| 热变形低碳钢中奥氏体静态再结晶介观尺度模拟 |
| 郑成武;兰勇军; 肖纳敏; 李殿中; 李依依 |
| 中国科学院金属研究所 |
|
| SIMULATION OF STATIC RECRYSTALLIZATION OF HOT DEFORMED AUSTENITE IN A LOW CABON STEEL ON MESOSCALE |
| 中国科学院金属研究所 |
引用本文:
郑成武; 兰勇军; 肖纳敏; 李殿中; 李依依 . 热变形低碳钢中奥氏体静态再结晶介观尺度模拟[J]. 金属学报, 2006, 42(5): 474-480 .
[1] Raabe D. Computational Materials Science. Weinheim: Wiley-VCH , 1998: 201 [2] Hesselbarth H W, Gobel I R. Acta Metall Mater, 1991; 39: 2135 [3] Marx V, Reher F R, Gottstein G. Acta Mater, 1999; 47: 1219 [4] Raabe D. Ann Rev Mater Res, 2002; 32: 53 [5] Goetz R L, Seetharaman V. Metall Mater Trans, 1998; 29A: 2307 [6] Ding R, Guo Z X. Acta Mater, 2001; 49: 3163 [7] Kroc J. Lect Note Comp Sci, 2002; 2329: 773 [8] Kugler G, Turk R. Acta Mater, 2004; 52: 4659 [9] Sun J H, Liu Y Z, Zhou L Y. Spec Steel, 2004; 25: 12 (孙景宏,刘雅政,周乐育.特殊钢,2004;25:12) [10] Dewri R, Chakraborti N. Model Simul Mater Sci Eng, 2005; 13: 173 [11] Doherty R D, Hughes D A, Humphreys F J, Jonas J J, Jensen D J, Kassner M E, King W E, McNelley T R, McQueen H J, Rollett A D. Mater Sci Eng, 1997; A238: 219 [12] Solas D E, Tome C N, Engler O, Wenk H R. Acta Mater, 2001: 49: 3791 [13] Choi S H, Cho J H. Mater Sci Eng, 2005; A405: 86 [14] Hill R, Rice J R. J Int Phys Solids, 2004; 20: 339 [15] Radhakrishnan B, Sarma G B, Zacharia T. Acta Mater, 1998; 46: 4415 [16] Raabe D, Becker R C. Model Simul Mater Sci Eng, 2000; 8: 445 [17] Humphreys F J. Mater Sci Forum, 2004; 467-470: 107 [18] Song X Y, Rettenmayr M, Muller C, Exner H E. Metall Mater Trans, 2001; 32A: 2199 [19] Davies C H J. Scr Mater, 1997; 36: 35 [20] Hutchinson W B. Int Met Rev, 1984; 29: 25 [21] Tong M M, Mo C L, Li D Z, Li Y Y. Chin J Mater Res, 2002; 16: 485 (佟铭明,莫春立,李殿中,李依依.材料研究学报,2002;16: 485) [22] Read W T, Shockley W. Phys Rev, 1950; 78: 275 [23] Hibbitt, Karlsson and Sorensen. Abaqus/Standard User's Manual, Vol.3, Pawtucket, RI, USA, 1999: 24.2.30-1 [24] Xiao N M, Yue Z F, Lan Y J, Tong M M, Li D Z. Acta Metall Sin, 2005; 41: 496 (肖纳敏,岳珠峰,兰勇军,佟铭明,李殿中.金属学报,2005; 41:496) [25] Lan Y J, Xiao N M, Li D Z, Li Y Y. Acta Mater, 2005; 53: 991 [26] Rollett A D. Prog Mater Sci, 1997; 42: 79 [27] Rios P R, Padilha A F. Mater Res, 2003; 6: 605 [28] Rollett A D, Srolovitz D J, Doherty R D, Anderson M P. Acta Metall Mater, 1989; 37: 627 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|