| Cr,Cu,Co对Fe-Si-B非晶合金磁致伸缩系数的影响 |
| 何正明;赵妙余;张玲芬;汪晓光 |
| 中国科学技术大学物理系;讲师;合肥(230026);中国科学技术大学;中国科学技术大学;中国科学技术大学 |
|
| EFFECT OF Cr, Cu AND Co ON MAGNETOSTRICTION OF Fe-Si-B AMORPHOUS ALLOYS |
| HE Zhengming;ZHAO Miaoyu;ZHANG Lingfen;WANG Xiaoguang University of Science and Technology of China; Hefei HE Zhengming; Department of Physics; University of Science and Technology of China; 230026 Hefei |
引用本文:
何正明;赵妙余;张玲芬;汪晓光. Cr,Cu,Co对Fe-Si-B非晶合金磁致伸缩系数的影响[J]. 金属学报, 1989, 25(5): 115-118.
,
,
,
.
EFFECT OF Cr, Cu AND Co ON MAGNETOSTRICTION OF Fe-Si-B AMORPHOUS ALLOYS[J]. Acta Metall Sin, 1989, 25(5): 115-118.
1 Tsuya N, Arai K I. J Magn Magn Mater, 1983; 31--34: 1594--1596 2 Kazama N S, Masumoto T, Mithera M. J Magn Magn Mater, 1980; 15--18: 1331--1335 3 Mizoguchi T. AIP Conf Proc, 1976; 34: 286 4 Narita K, Yamasaki J, Fukunaga H. J Appl Phys, 1979; 50: 7591--7593 S Tsuga N, Arai K I, Ohsaka T. IEEE Trans Magn, 1978; MAG-14 6 Hoselitz K. J Magn Magn Mater, 1982; 26: 106--108 7 Aso K, Uedaira S, Hayakawa M, Hotai K, Ochiai Y, Hayashi K, Ymakino J Magn Magn Mater, 1983; 31--34: 1546--1548 |
|