| 用球滚接触疲劳法评定硬质薄膜的结合强度 |
| 朱晓东 黄鹤 胡奈赛 何家文 |
| 西安交通大学金属材料强度国家重点实验室; 西安 710049 |
|
引用本文:
朱晓东; 黄鹤; 胡奈赛; 何家文 . 用球滚接触疲劳法评定硬质薄膜的结合强度[J]. 金属学报, 1999, 35(5): 523-526 .
[1] Van J, Vac J. Set Technol, 1986: A4, 3007 [2] Zheng S L, He J W, Zhang P Y, Zhang X S. Thin Film SetTechnol, 1993; 6(2): 85(郑森林,何家文,张平余,张绪寿,薄膜科学与技术, 1993;6(2).85) [3] Cheng H S, Chang T P, Sproal W D. Mechanics of CoatingsTribologg Series 17, 1990: 81 [4] He J W, Hendrix B C, Hu N S, Wa K W, Bell T, Sun Y,Mao K. Scarce Eng, 1996; 12(1): 49 [5] Hu N S, Xu K W, He J W. China Suffoce Egg, 1998: 11(1).33(胡奈赛,徐可为,何家文.中国表面工程, 1998; 11(1): 33) [6] Chen W T. Int J Egg Sc2, 1971; 9, 775 [71 Xu K W, Bat C D, He J W. Acta Metall Sin, 1995; 31B: 429(徐可为,白辰东,何家文,金属学报,1995, 31B. 429) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |