 1993; 9: 907
[11] Richmonda O, Alexandrov S. J Mech Phys Solids, 2000; 48: 1735
[12] Chung K, Lee W, Richmond O, Alexandrov S. Int J Plast, 2005; 21: 1322
[13] Boisse P, Ladeveze P, Poss M, Rougee P. Int J Plast, 1991; 7: 65
[14] Abdali A, Benkrid K, Bussy P. J Mater Process Technol, 1996; 60: 255
[15] Jourdan F, Bussy P. Comput Meth Appl Mech Eng, 2000; 190: 1245
[16] Liu B S, Liu Y. J Plast Eng, 1999; 6(2): 17
(柳葆生, 刘渝. 塑性工程学报, 1999; 6(2):17)
[17] Simo J C, Ortiz M. Comput Meth Appl Mech Eng, 1985; 49: 221
[18] Brunig M. Comput Struct, 1998; 69: 117
[19] Wang P, Dong X H, Fu L J. J Plast Eng, 2008; 15(4): 72
(王鹏, 董湘怀, 傅立军. 塑性工程学报, 2008; 15(4): 72)
[20] Il′yushin A A. Plasticity. Moscow: Gostekhizdat Publishing, 1948
(Ильюшин А А. Пластичность Москва: Государственное Издательство Технико-Теоретической Литературы, 1948)
[21] Kobayashi S, Oh S I, Altan T. Metal Forming and the Finite–Element Method. New York: Oxford University Press Publishing, 1989: 86 |
|