| SnCu钎料合金镀层钎焊连接机理及界面反应 |
| 黄 毅 王春青 赵振清 |
| (哈尔滨工业大学材料科学与工程学院微连接研究室; 哈尔滨 150001) |
|
引用本文:
黄毅; 王春青; 赵振清 . SnCu钎料合金镀层钎焊连接机理及界面反应[J]. 金属学报, 2005, 41(8): 881-885 .
[1] Sugiyama Y. Weld Int, 1989; 3(10): 700 [2] Hattori T, Sakai S, Sakamoto A, Fujiwara C. Weld J, 1994; 73: 233 [3] Kawas H, Takemoto T, Asano M, Kawakatsu I, Liu K. Weld J, 1989; 68: 396 [4] Tsao L C, Chiang M J, Lin W H, Cheng M D, Chuang T H. Mater Charact, 2002; 48: 341 [5] Humpston G, Sangha S-P-S, Jacobson D-M. Mater Sci Technol, 1995; 11: 1161 [6] Suzuki K, Kagayama M, Takeuchi Y. J Jpn Inst Light Met, 1993; 43: 533 (铃木鼎,加贺山宾,竹内庸.轻金属,1993;43:533) [7] Jacobson D-M, Humpston G, Sangha S-P-S. Weld J, 1996; 75(8): 243 [8] Zhang Q Y, Zhuang H S. Manual of Brazing and Soldering. Beijing: China Machine Press, 1999: 55 (张启运,庄鸿寿.钎焊手册.北京:机械工业出版社, 1999: 55) [9] Xu R D, Wang J L, Xue F Q, Han X Y, Guo Z C. Elec- troplat Finish, 2003; 22(3): 44 [10] Gu T R, Li W L. Surface Chemistry, Beijing: Science Press, 1994: 359 (顾惕人,李外郎.表面化学.北京:科学出版社, 1994:359) [11] Li K Y. Physical Chemistry of Interface and Colloid, Harbin: Harbin Institute of Technology Press, 1998: 85 (李葵英.界面与胶体的物理化学.哈尔滨:哈尔滨工业大学出 版社, 1998:85) [12] Zhou Y H, Hu Z Q, Jie W Q. Technics of Solidification. Beijing: China Machine Press, 1998: 77 (周尧和,胡壮麒,介万奇.凝固技术.北京:机械工业出版社, 1998:77) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|