Please wait a minute...
金属学报  2004, Vol. 40 Issue (5): 537-540     
  论文 本期目录 | 过刊浏览 |
偏压对电弧离子镀沉积类金刚石膜的影响
邹友生; 汪伟;郑静地;孙超;黄荣芳;闻立时
中国科学院金属研究所; 沈阳 110016;中国科学院金属研究所沈阳材料科学国家(联合)实验室; 沈阳 110016
Influence of Bias Voltage on Diamond-Like Carbon Film Deposited by Arc Ion Plating
ZOU Yousheng; WANG Wei; ZHENG Jingdi; SUN Chao;HUANG Rongfang; WEN Lishi
Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016;Shenyang National Laboratory for Materials Science; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016
引用本文:

邹友生; 汪伟; 郑静地; 孙超; 黄荣芳; 闻立时 . 偏压对电弧离子镀沉积类金刚石膜的影响[J]. 金属学报, 2004, 40(5): 537-540 .
, , , , , . Influence of Bias Voltage on Diamond-Like Carbon Film Deposited by Arc Ion Plating[J]. Acta Metall Sin, 2004, 40(5): 537-540 .

全文: PDF(2599 KB)  
摘要: 采用电弧离子镀方法, 在Si(100)基底上沉积了类金刚石(DLC)膜. 用激光Raman谱和X射线 光电子能谱(XPS)对不同偏压下沉积的类金刚石膜的结构进行了分析. 结果表明, Raman谱的 D峰和G峰的强度之比ID/IG 随着脉冲负偏压的增加先减小后增大, sp3键含量随着负 偏压的增加先增加 后减小. 偏压为-200 V 时, ID/IG 值最小为0.70, sp3键含量最大为26.7%. 纳米压痕仪测量结果表明, 随着脉冲负偏压增加, 硬度和弹性模量先增加后下降. 偏压为-200 V 时, DLC膜的硬度 和弹性模量最大, 分别为30.8和250.1 GPa.
关键词 : 类金刚石膜,  电弧离子镀,  脉冲偏压    
Abstract:The microstructures of the diamond-like carbon (DLC) films deposited on Si (100) substrate by using arc ion plating (AIP) under different pulse bias voltage were characterized using Raman spectra and X-ray photoelectron spectra (XPS). The results show that the ratio ID/IG decreases and sp3 bond content increases with increasing pulse bias voltage firstly, and then the ratio ID/IG increases and sp3 bond content decreases after the pulse bias voltage exceeding -200 V. The minimal ratio ID/IG is 0.70 and the content of sp3 bond is 26.7% at the bias voltage of -200 V. The hardness and modulus determined by using nanoindentation technique increase and then decrease with increasing pulse bias voltage. The hardness and modulus of the DLC films obtained at bias voltage of -200 V reaches a maximum value of 30.8 and 250.1 GPa, respectively.
Key words: diamond-like carbon film    arc ion plating    pulse bias voltage
收稿日期: 2003-05-26     
ZTFLH:  O484.4  
[1] Martínez E, Aadújar J L, Polo M C, Esteve J, Robertson J, Milne W I. Diamond Relat Mater, 2001; 10:145
[2] Kteps I, Nicolaescu D, Stamatin I, Correia A, Gil A, Zlatkin A. Appl Surf Sci, 1999; 146:152
[3] Grill A. Diamond Relat Mater, 1999; 8:428
[4] Mei X X, Xu J, Ma T C. Acta Phys, 2002; 51:1875(梅显秀,徐军,马腾才.物理学报,2002:51:1875)
[5] Robertson J. Thin Solid Films, 1997; 296:61
[6] Wei Q, Narayan J. Int Mater Rev, 2000; 45(4) : 133
[7] Amaratunga G A J, Silva S R P. Appl Phys Lett, 1996; 68:2529
[8] Ronkainen H, Koskinen J, Varjus S, Holmberg K. Surf Coat Technot, 1999; 122:150
[9] Yagi H, Ide T, Toyota H, Mori Y. J Mater Res, 1998; 13: 1724
[10] Sheeja D, Tay B K, Yu L, Lau S P. Surf Coat Technol, 2002; 154:289
[11] Li X D, Bhushan B. Thin Solid Films, 1999; 355-356:330
[12] Huang R F, Chan C Y, Lee C H, Gong J, Lai K H, Lee C S, Li K Y, Wen L S, Sun C. Diamond Relat Mater, 2001; 10:1850
[13] Sheeja D, Tay B K, Lau S P, Shi X. Shi J, Li Y, Ding X, Liu E, Sun Z. Surf Coat Technol, 2000; 127:247
[14] Robertson J. Diamond Relat Mater, 1993; 2:984
[15] Tamor M A, Vassell W C. J Appl Phys, 1994; 76:3823
[16] Li L H, Zhang H Q, Cui X M, Zhang Y H, Xia L F, Ma X X, Sun Y. Acta Phys, 2001; 50:1549(李刘合,张海泉,崔旭明,张彦华,夏立芳,马欣新,孙跃.物理学报,2001;50:1549)
[17] Müller U, Hauert R, Oral B, Tobler M. Surf Coat Techol, 1995; 76-77:367
[18] Zhang W, Tanaka A, Wazumi K, Koga Y. Diamond Relat Mater, 2002; 11:1837
[19] Robertson J. Mater Sci Eng, 2002; 37R: 129
[1] 刘冠熙, 黄光宏, 罗学昆, 申造宇, 何利民, 李建平, 牟仁德. 表面喷丸处理对NiCrAlYSi涂层恒温氧化行为的影响[J]. 金属学报, 2021, 57(5): 684-692.
