| 金属及合金中射程参数的研究 |
| 王德宁;王渭源 |
| 中国科学院上海冶金研究所第六研究室;副研究员;上海(200050);中国科学院上海冶金所离子束开放实验室 |
|
| INVESTIGATION OF RANGE PARAMETERS IN METAL AND ALLOY |
| WANG Dening;WANG Weiyuan Ion implantation Laboratory; Shanghai Institute of Metallurgy; Academia Sinica associate ptofessor;Laboratory No.6;Shanghai Institute of Metallurgy;Academia Sinica; Shanghai 200050 |
引用本文:
王德宁;王渭源. 金属及合金中射程参数的研究[J]. 金属学报, 1990, 26(3): 30-34.
,
.
INVESTIGATION OF RANGE PARAMETERS IN METAL AND ALLOY[J]. Acta Metall Sin, 1990, 26(3): 30-34.
1 Anderson H H, Ziegler J F. Hydrogen Stopping Power and Range in all Element, Vol. III, New York: Pergamon, 1977: 1 2 Anderson H H, Ziegler J F. Helium Stopping Power and Range in all Element. Vol. IV, New York: Pergamon, 1978: 1 3 Beck P A. Electronic Structure and Alloy Chemistty of the Transition Element, New York: Interscience, 1982: 139 4 Brandt W, Kitagawa. Phys Rev, 1982; B25: 5631 S Gibbons J F. Project Range Statistics in Semiconductors, 2nd ed, New York: Halstead Press, 1975: 30 6 Biersack J P, Eckstein W. Appl Phys, 1984; A34: 73 7 Oen O S, Holmes D K, Robinson M T. J Appl Phys, 1963; 34: 302 8 Lindhard J, Scharff M, Schiφtt H E. Mat Fys Medd Dan Vid Solsk, 1964; 34 (4) : 1 9 Neuwirth W, Pietsch W, Richter K, Hauser U. Z Phys, 1975; A275: 215 10 Neuwirth W, Pietsch W, Richter K, Hauser U. Z Phys, 1975; A275: 209 11 Alonso J A, Girifalco L A. J Phys Chem Solids, 1978; 39: 79b |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|