| 非比例加载下Zr-4合金的宏观响应及其微观机理 |
| 肖林;匡震邦 |
| 西安交通大学金属材料强度国家重点实验室;西安;710049;上海交通大学工程力学系;上海;200030 |
|
| MACROSCOPIC RESPONSE AND MICROSCOPIC MECHANISM OF ZIRCALOY-4 UNDER NONPROPORTIONAL LOADING |
| XIAO Lin(State Key Laboratory for Mechanical Behaviour of Materials; Xi'an Jiaotong University; Xi'an 710049)KUANG Zhenbang(Department of Engineering Mechanics; Shanghai Jiaotong University; Shanghai 200030) |
引用本文:
肖林;匡震邦. 非比例加载下Zr-4合金的宏观响应及其微观机理[J]. 金属学报, 1998, 34(3): 242-248.
,
.
MACROSCOPIC RESPONSE AND MICROSCOPIC MECHANISM OF ZIRCALOY-4 UNDER NONPROPORTIONAL LOADING[J]. Acta Metall Sin, 1998, 34(3): 242-248.
1 著,吕允文,高绣雯译核工程材料北京:原子能出版社,1987write, Lu Yunwen, Gao Xiuwen translate. Materiais in NuclearEngineeriny. Beijing: Atom Publisher, 1987) 2肖林.复合加载下材料塑性变形行为及其微观机理西安交通大学博士后研究报告,1996(Xiao Lin. Plastic Deformation Behavior and Mcroscopic Mechanism of Materials Under Combined Loading. Postdoctor Thesis, Xi'an Jiaotong University, 1996) 3 Valanis K C. Areh Mech, 1980; 32:171 4 Xiao Lin, Kuang Zhenbang. Acta Maten 1996; 44: 3059 5 Doong S H, Socie D F, Robertson I M. ASME J Eng Mater Technol, 1990; 112: 456 6 McDowell D L. J Mech Phys Solids, 1985; 33: 559 7 Doong S H, Socie D F. ASME i Eny Mater Technol, 1991; 113: 23 8 肖林. 中国钼业,1997; 21: 30(Xiao Lin. Chin Molybdenum Ind, 1997; 21: 30) 9 Xiao Lin, Gu Haicheng, Kuang Zhenbang. Acta Metall Sin (Engl Lett), 1995; 8: 219 10 Xiso Lin, Gu Haicheng. Scr Metall Mater, 1994; 30: 175 11 Xiso Lin, Gu Haicheng. Metall Mater Trans, 1997; 28A: 1021 12 Miura S, Umeda K. Scr Metall, 1973; 7: 337 |
|