    					| 氮在灰铸铁溶液中溶解度的热力学研究 | 
  					 
  					  										
						| 翟启杰;胡汉起 | 
					 
															
					| 北京科技大学;北京科技大学 | 
					 
										
						 | 
					 
   										
    					| THERMODYNAMIC STUDY ON SOLUBILITY OF NITROGEN IN GRAY CAST IRON MELTS | 
  					 
  					  					  					
						| ZHAI Qijie;HU Hanqi University of Science and Technology Beijing | 
					 
														 
				
				引用本文: 
				
								翟启杰;胡汉起. 氮在灰铸铁溶液中溶解度的热力学研究[J]. 金属学报, 1991, 27(4): 145-147.	
																												 																				 ,
																												 . 
				THERMODYNAMIC STUDY ON SOLUBILITY OF NITROGEN IN GRAY CAST IRON MELTS[J]. Acta Metall Sin, 1991, 27(4): 145-147.	                                                        				  
				
				
					
						
							
								
									
									
									
									
									 
          
          
            
                         
            
									            
									                
																														  
																  1 翟启杰,马蕊,胡汉起.钢铁研究学报,1990;2(3) :89-94 2 丁培墉.物理化学.北京:冶金工业出版社,1979:105,114-115 3 Hughes I C H. Trans Am Foundrymen's Soc, 1969; 77: 121--133 4 Dawson J V. Foundry Trade J, 1985; 158(3304) : 315--322 5 徐祖耀.金属材料热力学.北京:科学出版社,1981:138 6 马理.北京科技大学学报(物质结构分析和化学分析专辑),1989:(3) :96-100M | 
															   
																													 
									             
									           
             
			            			 
			 
             
												
											    	
											        	 | 