| 氢在Gasar工艺常用纯金属中的溶解度 |
| 张华伟 李言祥 刘源 |
| 清华大学机械工程系; 先进成形制造教育部重点实验室; 北京 100084 |
|
| Hydrogen Solubility in Pure Metals for Gasar Process |
| Hua-Wei ZHANG;; |
| 先进成形制造教育部重点实验室;清华大学机械工程系 |
引用本文:
张华伟; 李言祥; 刘源 . 氢在Gasar工艺常用纯金属中的溶解度[J]. 金属学报, 2007, 43(2): 113-118 .
,
,
.
Hydrogen Solubility in Pure Metals for Gasar Process[J]. Acta Metall Sin, 2007, 43(2): 113-118 .
[1]et al.Translated by Huang L Y,Yan M S.Gas in Non-ferrous Metals and Alloys.Beijing:Metallurgical Industry Press,1989:126,75,65,68(等著.黄良余,严名山译.有色金属及其合金中的气体.北京:冶金工业出版社,1989:126,75,65,68) [2]Foundry Institute of Chinese Mechanical Engineering So-ciety.Foundry Handbook Vol.3 Non-ferrous Cast Alloys.Beijing:China Machine Press,1999:2,29(中国机械工程学会铸造专业学会.铸造手册,第3卷:铸造非铁合金.北京:机械工业出版社,1999:2,29) [3]Manchester F D.Phase Diagrams of Binary Hydrogen Alloys.Materials Park,Ohio:ASM International,2000:4,83,46 [4]Anyalebechi P N.Scr Metall Mater,1995;33:1209 [5]Dong R J.Principles of Cast Alloy Melting.Beijing:China Machine Press,1991:151(董若璟.铸造合金熔炼原理.北京:机械工业出版社,1991:151) [6]Lu W H,Li L S,Huang L Y.Cast Alloy & Melting.Beijing:China Machine Press,1996:303,306(陆文华,李隆盛,黄良余.铸造合金及其熔炼.北京:机械工业出版社,1996:303,306) [7]Talbot D E J,Anyalebechi P N.Mater Sci Technol J,1988;4:1 [8]Yin Z X.Light Met,2006;(1):53 (尹卓湘.轻金属,2006;(1):53) [9]Zhou J R.Questions and Answers about Melting and Casting of Aluminium Alloys.Beijing:Metallurgical Industry Press,1987:55(周家荣.铝合金熔铸问笞.北京:冶金工业出版社,1987:55) [10]Eichenauer W,Hattenbach K,Pebler A.Z Metallkd,1961;52:682 [11]Lin R Y,Hoch M.Metall Trans,1989;20A:1785 [12]Scully J R,Young G A Jr,Smith S W.Mater Sci Forum,2000;331-337:1583 [13]Ichimura M,Sasajima Y,Imabayashi M.Mater Trans,JIM,1991;32:1109 [14]Ichimura M,Katsuta H,Sasajima Y,Imabayashi M.J Phys Chem Solids,1988;49(10):1259 [15]Zhang C F,Gong J S,Huang X R,Wang K G.Purification & Modification of Liquid Metals.Shanghai:Shanghai Science and Technology Press,1989:60(张承甫,龚建森,黄杏蓉,王凯歌.液态金属的净化与变质.上海:上海科学技术出版社,1989:60) [16]Fromm E,Gebhardt E.Gase und Kohlenstoff in Metallen.(Gas and Carbon in Metals).Berlin:Springer-Verlag,1976 [17]Shapovalov V I,Semik A P,Timchenko A G.Russia Metallurgy.1993;(3):25 [18](?)vrelid E,Flφistand G B,Rosenqvist T,Bakke P,Engh T A.Scand J Metall,1998;27(3):133 [19]Nishimura C,Komaki M,Amano M.J Alloy Compds,1999;293(1):329 [20]Bakke P,Lauritzen J L,Engh T A,Oymo D.Light Metals.New Orlears,Louisiana,1991:1015 [21]Huang Y C,Watanabe T,Komatsu R.In:Saito T ed,Proc 4th Int Confn Vacuum Metall,Tokyo,Japan:The Iron and Steel Institute of Japan,1974:176 [22]San-Martin A,Manchester F D.Bull Alloy Phase Diagrams,1987;8(5):431 [23]Verbetsky V N,Mitrokhin S V.In:Lewis F A,Aladjem A eds,Diffusion and Defect Data,Part B:Solid State Phenomena,(Vol.73-75)Switzerland:Scitec Publications Ltd,2000:503 [24]Yamamura S,Shiota H,Murakami K.Mater Sci Eng,2001;A318:137 [25]Sokolov V M,Fedorenko I V.Int J Hydrogen Energy,1996;21:931 [26]Schenck H,Lange K W.Arch Eisenhüttenwes,1966;37:739 [27]Schürmann E,Sittard M,V(?)iker R.Z Metallkd,1987;78:457 [28]Brandes E A,Brook G B.Smithells Metals ReferenceBook.7th ed.,Boston:Butterworth-Heinemann Ltd,1992:12-5 [29]McLellan R B,Oates W A.Acta Metall,1973;21:181 [30]Staeford S W,McLellan R B.Acta Metall,1974;22:1463 [31]Robertson W M.Z Metallkd,1973;64:436 [32]Louthan M R,Donovan J A,Caskey G R.Acta Metall,1975;23:745 [33]Serdyuk N P,Trofimenko V V,Dukelskii Y M.Metally,1992;(5):201(1992;(5):201) [34]Lei Y Q.Chemicophysics of Casting Process.Beijing:New Times Press,1982:161(雷水泉.铸造过程物理化学.北京:新时代出版社,1982:161) [35]Svoboda J M et al.Zhu P Y etc.,trans.Gases in Cast Metals.Beijing:China Machine Press,1984:18(Svoboda J M等著.Zhu P Y等译.铸造金属中的气体北京:机械工业出版社,1984:18) [36]Shi L.Thermodynamics of Metals and Alloys.Beijing:China Machine Press,1992:166(石霖.合金热力学.北京:机械工业出版社,1992:166) [37]Frohberg M G,Anik S.Arch Eisenhüettenwesen,1984;55(2):45 [38]Da Silva J R G,McLellan R B.J Less-Common Met,1976;50(1):1 [39]Da Silva J R G,Stafford S W,McLellan R B.J Less Common Met,1976;49:407 [40]Kubaschewski O.Iron-Binary Phase Diagrams.Berlin:Springer-Verlag,1982:46 [41]Quick N R,Johnson H H.Acta Metall,1978;26:903 [42]Fujita F E.In:Oriani R A,Hirth J P,Smialowski M eds,Hydrogen Degradation of Ferrous Alloys,New Jersey:Noyes Publications,1985:1 [43]Zhang H W,Li Y X,Liu Y.Acta Metall Sin,2006;42:1165(张华伟,李言祥,刘源.金属学报,2006;42:1165) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|