[2] 彭新, 姜肃猛, 孙旭东, 宫骏, 孙超. 梯度NiCoCrAlYSi涂层的循环氧化及热腐蚀行为*[J]. 金属学报, 2016, 52(5): 625-631.
[3] 韩克昌,刘一奇,林国强,董闯,邰凯平,姜辛. 宽固溶区过渡金属氮化物MNx (M=Ti, Zr, Hf)硬质薄膜原子尺度强化机制研究*[J]. 金属学报, 2016, 52(12): 1601-1609.
[4] 吴多利, 姜肃猛, 范其香, 宫骏, 孙超. 镍基高温合金Al-Cr涂层的恒温氧化行为*[J]. 金属学报, 2014, 50(10): 1170-1178.
[5] 于大千,卢旭阳,马军,姜肃猛,刘山川,宫骏,孙超. 梯度NiCrAlY涂层的1000和1100 ℃氧化行为研究[J]. 金属学报, 2012, 48(6): 759-768.
[6] 常正凯, 肖金泉, 陈育秋, 刘山川, 宫骏, 孙超. 电弧离子镀沉积磁性薄膜的研究[J]. 金属学报, 2012, 48(5): 547-554.
[7] 卢旭阳, 于大千, 姜肃猛, 刘山川,宫骏, 孙超. (NiCoCrAlYSiB+AlSiY)复合涂层热腐蚀行为的研究[J]. 金属学报, 2012, 48(4): 461-468.
[8] 时婧 裴志亮 宫骏 孙超 MUDERS C M 姜辛. Si含量对电弧离子镀Ti-Al-Si-N薄膜组织结构和力学性能的影响[J]. 金属学报, 2012, 48(11): 1349-1356.
[9] 王维新 姜肃猛 卫广智 马军 宫骏 孙超. NiCoCrAlYSiB+AlSiY梯度涂层恒温氧化行为[J]. 金属学报, 2011, 47(5): 578-586.
[10] 肖金泉 郎文昌 赵彦辉 宫骏 孙超 闻立时. 轴对称磁场对电弧离子镀TiN薄膜结构及摩擦性能的影响[J]. 金属学报, 2011, 47(5): 566-572.
[11] 杨巍 汪爱英 柯培玲 蒋百灵. 镁基表面微弧氧化/类金刚石膜的性能表征[J]. 金属学报, 2011, 47(12): 1535-1540.
[12] 董瑜亮 闫旭波 赵升升 宫骏 孙超. (Ti, Al)N/Ti2AlN涂层的制备[J]. 金属学报, 2010, 46(6): 743-747.
[13] 万先松 师玉英 马军 李海庆 宫骏 孙超. 电弧离子镀CrN涂层盐雾腐蚀行为[J]. 金属学报, 2010, 46(5): 600-606.
[14] 郎文昌 肖金泉 宫骏 孙超 黄荣芳 闻立时. 轴对称磁场对电弧离子镀弧斑运动的影响[J]. 金属学报, 2010, 46(3): 372-379.
[15] 吴博 李红凯 林国强 付宇 候明 衣宝廉. 不锈钢双极板电弧离子镀Cr1-xNx薄膜改性研究[J]. 金属学报, 2009, 45(9): 1125-1129.