| 低频机械谱术测量薄膜切变模量及微量油膜探测 |
| L.B.Magalas 方前锋 |
| AkademiaG6rniczo-Hutnicza;30-059Krak6w;Poland |
|
引用本文:
L.B.Magalas; 方前锋 . 低频机械谱术测量薄膜切变模量及微量油膜探测[J]. 金属学报, 2003, 39(11): 1228-1232 .
[1] Li Z S, Fang Q F, Veprek S, Li S Z. Rev Sci Instrum, 2003;74: 2477 [2] Magalas L B, Malinowski T. Solid State Phenom, 2003;89: 349 [3] Magalas L B, Malinowski T. Solid State Phenom, 2003;89: 247 [4] Magalas L B. J Alloy Compd, 2000; 310: 269 [5] Mencik J, Munz D, Quandt E, Ludwig A. Z Metallkd,1999; 90: 766 [6] Magalas L B, Kwasniewski J. Solid State Phenom, 2003;89: 355 [7] Magalas L B, Etienne S, David L, Malinowski T. Solid State Phenom, 2003; 89: 321 [8] Magalas L B, Malinowski T, Etienne S, David L, Kostro J. Non-Destr Test, 2000; 5: 223(Warsaw: SIMP, Poland, 2000) [9] Magalas L B, Etienne S, David L. Non-Destr Test, 2002;7: 257(Warsaw: SIMP, Poland, 2002) [10] Magalas L B. Ada Metall Sin, 2003; 39: 1145(Magalas L B.金属学报,20030;39:1145) |
|