| 老化化温度和老化时间对环氧酯漆涂层性能的影响 |
| 方丙炎 韩恩厚 王俭秋 |
| 中国科学院金属研究所 金属腐蚀与防护国家重点实验室 110016 |
|
引用本文:
方丙炎; 韩恩厚; 王俭秋 . 老化化温度和老化时间对环氧酯漆涂层性能的影响[J]. 金属学报, 2003, 39(5): 533-540 .
[1] Kendig M, Mansfeld F. Corrosion, 1983; 39: 466 [2] Mansfeld F. Corrosion, 1988; 44: 856 [3] Reinhard G, Rammelt V, Rammelt K. Corros Sci, 1986; 26: 109 [4] Skerry B S, Eden D A. Prog Org Coat, 1987; 15: 269 [5] Rammelt U, Reinhard G. Prog Org Coat, 1992; 21: 205 [6] Amirudin A, Thierry D. Prog Org Coat, 1995; 26: 1 [7] Brett C M A. J Appl Electrochem, 1990; 20: 1O00 [8] Mansfeld F, Kendig M, Tsai S. Corrosion, 1982; 38: 478 [9] Kendig M, Scully J. Corrosion, 1990; 46: 22 [10] Kendig M, Mansfeld F, Tsai S. Corros Sci, 1983, 23: 317 [11] Harhock M A, Lentz L A, Davis B L, Krishman K. Appll Spectrosc, 1986; 40: 210 [12] Skrovanek D J. J Coat Technol, 1989; 61: 31 [13] He D, Lei J Z, Hua X H. Aviation Paint and Coating Technol. Beijing: Chemical Industry Press, 2000: 52(何鼎,雷骏志,华信浩.航空涂料与涂装技术.北京:化学工业出版社,2000:52) [14] Fang B Y, Han E H, Wang J Q, Zhu Z Y, Ke W, Hu J P, Xu Z G. Corros Sci Prot Technol, in press(方丙炎,韩恩厚,王俭秋,朱自勇,柯伟,胡建平,徐志刚.腐蚀科学与防护技术,待发表) [15] Zhu J L, Wu S N. Pigment Technological Skill. Beijing: Chemical Industry Press, 1989: 252(朱骥良,吴申年.颜料工艺学.北京:化学工业出版社,1989:252) [16] Brasher M D, Kingsbury A H. J Appl Chem, 1954; 4. 62 [17] Armstrong R D, Wright J D. Electrochim Acta, 1799; 38: 1993 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|