| (Ni, Pd)Al涂层的高温热腐蚀 |
| 李猛进 孙晓峰 管恒荣 姜晓霞 胡壮麒 |
| 中国科学院金属研究所高温合金研究部; 沈阳 110016 |
|
| HIGH TEMPERATURE HOT-CORROSION BEHAVIOR OF (Ni, Pd)Al COATING |
| LI Mengjin; SUN Xiaofeng; GUAN Hengrong; JIANG Xiaoxia; HU Zhuangqi |
| Superalloy Research Division; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
李猛进; 孙晓峰; 管恒荣; 姜晓霞; 胡壮麒 . (Ni, Pd)Al涂层的高温热腐蚀[J]. 金属学报, 2004, 40(7): 773-778 .
,
,
,
,
.
HIGH TEMPERATURE HOT-CORROSION BEHAVIOR OF (Ni, Pd)Al COATING[J]. Acta Metall Sin, 2004, 40(7): 773-778 .
[1] Vogel D. Determination of the Ductile to Brittle Transition Temperature of Platinum. Aluminide Gas Turbine Blade Coatings, NPS Thesis, Montery, CA, Sept. 1985 [2] Schneider K, Arnim H V, Grunling H W. Thin Solid Films, 1981; 84: 29 [3] Alperine S, Steinmetz P. Surf Coot Technol, 1990; 43/44: 347 [4] He D X, Guan H R, Sun X F, Jiang X X. Thin Solid Films, 2000; 376: 144 [5] Li M J, Sun X F, Guan H R, Jiang X X, Hu Z Q. Oxid Met, 2003; 59: 486 [6] Li M J, Sun X F, Guan H R, Jiang X X, Hu Z Q. Surf Coat Technol, 2003; 167: 106 [7] Bianco R. J Electrochem Soc, 1989; 136: 265 [8] Johnson J B, Nicholls J R, Hurst R C, Hancock P. Corros Sci, 1978; 18: 543 [9] Goward G W, Boone D H. Oxid Met, 1971; 3: 475 [10] Bornstein N S, DeCrescente M A. Metall Mater Trans,1971; 2: 2875 [11] Goebel J A, Pettit F S. Metall Mater Trans, 1970; 1: 1943 [12] Goebel J A, Pettit F S, Goward G W. Metall Mater Trans,1973; 4: 261 [13] Rapp R A, Goto K S. In: Brauntein J ed., Proc Fused Salts Symp Ⅱ, The Electrochem Soc, Princeton, 1979 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|