| Ni-NbC合金中强化相的形核与分支特点 |
| 李顺朴;赵德乾;陈熙琛 |
| 中国科学院物理研究所 |
|
| CHARACTER OF NUCLEATION AND BRANCHING OF STRENGTHENING PHASE IN Ni-NbC ALLOYS |
| LI Shunpu; (Institute of Physics; Chinese Academy of Sciences; Beijing 100080) ZHAO Deqian; CHEN Xichen (Institute of Physics; Chinese Academy of Sciences; Beijing 100080); BARABASH O M; OSHKADEROV S P (Institute of Metal Physics; Academia Sinica. Kiev; Ukraine 252142) |
引用本文:
李顺朴;赵德乾;陈熙琛. Ni-NbC合金中强化相的形核与分支特点[J]. 金属学报, 1995, 31(9): 405-410.
,
,
.
CHARACTER OF NUCLEATION AND BRANCHING OF STRENGTHENING PHASE IN Ni-NbC ALLOYS[J]. Acta Metall Sin, 1995, 31(9): 405-410.
| 1ShamsuzzohaM,HoganLM.JCrystalGrowth,1986;76:4292ShamsuzzohaM,HoganLM.JCrystalGrowth,1985;72:7353KobayashiK,HoganLM.JMatSci,1985:20:196641961:355李顺朴,陈熙琛,OM.科学通报,1995:40:(1)109 |
|