| 零夹杂42CrMo高强钢的超长寿命疲劳性能 |
| 张继明 杨振国 张建锋 李广义 李守新 惠卫军 翁宇庆 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室; 沈阳 110016 |
|
引用本文:
张继明; 杨振国; 张建锋; 李广义; 李守新; 惠卫军; 翁宇庆 . 零夹杂42CrMo高强钢的超长寿命疲劳性能[J]. 金属学报, 2005, 41(2): 145-149 .
[1] Fukumoto S, Mitchell A. Proceeding of the 1991 VacuumMetallurgy Conference on the Melting and Processing ofSpecialty Materials I & SS, USA: Pittsburgh, 1991: 3 [2] Naito T, Ueda H, Kikuchi M. Met Trans, 1984; 15A: 1431 [3] Asami K, Sugiyama Y. Heat Treatment Technol Assoc,1985; 25: 147 [4] Murakami Y. In: Blom A F ed., Proceedings of the 8th International Fatigue Congress, EMAS, Stockholm, Sweden, June, 2002: 2927 [5] Hu C T, Tarn C L. Mater Sci Eng, 1989; A118: 25 [6] Rittel D, Roman I. Int J Fat, 1989; 111: 177 [7] Solberg J K. Mater Sci Eng, 1988; 101: 39 [8] Murakami Y. J Res Natl Inst Stand Technol, 1994; 99:345 [9] Atkinson H V, Shi G. Prog Mater Sci, 2003; 48: 457 [10] Zhang J M, Zhang J F, Yang Z G, Li S X, Hui W J, Weng Y Q. Ada Metall Sin, 2004; 40: 846(张继明,张建锋,杨振国,李守新,惠卫军,翁宇庆.金属学报,2004;40:846) [11] Li S X. The Mechanical Behavior of Ultra-fine Grained Steel, The Ultra-fine Grained Steel, Beijing: Metallurgical Industry Press, 2003: 891(李守新.超细晶钢的力学行为,超细晶钢.北京:冶金工业出版社,2003:891) [12] Yang Z G, Zhang J M, Li S X, Chu Z M, Hui W J, Weng Y Q. Acta Metall Sin, 2004; 40: 367(杨振国,张继明,李守新,褚作明,惠卫军,翁宇庆.金属学报,2004;40:367)> |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|