| 稀土元素在Al中固溶度亚稳扩展研究 |
| 宁远涛;周新铭;戴红 |
| 昆明贵金属研究所;昆明贵金属研究所;昆明贵金属研究所 |
|
| METASTABLE EXTENSION OF SOLID SOLUBILITY OF RARE EARTH ELEMENTS IN Al |
| NING Yuantao;ZHOU Xinming;DAI Hong Institute of Precious Metals; Kunming |
引用本文:
宁远涛;周新铭;戴红. 稀土元素在Al中固溶度亚稳扩展研究[J]. 金属学报, 1992, 28(3): 49-54.
,
,
.
METASTABLE EXTENSION OF SOLID SOLUBILITY OF RARE EARTH ELEMENTS IN Al[J]. Acta Metall Sin, 1992, 28(3): 49-54.
1 Falkenhagen G, Hofmann W. Z Metallk, 1952; 43: 69 2 Duwez P, Willens R H, Klement W Jr. J Appl Phys, 1960; 31: 1136 3 Anantharaman T R, Ramachandrarao P, Suryanarayana C, Lele S, Chattopadhyay K. Trans Indian Inst Met, 1977; 30: 423 4 Jones H. Aluminium, 1978; 54: 274 5 Ning Yuantao, Zhou Xinming, Dai Hong. Chin J Met Sci Technol, 1991; 7: 391 6 Jones H. J Mater Sci, 1984; 19: 1043 7 Staudihammer K P, Murr L E. Atlas of Binary Alloy. New York: Marcel Dekker Inc, 1973: 6 8 JCPDS, Set 19--26, in Powder Diffraction File, Inorganic Volume, No. PDIS--20iRB, 1979: 9 9 JCPDS, Set 18--20, in Powder Diffraction File, Inorganic Volume, No. PDIS--18iRB, 1974: 571 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|