| 电弧离子镀沉积Cr-O-N活性扩散阻挡层 |
| 王启民;郭明虎;柯培玲;孙超;黄荣芳;闻立时 |
| 中国科学院金属研究所金属腐蚀与防护国家重点实验室; 沈阳 110016 |
|
| Cr-O-N FILMS DEPOSITED BY ARC ION PLATING AS ACTIVE DIFFUSION BARRIERS |
| WANG Qimin; GUO Minghu; KE Peiling; SUN Chao; HUANG Rongfang; WEN Lishi |
| State Key Laboratory for Corrosion and Protection; Institute of Metal Research; |
引用本文:
王启民; 郭明虎; 柯培玲; 孙超; 黄荣芳; 闻立时 . 电弧离子镀沉积Cr-O-N活性扩散阻挡层[J]. 金属学报, 2004, 40(12): 1264-1268 .
,
,
,
,
,
.
Cr-O-N FILMS DEPOSITED BY ARC ION PLATING AS ACTIVE DIFFUSION BARRIERS[J]. Acta Metall Sin, 2004, 40(12): 1264-1268 .
[1] Rhys-Jones T N. Corros Sci, 1989; 29: 623 [2] Morral J E, Thompson M S. Surf Coat Technol, 1990;43/44:371 [3] Knotek O, Loffler F, Beele W. Surf Coat Technol, 1993;61: 6 [4] Cremer R,Witthaut M, Reichert K, Schierling M,Neuschutz D. Surf Coat Technol, 1998; 108/109: 48 [5] Reichert K. Surf Eng, 1999; 15: 163 [6] Muller J, Schierling M, Zimmermann E, Neuschiitz D.Surf Coat Technol, 1999; 120/121: 16 [7] Knotek O, Lugscheider E, Loffler F, Beeler W. Surf CoatTechnol, 1994; 68/69: 26 [8] Wang Q M, Wu Y N, Ji A L, Ke P L, Sun C, Huang R F,Wen L S. Ada Metall Sin, 2004; 40: 83 (王启民,武颖娜,纪爱玲,柯培玲,孙超,黄荣芳,闻立时. 金属学报,2004;40:83) [9] Liang Y J, Che Y C. Handbook of Thermodynamic Data for Inorganic Compounds. Shenyang: Northeast University Press, 1993 (梁英教,车荫昌.无机物热力学数据手册.沈阳:东北大学出 版社,1993) [10] Wang B, Song G H, Gong J, Sun C, Wen L S, Han Y F.Oxid Met, 2001; 56(1/2): 1 [11] Lou H Y. J Chin Soc Corros Prot, 1997; 17 (Suppl.): 464 (楼翰一.中国腐蚀与防护学报,1997;17(增刊):464) [12] Lou H Y, Wang F H. Vacuum, 1992; 43: 757) |
|