| 铸态Ti--Zr--Ni准晶基合金的室温力学性能 |
| 羌建兵;王英敏;袁力江 |
| 大连理工大学材料工程系 |
|
| Mechanical Properties Of The As--Cast Ti--Zr--Ni Bulk Quasicrystalline Alloys |
| QIANG Jianbing; WANG Yingmin; YUAN Lijiang |
| Department of Materials Engineering; Dalian University of Technology |
引用本文:
羌建兵; 王英敏; 袁力江 . 铸态Ti--Zr--Ni准晶基合金的室温力学性能[J]. 金属学报, 2004, 40(1): 62-66 .
,
,
.
Mechanical Properties Of The As--Cast Ti--Zr--Ni Bulk Quasicrystalline Alloys[J]. Acta Metall Sin, 2004, 40(1): 62-66 .
[1] Dubois J M. Mater Sci Eng, 2000; 294-296A: 4 [2] Nicula R, Jianu A, Ponkratz U, Burkel E. Phys Rev, 2000; 62B: 8844 [3] Ponkratz U, Nicula R, Jianu A, Burkel E. Ferroelectrics, 2001; 250:269 [4] Ponkratz U, Nicula R, Jianu A, Burkel E. J Phys, 2000;12:8071 [5] Foster K, Leisure R G, Shaklee J B, Kim J Y, Kelton K F. Phys Rev, 2000; 61B: 241 [6] Qiang J B, Wang Y M, Wang D H, Kramer M J, Dong C. J Non-Crystlline Solids, 2003; in Press [7] Qiang J B, Wang Y M, Wang D H, Kramer M J. Philos Mag Lett, 2003; 83:467 [8] Sigl L S, Mataga P A, Dalgleish B J, Meecking R M, Evans A G. Acta Metal Mater, 1988; 36:945 [9] Cahn J W, Shechtman D, Gratias D. J Mater Res, 1986; 1:13 [10] Bresson L. In: Hippert F, Gratias D eds., Lectures on Quasicrystals. Les Ulis: Les Editios de Physique, 1994: 549 [11] Koster U, Liebertz H, Liu W. Mater Sci Eng, 1994: 181-182A: 777 [12] Dong C. Quasicrystalline Materials. Beijing: National Defence Industry Press, 1998:159(董闯.准晶材料.北京:国防工业出版社,1998:159) [13] Zhang T, Inoue A. Mater Trans JIM, 1998; 39:1230 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|