| 金属学报 DOI: 10.11900/0412.1961.2026.00202 |
|
|
|
| Nb-V微合金化钢的抗高压氢脆机制 |
刘 璐1 齐亚猛2,3 张忠铧2,3 施 浩2,3 李 喜1
|
1 上海交通大学 材料科学与工程学院 上海 200240
2 宝山钢铁股份有限公司 中央研究院 上海 201900
3 宝山钢铁股份有限公司 油气钻采输送装备全国重点实验室 上海 201900
|
|
| High-Pressure Hydrogen Embrittlement Resistance Mechanism of Nb and V Microalloyed Steel |
LIU Lu 1, QI Yameng 2,3,
ZHANG Zhonghua 2,3, SHI Hao 2,3, LI Xi 1
|
1 School of Materials
Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China
2 Baosteel Research Institute,
Baoshan Iron and Steel Co. Ltd., Shanghai 201900, China
3 State Key Laboratory of
Oil and Gas Equipment, Baoshan Iron and Steel Co. Ltd, Shanghai 201900, China
|
引用本文:
刘璐, 齐亚猛, 张忠铧, 施浩, 李喜. Nb-V微合金化钢的抗高压氢脆机制[J]. 金属学报, DOI: 10.11900/0412.1961.2026.00202.
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|