| 高温退火过程中铅合金晶界特征分布的演化 |
| 夏爽;周邦新;陈文觉;王卫国 |
| 上海大学材料研究所 |
|
| Evolution of Grain Boundary Character Distributions in Pb Alloy During High Temperature Annealing |
| Shuang Xia |
| 上海大学材料研究所 |
引用本文:
夏爽; 周邦新; 陈文觉; 王卫国 . 高温退火过程中铅合金晶界特征分布的演化[J]. 金属学报, 2006, 42(2): 129-133 .
,
,
,
.
Evolution of Grain Boundary Character Distributions in Pb Alloy During High Temperature Annealing[J]. Acta Metall Sin, 2006, 42(2): 129-133 .
[1] Watanabe T. Res Mech, 1984; 11(1): 47 [2] Randle V. The Role of the Coincidence Site Lattice in Grain Boundary Engineering. Cambridge: Cambridge University Press, 1996: 2 [3] Palumbo G, Erb U. MRS Bull, 1999; 24(11): 27 [4] Lee D S, Ryoo H S, Hwang S K. Mater Sci Eng, 2003; A345: 106 [5] Shimada M, Kokawa H, Wang Z J. Acta Mater, 2002; 50: 2331 [6] Lin P, Palumbo G, Erb U. Scr Metall Mater, 1995; 33: 1387 [7] Lehockey E M, Palumbo G, Lin P. Scr Mater, 1997; 36: 1211 [8] Spigarelli S, Cabibbo M, Evangelista E. Mater Sci Eng, 2003; A352: 93 [9] Lehockey E M, Palumbo G. Mater Sci Eng, 1997; A237: 168 [10] Lehockey E M, Palumbo G, Lin P. Scr Mater, 1998; 39: 353 [11] Lehockey E M, Brennenstuhl A M, Thompson I. Corros Sci, 2004; 46: 2383 [12] King W E, Schwartz A J. Scr Mater, 1998; 38: 449 [13] Palumbo G, Aust K T, Lehockey E M. Scr Mater, 1998; 38: 1685 [14] Mykura H. Grain-Boundary Structure and Kinetics. Metals Park, Ohio: American Society of Metals, 1980: 79! |
|
Viewed |
|
|
|